# US 6,727,183 B1 · Prevention of spiking in ultra low dielectric constant material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,183 B1
- Document ID: US6727183B1
- Status: Granted
- Kind: B1
- Application number: 09/915,842
- Filed: 2001-07-27
- Granted: 2004-04-27
- Earliest claimed: 2001-07-27
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Ching-Hui Ma; Jen-Cheng Liu; Li-Chih Chao
- Web page: https://patentgrep.com/patent/US6727183B1

## CPC

- H10W 20/081: {by forming openings in the dielectric parts}
- H10P 50/283: {by chemical means}
- H10W 20/084: {for dual-damascene structures}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A novel etching method for preventing spiking and undercutting of an ultra low-k material layer in damascene metallization is described. A region to be contacted is provided in or on a semiconductor substrate. A liner layer is deposited overlying the region to be contacted. An ultra low-k dielectric layer is deposited overlying the liner layer. A damascene opening is etched through the ultra low-k dielectric layer to the liner layer overlying the region to be contacted wherein this etching comprises a high F/C ratio etch chemistry, high power, and low pressure. The liner layer within the damascene opening is etched away to expose the region to be contacted wherein this etching comprises a high F/C ratio etch chemistry, low power, and low pressure to complete formation of a damascene opening in the fabrication of an integrated circuit device.

## Claims

### Claim 1

A method of forming a damascene opening in the fabrication of an integrated circuit device comprising:
providing a contact region in or on a substrate;
depositing a liner layer overlying said contact region;
depositing a dielectric layer overlying said liner layer wherein all portions of said dielectric layer have a dielectric constant less than 2.5;
first etching said damascene opening through said dielectric layer to said liner layer overlying said contact region wherein said first etching comprises a high F/C ratio etch chemistry, high power, and low pressure; and
second etching said liner layer within said damascene opening to expose said contact region wherein said second etching comprises a high F/C ratio etch chemistry, low power, and low pressure to complete formation of said damascene opening in said fabrication of said integrated circuit device.

### Claim 2 (depends on 1)

The method according to claim 1 wherein said contact region is a gate electrode, a source region, a drain region, or a metal line.

### Claim 3 (depends on 1)

The method according to claim 1 wherein said liner layer is silicon nitride or silicon carbide and has a thickness of between about 300 and 700 Angstroms.

### Claim 4 (depends on 1)

The method according to claim 1 wherein said dielectric layer is Black Diamond or organic dielectric materials and has a thickness of between about 6000 and 10,000 Angstroms.

### Claim 5 (depends on 1)

The method according to claim 1 wherein said high F/C ratio etch chemistry of said first etching comprises CF4 gas flowed at 0 to 150 sccm, O2 gas flowed at 2 to 20 sccm, and Ar gas flowed at 0 to 300 sccm.

### Claim 6 (depends on 1)

The method according to claim 1 wherein said high power of said first etching comprises 700 to 1000 watts.

### Claim 7 (depends on 1)

The method according to claim 1 wherein said low pressure of said first etching comprises between about 80 and 150 mTorr.

### Claim 8 (depends on 1)

The method according to claim 1 wherein said high F/C ratio etch chemistry of said second etching comprises CF4 gas flowed at 0 to 80 sccm and O2 gas flowed at 0 to 50 sccm.

### Claim 9 (depends on 1)

The method according to claim 1 wherein said high F/C ratio etch chemistry of said second etching comprises CHF3 gas flowed at 0 to 80 sccm and O2 gas flowed at 0 to 50 sccm.

### Claim 10 (depends on 1)

The method according to claim 1 wherein said low power of said second etching comprises 250 to 500 watts.

### Claim 11 (depends on 1)

The method according to claim 1 wherein said low pressure of said second etching comprises between about 30 and 70 mTorr.

### Claim 12 (depends on 1)

The method according to claim 1 further comprising:
depositing a barrier metal layer within said damascene opening;
depositing a metal layer overlying said barrier metal layer; and
polishing down said metal layer to leave said metal layer only within said damascene opening.

### Claim 13 (depends on 12)

The method according to claim 12 wherein said metal layer is copper or aluminum-copper alloys.

