# US 6,727,200 B2 · High dielectric constant very low fired X7R ceramic capacitor, and powder for making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,200 B2
- Document ID: US6727200B2
- Status: Granted
- Kind: B2
- Application number: 10/036,205
- Filed: 2001-10-29
- Published: 2002-05-16
- Granted: 2004-04-27
- Earliest claimed: 2000-08-31
- Assignees: MRA Laboratories, Inc.
- Inventors: Galeb H. Maher; Samir Maher
- Web page: https://patentgrep.com/patent/US6727200B2

## CPC

- C04B 35/6303: {Inorganic additives}
- B32B 18/00: Layered products essentially comprising ceramics, e.g. refractory products
- C04B 35/465: based on alkaline earth metal titanates
- C04B 35/468: based on barium titanates
- C04B 35/4682: {based on BaTiO3 perovskite phase}
- C04B 35/628: Coating the powders {or the macroscopic reinforcing agents}
- H01G 4/1218: {based on titanium oxides or titanates (H01G4/1245 takes precedence)}
- H01G 4/1227: {based on alkaline earth titanates}
- H01G 4/1245: {containing also titanates}
- H01G 4/30: Stacked capacitors (H01G4/33 takes precedence)
- B32B 2311/08: Silver
- C04B 2235/3201: Alkali metal oxides or oxide-forming salts thereof
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3215: Barium oxides or oxide-forming salts thereof
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3229: Cerium oxides or oxide-forming salts thereof
- C04B 2235/3232: Titanium oxides or titanates, e.g. rutile or anatase
- C04B 2235/3236: Alkaline earth titanates
- C04B 2235/3239: Vanadium oxides, vanadates or oxide forming salts thereof, e.g. magnesium vanadate
- C04B 2235/3244: Zirconium oxides, zirconates, hafnium oxides, hafnates, or oxide-forming salts thereof
- C04B 2235/3251: Niobium oxides, niobates, tantalum oxides, tantalates, or oxide-forming salts thereof
- C04B 2235/3255: Niobates or tantalates, e.g. silver niobate
- C04B 2235/3256: Molybdenum oxides, molybdates or oxide forming salts thereof, e.g. cadmium molybdate
- C04B 2235/3258: Tungsten oxides, tungstates, or oxide-forming salts thereof
- C04B 2235/3262: Manganese oxides, manganates, rhenium oxides or oxide-forming salts thereof, e.g. MnO
- C04B 2235/3294: Antimony oxides, antimonates, antimonites or oxide forming salts thereof, indium antimonate
- C04B 2235/3409: Boron oxide, borates, boric acids, or oxide forming salts thereof, e.g. borax
- C04B 2235/365: Borosilicate glass
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/77: Density
- C04B 2235/78: Grain sizes and shapes, product microstructures, e.g. acicular grains, equiaxed grains, platelet-structures
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/786: Micrometer sized grains, i.e. from 1 to 100 micron
- C04B 2235/79: Non-stoichiometric products, e.g. perovskites (ABO3) with an A/B-ratio other than 1
- C04B 2237/346: Titania or titanates
- C04B 2237/40: Metallic
- C04B 2237/408: Noble metals, e.g. palladium, platina or silver
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A dielectric ceramic powder and multilayer ceramic capacitors made from the powders are disclosed. A dielectric start powder mixture includes at least ninety weight percent essentially pure barium titanate powder having an average particle size of from 0.2 to 1.2 microns; from 0.2 to 2.5 weight percent of barium lithium borosilicate; from 0.1 to 0.3 weight percent of MnCO3; 0.4 to 1.50 weight percent Nb205 or a niobate compound, or a molar equivalent of Ta2O5 or a tantalum compound as a grain growth inhibitor; and, 0.4 to 1.2 weight percent of gadolinium oxide (Gd2O3). The start powder mixture is calcined and then sintered in an open zirconia setter at from 950° C. to 1,025° C. to produce a dielectric ceramic body that satisfies X7R capacitor performance characteristics; that includes no hazardous heavy metal oxides; and, that may include silver-palladium electrodes having 85 weight percent or more of silver.

