# US 6,727,190 B2 · Method of forming fluorine doped boron-phosphorous silicate glass (F-BPSG) insulating materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,190 B2
- Document ID: US6727190B2
- Status: Granted
- Kind: B2
- Application number: 09/146,839
- Filed: 1998-09-03
- Published: 2001-09-13
- Granted: 2004-04-27
- Earliest claimed: 1998-09-03
- Assignees: Micron Technology, Inc.
- Inventors: Anand Srinivasan; Gurtej Sandhu; Ravi Iyer
- Web page: https://patentgrep.com/patent/US6727190B2

## CPC

- H10P 14/6924: {the material being halogen doped silicon oxides, e.g. FSG}
- C23C 16/401: {containing silicon}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 14/6923: {the material being boron or phosphorus doped silicon oxides, e.g. BPSG, BSG or PSG}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

In one aspect, the invention includes a method of forming an insulating material comprising: a) providing a substrate within a reaction chamber; b) providing reactants comprising a Si, F and ozone within the reaction chamber; and c) depositing an insulating material comprising fluorine, silicon and oxygen onto the substrate from the reactants. In another aspect, the invention includes a method of forming a boron-doped silicon oxide having Si—F bonds, comprising: a) providing a substrate within a reaction chamber; b) providing reactants comprising Triethoxy fluorosilane, a boron-containing precursor, and ozone within the reaction chamber; and c) depositing a boron-doped silicon oxide having Si—F bonds onto the substrate from the reactants. In yet another aspect, the invention includes a method of forming a phosphorus-doped silicon oxide having Si—F bonds, comprising: a) providing a substrate within a reaction chamber; b) providing reactants comprising triethoxy fluorosilane, a phosphorus-containing precursor, and ozone within the reaction chamber; and c) depositing a phosphorus-doped silicon oxide having Si—F bonds onto the substrate from the reactants.

## Claims

### Claim 1

A method of forming a boron and phosphorus doped silicon oxide having Si—F bonds, comprising:
providing a substrate within a CVD reaction chamber at a pressure of from about 1 Torr to about 760 Torr and at a substrate temperature of from about 400° C. to about 700° C.;
flowing F-TES into the reaction chamber at a flow rate of from about 100 mg/min to about 1,000 mg/min;
flowing an ozone-containing gas into the reaction chamber at a flow rate of from about 1,000 sccm to about 8,000 sccm, the gas containing a mixture of from about 5 vol % to about 15 vol % ozone in O2;
flowing TEPO into the reaction chamber at a flow rate of from about 25 mg/min to about 400 mg/min;
flowing TEB into the reaction chamber at a flow rate of from about 25 mg/min to about 400 mg/min;
providing the F-TES, ozone-containing gas, TEPO, and TEB simultaneously in the reaction chamber; and
depositing a boron and phosphorous doped silicon oxide having Si—F bonds onto the substrate at a rate of from about 500 Å/min to about 10,000 Å/min with a plasma present in the reaction chamber, the doped silicon oxide comprising from about 3 atomic % to about 12 atomic % total of boron and phosphorous, comprising from about 0.1 atomic % to about 10 atomic % flourine, comprising more flourine than occurs in a doped silicon oxide deposited from an otherwise identical method using O2 or H2O2 instead of O3, exhibiting a flow temperature that is from about 50° C. to about 100° C. less than occurs in an otherwise identical doped silicon oxide lacking the fluorine, exhibiting a dielectric constant that is less than occurs in an otherwise identical doped silicon oxide lacking the fluorine, and exhibiting a fixed charge that is less than occurs in a doped silicon oxide deposited from an otherwise identical method using TEOS instead of F-TES.

### Claim 2 (depends on 1)

The method of claim 1 wherein the CVD reaction chamber comprises a single wafer, cold wall chamber.

### Claim 3 (depends on 1)

The method of claim 1 wherein the pressure comprises from about 10 Torr to about 700 Torr.

### Claim 4 (depends on 1)

The method of claim 1 wherein the pressure comprises from about 400 Torr to about 700 Torr.

### Claim 5 (depends on 1)

The method of claim 1 wherein the doped silicon oxide comprises from about 2 atomic % to about 10 atomic % flourine.

### Claim 6 (depends on 1)

The method of claim 1 wherein the doped silicon oxide comprises 2 atomic % fluorine.

### Claim 7 (depends on 1)

The method of claim 1 wherein the depositing occurs at a rate of from about 8,000 Å/min to about 10,000 Å/min.

### Claim 8 (depends on 1)

The method of claim 1 wherein the pressure is 600 Torr, the substrate temperature is 500° C., the ozone-containing gas flow is 2,000 sccm, the deposition rate is 8,000 Å/min, the boron composition is 3 atomic %, and the phosphorous composition is 7 atomic %.