### Claim 14

A method of forming a damascene opening in the fabrication of an integrated circuit device comprising:
providing a contact region in or on a substrate;
depositing a liner layer overlying said contact region;
depositing a dielectric layer overlying said liner layer wherein said dielectric layer has a dielectric constant of less than 2.5 and wherein no etch stop layer is used within said dielectric layer;
first etching said damascene opening through said dielectric layer to said liner layer overlying said region to be contacted wherein said first etching comprises a high F/C ratio etch chemistry, power of 15 between 700 and 1000 watts, and pressure of between 20 and 150 mTorr and wherein a high polymer gas is not used; and
second etching said liner layer within said damascene opening to expose said region to be contacted wherein said second etching comprises a high F/C ratio etch chemistry, power of between 250 and 500 watts, and pressure of between 30 and 70 mTorr to complete formation of said damascene opening in said fabrication of said integrated circuit device.

### Claim 15 (depends on 14)

The method according to claim 14 wherein said contact region is a gate electrode, a source region, a drain regions, or a metal line.

### Claim 16 (depends on 14)

The method according to claim 14 wherein said liner layer is silicon nitride or silicon carbide and has a thickness of between about 300 and 700 Angstroms.

### Claim 17 (depends on 14)

The method according to claim 14 wherein said dielectric layer is Black Diamond or organic dielectric materials and has a thickness of between about 6000 and 10,000 Angstroms.

### Claim 18 (depends on 14)

The method according to claim 14 wherein said high F/C ratio etch chemistry of said first etching comprises CF4 gas flowed at 0 to 150 sccm, O2 gas flowed at 0 to 20 sccm, and Ar gas flowed at 0 to 300 sccm.

### Claim 19 (depends on 14)

The method according to claim 14 wherein said high F/C ratio etch chemistry of said second etching comprises CF4 gas flowed at 0 to 80 sccm and O2 gas flowed at 0 to 50 sccm.

### Claim 20 (depends on 14)

The method according to claim 14 wherein said high F/C ratio etch chemistry of said second etching comprises CHF3 gas flowed at 0 to 80 sccm and O2 gas flowed at 0 to 50 sccm.

### Claim 21 (depends on 14)

The method according to claim 14 further comprising:
depositing a barrier metal layer within said damascene opening;
depositing a metal layer overlying said barrier metal layer; and
polishing down said metal layer to leave said metal layer only within said damascene opening.

### Claim 22 (depends on 21)

The method according to claim 21 wherein said metal layer is copper or aluminum-copper alloys.

### Claim 23

A method of copper metallization in the fabrication of an integrated circuit device comprising:
providing a contact region in or on a substrate;
depositing a liner layer overlying said contact region;
depositing a dielectric layer overlying said liner layer wherein said dielectric layer has a dielectric constant of less than 2.5;
first etching said damascene opening through said dielectric layer to said liner layer overlying said region to be contacted wherein said first etching comprises a high F/C ratio etch chemistry of CF4, O2, and Ar gases, power of between 700 and 1000 watts, and pressure of between 20 and 150 mTorr and wherein a high polymer gas comprising C4F8, CH2F2, C2F2, or C2F6 is not used;
second etching said liner layer within said damascene opening to expose said region to be contacted wherein said second etching comprises a high F/C ratio etch chemistry, power of between 250 and 500 watts, and pressure of between 30 and 70 mTorr,
depositing a barrier metal layer within said damascene opening;
depositing a copper layer overlying said barrier metal layer; and
polishing down said copper layer and said barrier metal layer to leave said barrier metal layer and said copper layer only within said damascene opening to complete said copper metallization in said fabrication of said integrated circuit device.

### Claim 24 (depends on 23)

The method according to claim 23 wherein said contact region is a gate electrode, a source region, a drain regions, or a metal line.

### Claim 25 (depends on 23)

The method according to claim 23 wherein said liner layer is silicon nitride or silicon carbide and has a thickness of between about 300 and 700 Angstroms.

### Claim 26 (depends on 23)

The method according to claim 23 wherein said dielectric layer is Black Diamond or organic dielectric materials and has a thickness of between about 6000 and 10,000 Angstroms.

### Claim 27 (depends on 23)

The method according to claim 23 wherein said high F/C ratio etch chemistry of said first etching comprises CF4 gas flowed at 0 to 150 sccm, O2 gas flowed at 0 to 20 sccm, and Ar gas flowed at 0 to 300 sccm.

### Claim 28 (depends on 23)

The method according to claim 23 wherein said high F/C ratio etch chemistry of said second etching comprises CF4 gas flowed at 0 to 80 sccm and O2 gas flowed at 0 to 50 sccm.

### Claim 29 (depends on 23)

The method according to claim 23 wherein said high F/C ratio etch chemistry of said second etching comprises CHF3 gas flowed at 0 to 80 sccm and O2 gas flowed at 0 to 50 sccm.