# US 6,727,342 B1 · Use of polyester resins for the production of articles having good properties as barriers to water vapor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,342 B1
- Document ID: US6727342B1
- Status: Granted
- Kind: B1
- Application number: 09/786,097
- Filed: 2001-06-08
- Granted: 2004-04-27
- Earliest claimed: 1998-08-28
- Assignees: Ministero Dell'Universita'E Della Ricerca Scientifica Technologica
- Inventors: Catia Bastioli; Marco Foa'; Giandomenico Cella; Giovanni Floridi; Fernanda Farachi; Tiziana Milizia
- Web page: https://patentgrep.com/patent/US6727342B1

## CPC

- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- C08L 3/00: Compositions of starch, amylose or amylopectin or of their derivatives or degradation products
- Y10T 428/1331: Single layer [continuous layer]
- Y10T 428/31504: Composite [nonstructural laminate]
- Y10T 428/31786: Of polyester [e.g., alkyd, etc.]
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Polyester resins formed by recurring units X=[O—(CH2)n—OCO—(CH2)m—CO] and/or Y=[O—(CH2)k—CO], where the half-sum of n+m is equal to or greater than 6 and k is a number equal to or greater than 6, or by copolymers comprising units and/or sequences having the formula xi[O—(CH2)ni—OCO—(CH2)mi—CO]; yj[O—(CH2)kj—CO] where: i,j=1-5; ni=2-22; mi=0-20; kj=1=21; (Formula (1)) and xi and yj vary between 0 and 1 and are molar fractions of the various units such that (Formula (2)), are used for the preparation of products in which a permeability to water vapour of less than 350 g×30 μm/m2 per day, measured at 38° C. and 90% RH and good biodegradability are required. ∑ i = 1 5 ⁢ x i + ∑ j = 1 5 ⁢ y j = 1 ( 1 ) ∑ i = 1 5 ⁢ x i · ( n i + m i 2 ) + ∑ j = 1 5 ⁢ y j · k j ≥ 6 ( 2 )

## Claims

### Claim 1

A method of making a biodegradable article having a permeability to water vapor of less than 350 g×30 μm/m2 per day at 38° C. and 90% RH comprising:
manufacturing articles from aliphatic polyester resin,
wherein said aliphatic polyester resin further comprises
a) recurring units X=[O—(CH2)n—OCO—(CH2)m—CO] and/or Y=[O—(CH2)k—CO], where the half-sum of n+m is equal to or greater than 6 and k is a number equal to or greater than 6, or by copolymers comprising units and/or sequences having the formula xi[O—(CH2)ni—OCO—(CH2)mi—CO]; yj[O—(CH2)kj—CO] where: i, j=1-5; ni=2-22; mi=0-20; kj=1-21; ∑ i = 1 5 ⁢ x i + ∑ j = 1 5 ⁢ y j = 1
and xi and yj vary between 0 and 1 and are molar fractions of the various units such that ∑ i = 1 5 ⁢ x i · ( n i + m i 2 ) + ∑ j = 1 5 ⁢ y j · k j ≥ 6 ,
or
b) recurring units Z=[O—(CH2)a-OCO—(CH2)b-CO] where a=2-3, b=7-11, and has an intrinsic viscosity (in chloroform at 25° C.) greater than 0.7 and up to 2.5 dl/g, a melting point from 60° to 110° C., and a biodegradability such that, under composting conditions, a 30 μm film of said resin shows a decomposition of less than 10% in 14 days and more than 90% in six months.

### Claim 2 (depends on 1)

The method of claim 1, in which the polyester resin is produced by polycondensation of bicarboxylic aliphatic acids with from 2 to 22 carbon atoms and of diols with from 2 to 22 carbon atoms, selected in a manner such that the half-sum of the number of carbon atoms relating to the acid and to the diol is greater than 6, or by polycondensation of hydroxyl-acids, or by ring-opening of corresponding lactones or lactides having 7 to 22 carbon atoms.

### Claim 3 (depends on 2)

The method of claim 2, in which the diacids and the dialcohols are obtained from renewable resources.

