# US 6,727,173 B2 · Semiconductor processing methods of forming an utilizing antireflective material layers, and methods of forming transistor gate stacks

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,173 B2
- Document ID: US6727173B2
- Status: Granted
- Kind: B2
- Application number: 09/891,570
- Filed: 2001-06-25
- Published: 2001-11-22
- Granted: 2004-04-27
- Earliest claimed: 1998-09-03
- Assignees: Micron Technology, Inc.
- Inventors: Gurtej S. Sandhu; Sujit Sharan
- Web page: https://patentgrep.com/patent/US6727173B2

## CPC

- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- H10D 64/01326: {Aspects related to lithography, isolation or planarisation of the conductor}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 76/2043: {using an anti-reflective coating}
- H10P 76/2045: {Electron beam lithography processes}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

In one aspect, the invention includes a semiconductor processing method comprising exposing silicon, nitrogen and oxygen in gaseous form to a high density plasma during deposition of a silicon, nitrogen and oxygen containing solid layer over a substrate. In another aspect, the invention includes a gate stack forming method, comprising: a) forming a polysilicon layer over a substrate; b) forming a metal silicide layer over the polysilicon layer; c) depositing an antireflective material layer over the metal silicide utilizing a high density plasma; d) forming a layer of photoresist over the antireflective material layer; e) photolithographically patterning the layer of photoresist to form a patterned masking layer from the layer of photoresist; and f) transferring a pattern from the patterned masking layer to the antireflective material layer, metal silicide layer and polysilicon layer to pattern the antireflective material layer, metal silicide layer and polysilicon layer into a gate stack.

## Claims

### Claim 1

A semiconductor processing method comprising:
depositing a material comprising Si, N and O over a substrate utilizing a feed gas comprising SiH4, N2 and O2;
exposing the material to a high density plasma during the depositing;
forming a layer of photoresist over the material;
photolithographically patterning the layer of photoresist; and
wherein the deposition occurs at first temperature; further comprising exposing the material to a second temperature higher than the first temperature after the exposure of the material to the high density plasma; and wherein “n” and “k” values of the material change by less than 10% during the exposing to the second temperature.

### Claim 2 (depends on 1)

The method of claim 1 wherein the second temperature is greater than 800° C.

### Claim 3 (depends on 1)

The method of claim 1 wherein the second temperature is greater than 850° C.

### Claim 4

A semiconductor processing method comprising:
depositing a material comprising Si, N and O over a substrate utilizing a feed gas comprising SiH4, N2 and O2;
exposing the material to a high density plasma during the depositing;
forming a layer of photoresist over the material;
photolithographically patterning the layer of photoresist; and
maintaining at least a portion of the substrate at a temperature of from about 300° C. to about 800° C. during the depositing.

### Claim 5

A semiconductor processing method comprising:
depositing a material comprising Si, N and O over a substrate utilizing a feed gas comprising SiH4, N2 and O2;
exposing the material to a high density plasma during the depositing;
forming a layer of photoresist over the material;
photolithographically patterning the layer of photoresist;
wherein the depositing occurs in a reactor: and
wherein a temperature within the reactor during the depositing is from about 300° C. to about 800° C.

### Claim 6

A semiconductor processing method comprising:
depositing a material comprising Si, N and O over a substrate utilizing a feed gas comprising SiH4, N2 and O2;
exposing the material to a high density plasma during the depositing;
forming a layer of photoresist over the material;
photolithographically patterning the layer of photoresist;
wherein the depositing occurs in a reactor; and
wherein a pressure within the reactor during the depositing is from about 1 mTorr to about 100 mTorr.

### Claim 7

A semiconductor processing method comprising:
depositing a material comprising Si, N and O over a substrate utilizing a feed gas comprising SiH4, N2 and O2;
exposing the material to a high density plasma during the depositing;
forming a layer of photoresist over the material;
photolithographically patterning the layer of photoresist;
wherein the depositing occurs in a reactor;
wherein the substrate is biased to a power of about 100 watts during the depositing; and
wherein the plasma is induced at a power of about 2000 watts.

### Claim 8

A semiconductor processing method comprising:
depositing a material comprising Si, N and O over a substrate utilizing a feed gas comprising SiH4, N2 and O2;
exposing the material to a high density plasma during the depositing;
forming a layer of photoresist over the material;
photolithographically patterning the layer of photoresist;
wherein the depositing occurs in a reactor;
wherein a temperature within the reactor during the depositing is from about 300° C. to about 800° C.; and
wherein a pressure within the reactor during the depositing is from about 1 mTorr to about 100 mTorr.

### Claim 9

A material comprising silicon, nitrogen and oxygen, and having “n” and “k” values which change by less than 10% during exposure of the material to a temperature of at least about 850° C.

### Claim 10 (depends on 9)

The material of claim 9 formed over metal silicide.

### Claim 11 (depends on 9)

The material of claim 9 formed over and physically against metal silicide.

### Claim 12 (depends on 9)

The material of claim 9 formed on metal silicide, and wherein the metal silicide is over a monocrystalline silicon substrate.

### Claim 13 (depends on 9)

The material of claim 9 wherein the temperature is comprised by anneal conditions which include an exposure time to the temperature of at least about 30 minutes.

### Claim 14 (depends on 9)

The material of claim 9 wherein the temperature is comprised by anneal conditions which include a pressure of at least about 1 atmosphere and an exposure time to the temperature of at least about 30 minutes.

### Claim 15

A semiconductor processing method comprising:
forming a layer comprising silicon, nitrogen and oxygen; the layer being characterized by an “n” value and a “k” value;
exposing the deposited layer to a temperature of at least about 850° C.; and
the “n” and “k” values change by less than 10% during exposure to the temperature conditions.

### Claim 16 (depends on 15)

The method of claim 15 comprising exposing the layer to a high density plasma prior to exposing the layer to the temperature.

### Claim 17 (depends on 15)

The method of claim 15 wherein the duration of the exposure to the temperature is at least bout 30 minutes.

### Claim 18

A semiconductor processing method comprising:
forming a metal silicide layer over a monocrystalline silicon substrate;
depositing an antireflective material layer over the metal silicide layer;
exposing the antireflective material layer to a high density plasma during the depositing;
forming a layer of photoresist over the antireflective material layer;
photolithographically patterning the layer of photoresist; and
while the antireflective material layer is over the metal silicide layer, annealing the metal silicide layer.