# US 6,727,293 B2 · Novolac-epoxy resin foam, foamable composition for making novolac-epoxy resin foam and method of making novolac-epoxy resin foam

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,293 B2
- Document ID: US6727293B2
- Status: Granted
- Kind: B2
- Application number: 10/464,444
- Filed: 2003-06-19
- Published: 2003-11-20
- Granted: 2004-04-27
- Earliest claimed: 1999-11-09
- Assignees: American Foam Technologies, Inc.
- Inventors: Samuel L. Rader
- Web page: https://patentgrep.com/patent/US6727293B2

## CPC

- C08J 9/02: using blowing gases generated by the reacting monomers or modifying agents during the preparation or modification of macromolecules
- C08J 2205/052: Closed cells, i.e. more than 50% of the pores are closed
- C08J 2363/02: Polyglycidyl ethers of bis-phenols
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

Provided is a foamable composition adapted to form a cross-linked novolac-epoxy resin foam. The foamable composition is formulated from a composition comprising at least one novolac resin, at least one epoxy resin, and at least one blowing agent.

## Claims

### Claim 1

A novolac-epoxy resin foam having a cross-linked polymeric matrix formed by reacting a composition comprising:
at least one liquid novolac resin;
at least one liquid epoxy resin; and
at least one reactive blowing agent which generates a blowing gas by reaction during curing of the novolac resin and epoxy resin and provides heat of reaction to increase a cure speed, wherein the composition is formulated such that when the novolac resin and epoxy resin are combined during foaming no external heat beyond ambient temperature is required to initiate the formation of the foam and once foaming is initiated heat from the reactive blowing agent increases the cure speed.

### Claim 2 (depends on 1)

A foam according to claim 1, wherein at least 80% of the cells are closed.

### Claim 3 (depends on 1)

A foam according to claim 1, wherein at least 90% of the cells are closed.

### Claim 4 (depends on 1)

A foam according to claim 1, wherein the foam is a rigid novolac-epoxy resin foam formulated from more epoxy resin than novolac resin.

### Claim 5 (depends on 1)

A foam according to claim 1, wherein the foam is a flexible novolac-epoxy resin foam formulated from more novolac resin than epoxy resin.

### Claim 6 (depends on 1)

A loam according to claim 1, wherein said novolac resin is present in an amount of from about 5 to about 95% by weight and said epoxy resin is present in an amount of from about 5 to about 95% by weight, all weight % based on the total weight of the composition.

### Claim 7 (depends on 1)

A foam according to claim 1, wherein said novolac resin is present in an amount of from about 20 to about 80% by weight and said epoxy resin is present in an amount of from about 20 to about 80% by weight, all weight % based on the total weight of the composition.

### Claim 8 (depends on 1)

A foam according to claim 1, wherein said novolac resin is present in an amount of from about 40 to about 60% by weight and said epoxy resin is present in an amount of from about 40 to about 60% by weight, all weight % based on the total weight of the composition.

### Claim 9 (depends on 1)

A foam according to claim 1, wherein at least one novolac resin is free of epoxide groups.

### Claim 10 (depends on 1)

A foam according to claim 1, wherein the foam has a pH of from about 7 to about 9.

### Claim 11 (depends on 1)

A foam according to claim 1, wherein the foam has a pH of about 9.

### Claim 12 (depends on 1)

A foam according to claim 1, wherein the novolac resin has a number average molecular weight of from about 100 to about 500 and the epoxy resin has a number average molecular weight of about 250 to about 650.

### Claim 13 (depends on 1)

A foam according to claim 1, wherein a ratio between novolac resin and epoxy resin has been adjusted to provide a more flexible foam by increasing the amount of novolak resin.

### Claim 14 (depends on 1)

A foam according to claim 1, wherein a ratio between novolac resin and epoxy resin has been adjusted to provide a more rigid foam by increasing the amount of epoxy resin.

### Claim 15 (depends on 1)

A foam according to claim 1, wherein the foam was formed under ambient pressure to provide a foam having a closed-cell content of greater than 80%.

### Claim 16 (depends on 1)

A foam according to claim 1, wherein the foam was formed under ambient pressure to provide a foam having a closed-cell content of greater than 90%.

### Claim 17 (depends on 1)

A foam according to claim 1, wherein the reactive blowing agent comprises a compound having a reactive hydrogen group and the composition further comprises an amine catalyst such that when the reactive blowing agent and the amine catalyst are combined hydrogen gas is formed which blows the foam and heat is produced which increases the curing speed of the novlac and epoxy reaction.

### Claim 18 (depends on 17)

A foam according to claim 17, wherein the reactive blowing agent comprises a silicone compound having a reactive hydrogen group.

