# US 6,729,402 B2 · Method of recovering hydrocarbon fluids from a subterranean reservoir

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,729,402 B2
- Document ID: US6729402B2
- Status: Granted
- Kind: B2
- Application number: 10/251,742
- Filed: 2002-09-20
- Published: 2003-08-21
- Granted: 2004-05-04
- Earliest claimed: 2000-06-14
- Assignees: Ondeo Nalco Energy Services, L.P.
- Inventors: Kin-Tai Chang; Harry Frampton; James C. Morgan
- Web page: https://patentgrep.com/patent/US6729402B2

## CPC

- C09K 8/516: characterised by their form or by the form of their components, e.g. encapsulated material
- C09K 8/512: containing cross-linking agents
- C09K 8/588: characterised by the use of specific polymers {(polymeric surfactants C09K8/584)}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

This invention is directed to a composition comprising expandable cross linked polymeric microparticles having an unexpanded volume average particle size diameter of from about 0.05 to about 10 microns and a cross linking agent content of about 1,000 to less than about 9,000 ppm of labile cross linkers and from 0 to about 300 ppm of non-labile cross linkers and to the use of the composition for modifying the permeability of subterranean formations and increasing the mobilization and/or recovery rate of hydrocarbon fluids present in the formations.

## Claims

### Claim 1

A method of modifying the permeability to water of a subterranean formation comprising injecting into the subterranean formation a composition comprising highly cross linked expandable polymeric microparticles having an unexpanded volume average particle size diameter of from about 0.05 to about 10 microns and a cross linking agent content of about 1,000 to less than about 9,000 ppm of labile cross linkers and from 0 to about 300 ppm of non-labile cross linkers, wherein the microparticles have a smaller diameter than the pores of the subterranean formation and wherein the labile cross linkers break under the conditions of temperature and pH in the subterranean formation to form expanded microparticles.

### Claim 2 (depends on 1)

The method of claim 1 wherein the unexpanded volume average particle size diameter is from about 0.1 to about 3 microns.

### Claim 3 (depends on 1)

The method of claim 1 wherein the unexpanded volume average particle size diameter is from about 0.1 to about 1 microns.

### Claim 4 (depends on 1)

The method of claim 1 wherein the microparticle contains about 2,000 ppm to less than about 9,000 ppm of labile cross linkers.

### Claim 5 (depends on 1)

The method of claim 1 wherein the microparticle contains about 3,000 ppm to less than about 9,000 ppm of labile cross linkers.

### Claim 6 (depends on 1)

The method of claim 1 wherein the labile cross linker is selected from diacrylates and polyfunctional vinyl derivatives of a polyalcohol.

### Claim 7 (depends on 1)

The method of claim 1 wherein the polymeric microparticle is selected from the group consisting of cationic, anionic, amphoteric, ion-pair or betaine-containing polymeric microparticles.

### Claim 8 (depends on 6)

The method of claim 6 wherein composition is in the form of an emulsion or aqueous suspension.

### Claim 9 (depends on 7)

The method of claim 7 wherein the cross linked polymeric microparticle is anionic.

### Claim 10 (depends on 8)

The method of claim 8 wherein the anionic polymeric microparticle comprises from about 95 to about 10 mole percent of nonionic monomers and from about 5 to about 90 mole percent anionic monomers.

### Claim 11 (depends on 9)

The method of claim 9 wherein the nonionic monomer is acrylamide.

### Claim 12 (depends on 99)

The method of claim 99 wherein the anionic monomer is 2-acrylamido-2-methyl-1-propanesulfonic acid.

### Claim 13 (depends on 11)

The method of claim 11 wherein the labile cross linker is polyethyleneglycol diacrylate.

### Claim 14 (depends on 11)

The method of claim 11 wherein the non-labile cross linker is methylene bisacrylamide.

### Claim 15 (depends on 1)

The method of claim 1 wherein the composition comprises about 100 ppm to about 10,000 ppm, based on polymer actives, of the microparticle.

### Claim 16 (depends on 1)

The method of claim 1 wherein the composition comprises about 500 ppm to about 1,500 ppm, based on polymer actives, of the microparticle.

### Claim 17 (depends on 1)

The method of claim 1 wherein the composition comprises about 500 ppm to about 1,000 ppm, based on polymer actives, of the microparticle.

### Claim 18 (depends on 1)

The method of claim 1 wherein the composition is added to injection water as part of a secondary or tertiary process for the recovery of hydrocarbon from the subterranean formation.

### Claim 19 (depends on 17)

The method of claim 17 wherein the injection water is added to the subterranean formation at a temperature lower than the temperature of the subterranean formation.

### Claim 20 (depends on 1)

The method of claim 1 wherein the subterranean formation is a sandstone or carbonate hydrocarbon reservoir.

### Claim 21 (depends on 17)

The method of claim 17 wherein the composition is used in a carbon dioxide and water tertiary recovery project.

### Claim 22 (depends on 17)

The method of claim 17 wherein the composition is used in a tertiary oil recovery process, one component of which constitutes water injection.

### Claim 23 (depends on 17)

The method of claim 17 wherein the injection water is added to a producing well.

### Claim 24

A method of increasing the mobilization or recovery rate of hydrocarbon fluids in a subterranean formation comprising injecting into the subterranean formation a composition comprising highly cross linked expandable polymeric microparticles having an unexpanded volume average particle size diameter of from about 0.05 to about 10 microns and a cross linking agent content of about 1,000 to less than about 9,000 ppm of labile cross linkers and from 0 to about 300 ppm of non-labile cross linkers, wherein the microparticles have a smaller diameter than the pores of the subterranean formation and wherein the labile cross linkers break under the conditions of temperature and pH in the subterranean formation to decrease the mobility of the composition.

### Claim 25 (depends on 23)

The method of claim 23 wherein the composition comprises about 100 ppm to about 10,000 ppm, based on polymer actives, of the microparticle.

### Claim 26 (depends on 23)

The method of claim 23 wherein the composition comprises about 500 ppm to about 1,500 ppm, based on polymer actives, of the microparticle.

### Claim 27 (depends on 23)

The method of claim 23 wherein the composition comprises about 500 ppm to about 1,000 ppm, based on polymer actives, of the microparticle.

### Claim 28 (depends on 23)

The method of claim 23 wherein the composition is added to injection water as part of a secondary or tertiary process for the recovery of hydrocarbon from the subterranean formation.

### Claim 29 (depends on 23)

The method of claim 23 wherein the injection water is added to the subterranean formation at a temperature lower than the temperature of the subterranean formation.

### Claim 30 (depends on 23)

The method of claim 23 wherein the subterranean formation is a sandstone or carbonate hydrocarbon reservoir.

### Claim 31

A method of preparing highly cross linked expandable polymeric microparticles having an unexpanded volume average particle size diameter of from about 0.05 to about 10 microns comprising polymerizing one or more allylic, vinylic or acrylic monomers under free-radical forming conditions in the presence of about 1,000 to less than about 9,000 ppm of labile cross linkers and 0 to about 300 ppm of non-labile cross linkers.