# US 6,727,184 B1 · Method for coating a thick spin-on-glass layer on a semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,184 B1
- Document ID: US6727184B1
- Status: Granted
- Kind: B1
- Application number: 10/283,588
- Filed: 2002-10-29
- Published: 2004-04-29
- Granted: 2004-04-27
- Earliest claimed: 2002-10-29
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Wen-Yi Wang; Hsin-Chieh Huang
- Web page: https://patentgrep.com/patent/US6727184B1

## CPC

- H10P 95/064: {the removal being chemical etching}
- H10W 20/071: {of dielectric parts thereof}
- H10W 20/075: {of multilayered thin functional dielectric layers}
- H10W 20/097: {by thermally treating}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems and with improved planarization is disclosed. In the method, a pre-processed semiconductor structure that has a plurality of metal lines on top is first provided. After a first conformal layer of silicon oxide is deposited on top to insulate the metal lines, a first and a second layer of SOG are coated on top to a total thickness of at least 2500 Å. On top of the second SOG layers, is then deposited a second layer of silicon oxide by a plasma enhanced oxide deposition technique to a thickness of at least 1000 Å. A third and a fourth SOG layer are then coated on top of the stress buffer layer to a total thickness of at least 2500 Å.

## Claims

### Claim 1

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure comprising the steps of:
providing a pre-processed semiconductor structure with a plurality of metal lines formed on top;
depositing conformally a first layer of silicon oxide insulating said metal lines;
coating a first layer of spin-on-glass (SOG) on top of said first layer of silicon oxide;
coating a second layer of SOG on top of said first SOG layer;
annealing said semiconductor structure;
depositing a second layer of silicon oxide on top of said second SOG layer;
coating a third layer of SOG on top of said second layer of silicon oxide;
coating a fourth layer of SOG on top of said third SOG layer; and
etching back said third and fourth layers of SOG to substantially planarize said semiconductor structure.

### Claim 2 (depends on 1)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 1 further comprising the step of depositing said first, said second, said third and said fourth layer of SOG to a thickness of at least 1000 Å.

### Claim 3 (depends on 1)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 1 further comprising the step of depositing said first and second layer of silicon oxide by a plasma enhanced oxide (PEOX) deposition technique.

### Claim 4 (depends on 1)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 1 further comprising the step of coating said first and second layer of SOG to a total thickness of at least 3000 Å.

### Claim 5 (depends on 1)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 1 further comprising the step of coating said third and fourth layer of SOG to a total thickness of at least 3000 Å.

### Claim 6 (depends on 1)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 1 further comprising the step of conducting said annealing process at a first temperature and then at a second temperature higher than said first temperature.

### Claim 7 (depends on 6)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 6 further comprising the step of conducting said annealing process first at a temperature between about 300° C. and about 400° C. and then at a temperature between about 350° C. and about 450° C.

### Claim 8 (depends on 1)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 1 further comprising the step of annealing said semiconductor structure at a temperature of at least 300° C.

### Claim 9 (depends on 1)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 1 further comprising the step of etching back said third and fourth layers of SOG by a reactive ion etching technique.

### Claim 10 (depends on 1)

A method for coating a thick spin-on-glass layer without cracking problems on a semiconductor structure according to claim 1 further comprising the step of depositing said second layer of silicon oxide as a stress buffer layer.

### Claim 11

A method for coating a spin-on-glass layer on a semiconductor structure without cracking problems comprising the steps of:
providing a pre-processed semiconductor structure with a plurality of metal lines formed on top;
depositing conformally a first layer of silicon oxide insulating said metal lines;
coating a first layer of spin-on-glass (SOG) on top of said first layer of silicon oxide;
annealing said semiconductor structure;
depositing a stress buffer layer of an insulating material on top of said first SOG layer;
coating a second layer of SOG on top of said stress buffer layer of insulating material; and
etching back said second layer of SOG to substantially planarize said semiconductor structure.

### Claim 12 (depends on 11)

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems according to claim 11 further comprising the step of depositing a third layer of silicon oxide on top of said second layer of SOG to substantially planarize said semiconductor structure.

### Claim 13 (depends on 11)

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems according to claim 11 further comprising the step of depositing said first and second layer of silicon oxide to a thickness of at least 2500 Å.

### Claim 14 (depends on 11)

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems according to claim 11 further comprising the step of depositing said stress buffer layer of plasma enhanced oxide.

### Claim 15 (depends on 11)

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems according to claim 11 further comprising the step of conducting said annealing process at a first temperature and then at a second temperature higher than said first temperature.

### Claim 16 (depends on 15)

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems according to claim 15 further comprising the step of conducting said annealing process first at a temperature between about 300° C. and about 400° C. and then at a temperature between about 350° C. and about 450° C.

### Claim 17 (depends on 11)

A method for coating a thick spin-on-glass layer on a semiconductor structure according without cracking problems to claim 11 further comprising the step of depositing said stress buffer layer of insulating material to a thickness of at least 2000 Å.

### Claim 18 (depends on 11)

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems according to claim 11 further comprising the step of etching back said second layer of SOG by a reactive ion etching technique.

### Claim 19 (depends on 11)

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems according to claim 11 further comprising the step of depositing said stress buffer layer of silicon nitride.

### Claim 20 (depends on 11)

A method for coating a thick spin-on-glass layer on a semiconductor structure without cracking problems according to claim 11 further comprising the step of depositing said stress buffer layer of silicon oxynitride.