### Claim 19 (depends on 1)

A foam according to claim 1, wherein the reactive blowing agent is present in an amount such that during blowing the temperature is raised from ambient temperature to about 100 to 140° F. within 1 minute after combining the novolac resin and epoxy resin.

### Claim 20 (depends on 1)

A foam according to claim 1, wherein a surfactant was used to form the foam.

### Claim 21 (depends on 20)

A foam according to claim 20, wherein the surfactant is present in an amount of from about 0.01% to about 5% by weight.

### Claim 22 (depends on 1)

A foam according to claim 1, wherein foam is free of hydroxyl groups to increase non-flamability.

### Claim 23 (depends on 1)

A foam according to claim 1, further comprising a flame retardant to increase non-flamability of the foam.

### Claim 24 (depends on 23)

A foam according to claim 23, wherein the flame retardant is present in a amount of from about 10% to about 40% by weight.

### Claim 25 (depends on 1)

A foam according to claim 1, wherein the foam is a sprayed novolac-epoxy resin foam.

### Claim 26 (depends on 25)

A foam according to claim 25, wherein the composition has a viscosity of about 50 to about 1000 centipoise at 25° C.

### Claim 27 (depends on 25)

A foam according to claim 25, wherein the composition has a viscosity of about 50 to about 500 centipoise at 25° C.

### Claim 28 (depends on 25)

A foam according to claim 25, wherein the composition has a cure speed of about 5 minutes or less.

### Claim 29 (depends on 25)

A foam according to claim 25, further comprising at least two foam layers.

### Claim 30 (depends on 29)

A foam according to claim 29, wherein a first foam layer was sprayed on a second foam layer before the first foam layer cured so that the first and second foam layers co-cured to provide adhesion between the first and second layers.

### Claim 31 (depends on 25)

A foam according to claim 25, wherein the sprayed foam covers an article.

### Claim 32 (depends on 1)

A foam according to claim 1, wherein the epoxy resin has about 2 or more terminal epoxide groups on average.

### Claim 33 (depends on 1)

A foam according to claim 1, wherein the epoxy resin has about 3 terminal epoxide groups on average.

### Claim 34 (depends on 25)

A foam according to claim 25, wherein the epoxy resin has about 2 or more terminal epoxide groups on average.

### Claim 35 (depends on 1)

A foam according to claim 1, wherein the foam is an insulating foam suitable for automotive applications in that is has high temperature resistance and is light weight and non-toxic when burned.

### Claim 36 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for mining applications in that is has high temperature resistance and exhibits low outgassing.

### Claim 37 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for residential and commercial building applications in that it is self extinguishing and does not produce toxic fumes when burned.

### Claim 38 (depends on 37)

A foam according to claim 37, wherein the foam is in the form of a rigid support panel.

### Claim 39 (depends on 1)

A foam according to claim 1, wherein the foam is flexible or high strength rigid foam suitable for airplane applications in that it has light weight, non-toxic when burned, high temperature resistance, and corrosion resistance.

### Claim 40 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for ship applications in that it has high temperature resistance, corrosion protection, and low toxicity when burned.

### Claim 41 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for prototyping applications in that it has high temperature resistance and corrosion resistance.

### Claim 42 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for artistic applications in that it has high temperature resistance and corrosion resistance.

### Claim 43 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for aerospace applications in that it has high temperature resistance and flexibility over a wide temperature range.

### Claim 44 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for heat shielding applications in that it has high temperature resistance.

### Claim 45 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for mass transit applications in that it has high temperature resistance and is non-toxic.

### Claim 46 (depends on 1)

A foam according to claim 1, wherein the foam is suitable for applications requiring high temperature resistance, non-toxicity and non-corrosiveness.

### Claim 47 (depends on 25)

A foam according to claim 25, wherein the epoxy resin has about 3 terminal epoxide groups on average.

### Claim 48

A sprayed novolac-epoxy resin foam having a cross-linked polymeric matrix formed by spraying a foamable composition having a viscosity of about 50 to about 1000 centipoise at 25° C. comprising:
at least one liquid novolac resin having a viscosity of about 100 to about 3,000 centipoise at 25° C;
at least one liquid epoxy resin having a viscosity of about 100 to about 10,000 centipoise at 25° C.; and
at least one reactive blowing agent which generates a blowing gas by reaction during curing of the novolac resin and epoxy resin and provides heat of reaction to increase a cure speed, wherein the composition is formulated such that when the novolac resin and epoxy resin are combined during foaming no external heat beyond ambient temperature is required to initiate the formation of the foam and once foaming is initiated heat from the reactive blowing agent increases the cure speed.