### Claim 4 (depends on 1)

The method of claim 1, in which the polyester resin is selected from polyethylene sebacate, polybutandiol sebacate, polyhexandiol azelate, polyhexandiol sebacate, polynonandiol azelate, polynonandiol sebacate, polyoctandiol azelate, polyocatandiol brassilate, polydecandiol sebacate, and polydecandiol brassilate.

### Claim 5 (depends on 1)

The method of claim 1, in which the polyester resin is subjected to an upgrading process.

### Claim 6 (depends on 1)

The method of claim 1, in which the polyester resin is a component of a blend of unmodified or modified polysacchanides.

### Claim 7 (depends on 1)

The method of claim 1, in which the polyester resin contains mineral or vegetable fillers and/or additives selected from lubricants, plasticizers, colourings, flavourings, perfumes, flame-proofing agents, stabilizers with regard to hydrolysis and to thermal degradation, and antioxidants.

### Claim 8 (depends on 1)

The method of claim 1, in which the mean numeral molecular weight of the polyester resin is between 45000 and 70000.

### Claim 9 (depends on 1)

The method of claim 1, wherein said articles are selected from:
coatings which are produced by extrusion-coating, with water-vapour barrier properties, and which are usable for the packaging of fresh milk and dairy products, of meat, and of foods having high water content,
multilayer laminates with layers of paper, plastics material and or paper/plastics material, aluminum and metalized films,
films as such and multi-layer films with other polymer materials,
sacks for organic refuse and for grass cuttings with periods of use longer than 1 week,
single-layer and multi-layer food packaging comprising containers for milk, toghurt, cheeses, meat and beverages, in which the layer in contact with the food or beverage is formed by the aliphatic polyester,
composites with gelatinized or destructured starch, and/or complexed starch or natural starch as a filler,
mono-directional and bi-directional films,
semi-expanded and expanded products produced by physical and/or chemical means, by extrusion, injection, or agglomeration or pre-expanded particles,
expanded sheet and expanded containers for foods, for drugs, and for fast food,
fibres, fabrics and non-woven fabrics in the hygiene, sanitary, and clothing fields,
composites with mineral and vegetable fillers
thermoformed sheets for the food or fast-food packaging fields,
bottles for the food cosmetics and pharmaceutical fields,
fishing nets,
containers for fruit and vegetables,
extruded sections usable in the fast-food field and irrigation pipes in the agricultural field.

### Claim 10 (depends on 1)

Polyester resins as defined in claim 1 in blends with other biodegradable polymers having a permeability to water vapour greater than 300 g×30 μm/m2 per day at 38° C. and 90% RH.

### Claim 11 (depends on 1)

Polyester resins as defined in claim 1 in blends with polylactic acid.

### Claim 12 (depends on 1)

Polyester resins as defined in claim 1 in blends with other non-biodegradable polymers, the said polymers having a permeability to water vapour greater than 300 g×30 μm/m2 per day at 38° C. and 90% RH.

### Claim 13

An article of manufacture comprising:
a biodegradable article having a permeability to water vapor of less than 350 g×30 μm/m2 per day at 38° C. and 90% RH manufactured from aliphatic polyester resin,
wherein said aliphatic polyester resin further comprises
a) recurring units X=[O—(CH2)n—OCO—(CH2)m—CO] and/or Y=[O—(CH2)k—CO], where the half-sum of n+m is equal to or greater than 6 and k is a number equal to or greater than 6, or by copolymers comprising units and/or sequences having the formula xi[O—(CH2)ni—OCO—(CH2)mi—CO]; yj[O—(CH2)kj—CO] where: i, j=1-5; ni=2-22; mi=0-20; kj=1-21; ∑ i = 1 5 ⁢ x i + ∑ j = 1 5 ⁢ y j = 1
and xi and yj vary between 0 an 1 and are molar fractions of the various units such that ∑ i = 1 5 ⁢ x i · ( n i + m i 2 ) + ∑ j = 1 5 ⁢ y j · k j ≥ 6 ,
or
b) recurring units Z=[O—(CH2)a-OCO—(CH2)b-CO] where a=2-3, b=7-11, and
has an intrinsic viscosity (in chloroform at 25° C.) greater than 0.7 and up to 2.5 dl/g, a melting point from 60° to 110° C., and a biodegradability such that, under composting conditions, a 30 μm film of said resin shows a decomposition of less than 10% in 14 days and more than 90% in six months.