## Claims

### Claim 1

A dielectric ceramic start powder comprising:
a. at least ninety weight percent essentially pure barium titanate having an average particle size of from 0.2 to 1.2 microns;
b. from 0.2 to 2.5 weight percent barium lithium borosilicate;
c. from 0.1 to 0.3 weight percent MnCO3;
d. a grain growth inhibitor selected from the group consisting of niobium compounds Nb2O5, BaNb2O6, CaNb2O6, MgNb2O6, LiNbO3, or mixtures thereof such that a weight percent of Nb2O5 ranges from 0.4 wt % to 1.50 wt %, or tantalum compounds, or mixtures thereof, such that a weight percent of Ta2O5 ranges from 0.66 wt % to 2.50 wt %, or a mixture of molar equivalents of the niobium and tantalum compounds; and,
e. from 0.4 to 1.2 weight percent gadolinium oxide.

### Claim 2 (depends on 1)

The dielectric ceramic start powder of claim 1, wherein the weight percent of the gadolinium oxide is about 0.8 percent.

### Claim 3 (depends on 1)

The dielectric ceramic start powder of claim 1, wherein the weight percent of the grain growth inhibitor is about 1.0 percent Nb2O5.

### Claim 4 (depends on 1)

The dielectric ceramic start powder of claim 1, further comprising from 0.2 to 0.6 weight percent of WO3.

### Claim 5 (depends on 1)

The dielectric ceramic start powder of claim 1, further comprising from 0.07 to 0.2 weight percent of MoO3.

### Claim 6

A method for making a dielectric ceramic powder comprising the steps of:
a. preparing a mixture of a dielectric ceramic start powder including at least ninety weight percent essentially pure barium titanate having an average particle size of from 0.2 to 1.2 microns, from 0.2 to 2.5 weight percent barium lithium borosilicate, from 0.1 to 0.3 weight percent MnCO3, a grain growth inhibitor selected from the group consisting of niobium compounds Nb2O5, BaNb2O6, CaNb2O6, MgNb2O6, LiNbO3, or mixtures thereof such that a weight percent of Nb2O5 ranges from 0.4 wt % to 1.50 wt %, or tantalum compounds, or mixtures thereof, such that a weight percent of Ta2O5 ranges from 0.66 wt % to 2.50 wt %, or a mixture of molar equivalents of the niobium and tantalum compounds; and, from 0.4 to 1.2 weight percent gadolinium oxide;
b. mildly calcining the dielectric ceramic start powder at about 450° C. to about 550° C. to obtain a dielectric ceramic powder comprised of agglomerates of the mixture of start powder wherein each of the agglomerates has essentially the same compositional ratios as the start powder of the barium titanate, barium lithium borosilicate, Nb2O5, MnCO3, and gadolinium oxide;
to provide a dielectric ceramic powder capable of being sintered in open air at from 950° C. to 1,025° C. to produce a dielectric ceramic body that satisfies X7R capacitor performance characteristics.

### Claim 7 (depends on 6)

The method for making the dielectric ceramic powder of claim 6, wherein the weight percent of the gadolinium oxide is about 0.8 percent.

### Claim 8 (depends on 6)

The method for making the dielectric ceramic powder of claim 6, wherein the weight percent of the grain growth inhibitor is about 1.0 percent Nb2O5.

### Claim 9 (depends on 6)

The method for making the dielectric ceramic powder of claim 6, wherein the preparing a mixture step further comprises mixing from 0.2 to 0.6 weight percent of WO3 in the mixture and mixing from 0.07 to 0.2 weight percent of MoO3 in the mixture.

