# US 6,727,180 B2 · Method for forming contact window

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,180 B2
- Document ID: US6727180B2
- Status: Granted
- Kind: B2
- Application number: 09/839,365
- Filed: 2001-04-23
- Published: 2001-11-29
- Granted: 2004-04-27
- Earliest claimed: 1999-02-06
- Assignees: United Microelectronics Corp.
- Inventors: Chien-Li Kuo; Wei-Wu Liao
- Web page: https://patentgrep.com/patent/US6727180B2

## CPC

- H10W 20/082: {the openings being tapered via holes}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming contact window is disclosed. Essential concept of the invention comprises over coating layer formed over surface before forming contact window is formed and the etching rate of over coating layer is higher than etching rate of underlying layer. The method comprises following steps: First, forming semiconductor structures on surface of wafer. Second, forming a coating layer over the surface and covering these semiconductor structures. Third, forming an over coating layer on the coating layer, where etching rate of over coating layer is higher than etching rate of coating layer. Finally, form contact window with outwardly winded shape. Thus, contact window formed by the invention is more convenient for filling material than contact window formed by conventional method. In addition, because width of contact window is not obviously increased, this invention is more beneficial for deep-submicron fabrication.

## Claims

### Claim 1

A method for forming a contact window, said method comprise:
forming a plurality of semiconductor structures on a wafer;
forming a coating layer over the surface of said wafer, where the thickness of said coating layer is not less than the heights of said semiconductor structures;
forming an over coating layer over said coating layer, wherein the etching rate of said over coating layer is higher than the etching rate of said coating layer; and
forming said contact window in both said over coating layer and said coating layer by a single isotropic etching process, wherein upper part of said contact window is outwardly widened.

### Claim 2 (depends on 1)

The method of claim 1, wherein the lateral etching rate of said over coating layer is higher than the lateral etching rate of said coating layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein upper part of said contact window is outwardly oblique.

### Claim 4 (depends on 1)

The method of claim 1, wherein upper part of said contact window is outwardly crooked.

### Claim 5 (depends on 1)

The method of claim 1, wherein upper part of said contact window is outwardly smooth.

### Claim 6 (depends on 1)

The method of claim 1, wherein an opening of said contact window locates on top surface of said over coating layer and said contact window lands on said semiconductor structures.

### Claim 7 (depends on 1)

The method of claim 1, wherein an opening of said contact window locates on top surface of said over coating layer and said contact window lands on said wafer.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said semiconductor structures comprises gate, electrode of capacitor, isolation layer and multilevel interconnects.

### Claim 9 (depends on 1)

The method according to claim 1, wherein said coating layer comprises dielectric layer.

### Claim 10 (depends on 1)

The method according to claim 1, wherein material of said over coating layer is chosen from the group consisting of following: oxide and dielectric.

### Claim 11

A method for forming a metal plug, said method comprising:
forming a dielectric layer over a wafer;
planarizing the surface of said dielectric layer by a chemical mechanical polishing;
forming an oxide layer over said dielectric layer, where said oxide layer filling a plurality of polishing scars and said oxide layer having an etching rate which is higher than an etching rate of said dielectric layer;
forming a contact window in both said oxide layer and said dielectric layer by a single isotropic etching process, wherein upper part of said contact window is outwardly widen; and
filling a metal in said contact window.

### Claim 12 (depends on 11)

The method of claim 11, wherein upper part of said contact window is outwardly oblique.

### Claim 13 (depends on 11)

The method of claim 11, wherein upper part of said contact window is outwardly crooked.

### Claim 14 (depends on 11)

The method of claim 11, wherein upper part of said contact window is outwardly smooth.

### Claim 15 (depends on 11)

The method of claim 11, wherein an opening of said contact window locates on top surface of said oxide layer and said contact window lands on said wafer.

### Claim 16 (depends on 11)

The method according to claim 11, wherein said dielectric layer is an annealing oxide layer, said annealing is formed in about 800° C. and then etching rate of said annealing oxide layer is higher then said oxide layer.