# US 6,727,187 B2 · Fabrication method for semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,187 B2
- Document ID: US6727187B2
- Status: Granted
- Kind: B2
- Application number: 09/828,957
- Filed: 2001-04-10
- Published: 2001-11-08
- Granted: 2004-04-27
- Earliest claimed: 2000-04-27
- Assignees: Renesas Technology Corp.; Hitachi ULSI Systems Co., Ltd.
- Inventors: Yutaka Takeshima; Michimasa Funabashi; Kenji Tanaka
- Web page: https://patentgrep.com/patent/US6727187B2

## CPC

- C23F 1/18: for etching copper or alloys thereof
- H10P 70/234: {the processing being the formation of vias or contact holes}
- Y10S 438/906: Cleaning of wafer as interim step
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

For providing a cleaning technique capable of removing metal contamination at a low temperature and in a short period of time, an aqueous solution containing 0.1 to 15% by weight of hydrochloric acid, 0.01 to 0.3% by weight of hydrofluoric acid and 0.1 to 15% by weight of hydrogen peroxide is used as a cleaning solution for cleaning a semiconductor substrate after forming a gate electrode of a polymetal structure on the semiconductor substrate.

## Claims

### Claim 1

A semiconductor integrated circuit device fabrication method, using a wafer having a silicon material region and a Polymetal gate electrode having a lower silicon layer and an upper metal layer, comprising the step of cleaning a main surface of the wafer at a temperature of 15 to 40 degrees centigrade by using an aqueous solution containing 0.1 to 15% by weight of hydrochloric acid, 0.01 to 0.3% by weight of hydrofluoric acid and 0.1 to 15% by weight of hydrogen peroxide, wherein the cleaning time for the wafer is 2 minutes or less.

### Claim 2 (depends on 1)

A semiconductor integrated circuit device fabrication method according to claim 1, wherein the cleaning time for the wafer is 50 seconds or less.

### Claim 3 (depends on 1)

A semiconductor integrated circuit device fabrication method according to claim 1, wherein the ratio of hydrochloric acid to hydrofluoric acid contained in the aqueous solution is: hydrochloric acid: hydrofluoric acid=5 to 1500:1 (by weight ratio).

### Claim 4 (depends on 3)

A semiconductor integrated circuit device fabrication method according to claim 3, wherein the ratio of hydrochloric acid to hydrofluoric acid contained in the aqueous solution is: hydrochloric acid: hydrofluoric acid=5 to 1000:1 (by weight ratio).

### Claim 5 (depends on 4)

A semiconductor integrated circuit device fabrication method according to claim 4, wherein the ratio of hydrochloric acid to hydrofluoric acid contained in the aqueous solution is: hydrochloric acid: hydrofluoric acid=10 to 30:1 (by weight ratio).

### Claim 6 (depends on 1)

A semiconductor integrated circuit device fabrication method according to claim 1 wherein the aqueous solution contains at most 5% by weight of hydrochloric acid, at most 0.2% by weight of hydrofluoric acid and at most 5% by weight of hydrogen peroxide.

### Claim 7 (depends on 1)

A semiconductor integrated circuit device fabrication method according to claim 1, wherein the cleaning temperature for the semiconductor wafer is from 16 to 35° C.

### Claim 8 (depends on 7)

A semiconductor integrated circuit device fabrication method according to claim 7, wherein the cleaning temperature for the semiconductor wafer is from 18 to 28° C.

### Claim 9 (depends on 1)

A semiconductor integrated circuit device fabrication method according to claim 1, wherein the aqueous solution contains at most 3% by weight of hydrochloric acid, at most 0.1% by weight of hydrofluoric acid and at most 3% by weight of hydrogen peroxide.

### Claim 10

A semiconductor integrated circuit device fabrication method, using a wafer having a silicon material region, comprising the steps of:
(a) depositing a metal film over a silicon film over a main surface of a wafer,
(b) patterning the conductive film and,
(c) cleaning the main surface of the wafer at a temperature of 15 to 40° C. by using an aqueous solution containing 0.1 to 15% by weight of hydrochloric acid, 0.01 to 0.3% by weight of hydrofluoric acid and 0.1 to 15% by weight of hydrogen peroxide after the step (b), wherein the cleaning time for the wafer is 2 minutes or less.

### Claim 11 (depends on 10)

A semiconductor integrated circuit device fabrication method according to claim 10, wherein the metal film is a W or Mo film.

### Claim 12 (depends on 10)

A semiconductor integrated circuit device fabrication method according to claim 10, wherein the step of patterning the metal film and the silicon film is a step of forming the gate electrode of an MISFET.

### Claim 13 (depends on 12)

A semiconductor integrated circuit device fabrication method according to claim 12, which further comprises, after the step (c)
(d) cleaning the main surface of the wafer with pure water, and
(e) drying the main surface of the wafer after the step (d).

### Claim 14 (depends on 13)

A semiconductor integrated circuit device fabrication method according to claim 13, which further comprises, after the step (e), the steps of:
(f) forming source and drain of an MISFET to the wafer on both sides of the gate electrode,
(g) forming, after the step (f), an insulation film over the gate electrode,
(h) forming a contact hole for exposing the surface of the source and drain by etching the insulation film,
(i) cleaning the inside of the contact hole by using the aqueous solution of the same composition as that for the aqueous solution described above and
(j) forming, after the step (i), metal wirings electrically connected with the source and drain through the contact hole in the insulation film.

### Claim 15 (depends on 10)

A semiconductor integrated circuit device fabrication method according to claim 10, wherein the aqueous solution contains 0.3 to 5% by weight of hydrochloric acid, 0.02 to 0.2% by weight of hydrofluoric acid and 0.3 to 5% by weight of hydrogen peroxide.

### Claim 16 (depends on 15)

A semiconductor integrated circuit device fabrication method according to claim 15, wherein the aqueous solution contains 0.5 to 3% by weight of hydrochloric acid, 0.03 to 0.1% by weight of hydrofluoric acid and 0.5 to 3% by weight of hydrogen peroxide.

### Claim 17 (depends on 10)

A semiconductor integrated circuit device fabrication method according to claim 10, wherein the ratio of hydrochloric acid to hydrofluoric acid contained in the aqueous solution is hydrochloric acid: hydrofluoric acid=5 to 1500:1 (by weight ratio).

### Claim 18 (depends on 17)

A semiconductor integrated circuit device fabrication method according to claim 17, wherein the ratio of hydrochloric acid to hydrofluoric acid contained in the aqueous solution is hydrochloric acid: hydrofluoric acid=5 to 1000:1 (by weight ratio).

### Claim 19 (depends on 18)

A semiconductor integrated circuit device fabrication method according to claim 18, wherein the ratio of hydrochloric acid to hydrofluoric acid contained in the aqueous solution is hydrochloric acid: hydrofluoric acid=10 to 30:1 (by weight ratio).

### Claim 20 (depends on 10)

A semiconductor integrated circuit device fabrication method according to claim 10, wherein the cleaning temperature for the wafer is from 16 to 35° C.

### Claim 21 (depends on 20)

A semiconductor integrated circuit device fabrication method according to claim 20, wherein the cleaning temperature for the wafer is from 18 to 28° C.

### Claim 22 (depends on 10)