# US 6,727,176 B2 · Method of forming reliable Cu interconnects

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,176 B2
- Document ID: US6727176B2
- Status: Granted
- Kind: B2
- Application number: 09/986,267
- Filed: 2001-11-08
- Published: 2003-05-08
- Granted: 2004-04-27
- Earliest claimed: 2001-11-08
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Minh Van Ngo; Arvind Halliyal; Eric Paton
- Web page: https://patentgrep.com/patent/US6727176B2

## CPC

- H10W 20/059: {by reflowing or applying pressure}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Reliable Cu interconnects are formed by filling an opening in a dielectric layer with Cu and then laser thermal annealing in NH3 to reduce copper oxide and to reflow the deposited Cu, thereby eliminating voids and reducing contact resistance. Embodiments include laser thermal annealing employing an NH3 flow rate of about 200 to about 2,000 sccn.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, the method comprising:
forming an opening in a dielectric layer;
depositing copper (Cu) or a Cu alloy to fill the opening; and
laser thermal annealing the deposited Cu or Cu alloy in ammonia (NH3) to reflow the deposited Cu or Cu alloy.

### Claim 2 (depends on 1)

The method according to claim 1, comprising laser thermal annealing by impinging a pulsed laser light beam on the deposited Cu or Cu alloy at a radiant fluence of about 0.28 to about 0.34 joules/cm2.

### Claim 3 (depends on 2)

The method according to claim 2, comprising laser thermal annealing to heat the deposited Cu or Cu alloy to a temperature of about 983° C. to about 1183° C., thereby reflowing the deposited Cu or Cu alloy.

### Claim 4 (depends on 1)

The method according to claim 1, comprising laser thermal annealing employing an NH3 flow rate of about 200 to about 2,000 sccm.

### Claim 5 (depends on 1)

The method according to claim 1, comprising depositing a barrier layer lining the opening before depositing the Cu or Cu alloy.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the barrier layer is a composite comprising a tantalum nitride layer on the dielectric layer, a layer of alpha-tantalum (α-Ta) on the tantalum nitride layer.

### Claim 7 (depends on 5)

The method according to claim 5, comprising depositing a seedlayer on the barrier layer.

### Claim 8 (depends on 7)

The method according to claim 7, comprising depositing the Cu or Cu alloy by electroless plating or electroplating.

### Claim 9 (depends on 6)

The method according to claim 6, comprising conducting chemical mechanical polishing (CMP) such that an upper surface of the deposited Cu or Cu alloy is substantially co-planar with an upper surface of the dielectric layer.

### Claim 10 (depends on 9)

The method according to claim 9, comprising:
treating the upper surface of the Cu or Cu alloy in a plasma containing NH3 to remove copper oxide therefrom; and
depositing a silicon nitride capping layer on the plasma treated surface by plasma enhanced chemical vapor deposition.

### Claim 11 (depends on 1)

The method according to claim 1, comprising conducting chemical mechanical polishing (CMP) such that an upper surface of the deposited Cu or Cu alloy is substantially co-planar with an upper surface of the dielectric layer.

### Claim 12 (depends on 11)

The method according to claim 11, comprising:
treating the upper surface of the Cu or Cu alloy in a plasma containing NH3 to remove copper oxide therefrom; and
depositing a silicon nitride capping layer on the plasma treated surface by plasma enhanced chemical vapor deposition.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the opening is a dual damascene opening containing a lower via hole section in communication with an upper trench section, the method comprising depositing the Cu or Cu alloy to fill the opening to form an upper line in communication with an underlying via.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the dielectric layer comprises an oxide.

### Claim 15 (depends on 14)

The method according to claim 14, where the oxide is a fluorine-containing silicon oxide derived from fluorine-doped tetraethyl orthosilicate.