### Claim 10

A method for making a multilayer ceramic capacitor that satisfies X7R capacitor performance characteristics, comprising the steps of:
a. preparing a mixture of a dielectric ceramic start powder including at least ninety weight percent essentially pure barium titanate having an average particle size of from 0.2 to 1.2 microns, from 0.2 to 2.5 weight percent barium lithium borosilicate, from 0.1 to 0.3 weight percent MnCO3; a grain growth inhibitor selected from the group consisting of niobium compounds Nb2O5, BaNb2O6, CaNb2O6, MgNb2O6, LiNbO3, or mixtures thereof such that a weight percent of Nb2O5 ranges from 0.4 wt % to 1.50 wt %, or tantalum compounds, or mixtures thereof, such that a weight percent of Ta2O5 ranges from 0.66 wt % to 2.50 wt %, or a mixture of molar equivalents of the niobium and tantalum compounds; and, from 0.4 to 1.2 weight percent gadolinium oxide;
b. mildly calcining the dielectric ceramic start powder at about 450° C. to about 550° C. to obtain a dielectric ceramic powder comprised of agglomerates of the mixture of start powder wherein each of the agglomerates has essentially the same compositional ratios as the start powder of the barium titanate, barium lithium borosilicate, Nb2O5, MnCO3, and gadolinium oxide;
c. forming a slurry of the calcined ceramic powder;
d. preparing layers of the slurry;
e. forming a stack of a plurality of the layers and interleaving at least one silver-palladium electrode between adjacent layers;
f. heating to mature the stack of layers by sintering in open air at a temperature of between 950° C. to 1,025° C. to produce a multilayer ceramic capacitor body with at least one buried electrode.

### Claim 11 (depends on 10)

The method for making a multilayer ceramic capacitor of claim 10, wherein the silver-palladium electrode comprises 85 weight percent or more of silver.

### Claim 12 (depends on 11)

The method for making a multilayer ceramic capacitor of claim 11, wherein the weight percent of the gadolinium oxide is about 0.8 percent.

### Claim 13 (depends on 12)

The method for making the multilayer ceramic capacitor of claim 12 wherein the weight percent of the grain growth inhibitor Nb2O5 is about 1.0 percent Nb2O5.

### Claim 14 (depends on 13)

The method for making the multilayer ceramic capacitor of claim 13, wherein the preparing a mixture step further comprises mixing from 0.2 to 0.6 weight percent of WO3 in the mixture, and mixing from 0.07 to 0.2 weight percent of MoO3 in the mixture.

### Claim 15

A multilayer ceramic capacitor that satisfies X7R capacitor performance characteristics having a least one electrode buried within a body of the capacitor, and an external terminal connected to the at least one electrode, the body comprising:
a. at least ninety weight percent essentially pure barium titanate;
b. from 0.2 to 2.5 weight percent barium lithium borosilicate;
c. from 0.1 to 0.3 weight percent MnCO3;
d. a grain growth inhibitor selected from the group consisting of niobium compounds Nb2O5, BaNb2O6, CaNb2O6, MgNb2O6, LiNbO3, or mixtures thereof such that a weight percent of Nb2O5 ranges from 0.4 wt % to 1.50 wt %, or tantalum compounds, or mixtures thereof, such that a weight percent of Ta2O5 ranges from 0.66 wt % to 2.50 wt %, or a mixture of molar equivalents of the niobium and tantalum compounds; and,
e. from 0.4 to 1.2 weight percent gadolinium oxide.

### Claim 16 (depends on 15)

The multilayer ceramic capacitor of claim 15, wherein the electrode comprises a silver-palladium electrode having 85 weight percent or more of silver.

### Claim 17 (depends on 15)

The multilayer ceramic capacitor of claim 15, wherein wherein the weight percent of the gadolinium oxide is about 0.8 percent.

### Claim 18 (depends on 15)

The multilayer ceramic capacitor of claim 15, wherein the weight percent of the grain growth inhibitor is about 1.0 percent Nb2O5.

### Claim 19 (depends on 15)

The multilayer ceramic capacitor of claim 15, further comprising from 0.2 to 0.6 weight percent of WO3 and from 0.07 to 0.2 weight percent of MoO3.