# US 6,727,165 B1 · Fabrication of metal contacts for deep-submicron technologies

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,165 B1
- Document ID: US6727165B1
- Status: Granted
- Kind: B1
- Application number: 09/967,074
- Filed: 2001-09-28
- Granted: 2004-04-27
- Earliest claimed: 2001-09-28
- Assignees: LSI Logic Corporation
- Inventors: Helmut Puchner; Ming-Yi Lee
- Web page: https://patentgrep.com/patent/US6727165B1

## CPC

- H10P 14/44: Physical vapour deposition [PVD]
- H10D 64/0112: {using conductive layers comprising silicides}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Provided is a process for forming a semiconductor device having salicided contacts. A concentration of metal is formed at the substrate surface by exposing the substrate to a metal plasma. The concentration of metal is then annealed to produce a salicided contact. In a separate embodiment, the metallization plasma and salicide anneal occur in-situ in one process step.

## Claims

### Claim 1

A method of forming a semiconductor device having salicided contacts, the method comprising:
implanting a concentration of metal in a subsurface region of a substrate of a partially formed semiconductor device by exposing the substrate to a metal plasma; and
forming salicided contacts by annealing the concentration of metal in the subsurface region of the partially formed semiconductor device.

### Claim 2 (depends on 1)

The method as recited in claim 1 further comprising forming a barrier cap film on the formed concentration of metal.

### Claim 3 (depends on 2)

The method as recited in claim 2 wherein the barrier cap film comprises one of TiN and Ti.

### Claim 4 (depends on 1)

The method as recited in claim 1 wherein the annealing step is a Rapid Thermal Anneal process step.

### Claim 5 (depends on 2)

The method as recited in claim 2 wherein the barrier cap film is formed using plasma doping equipment.

### Claim 6 (depends on 1)

The method as recited in claim 1 wherein a flux of the metal plasma is adjustery at least one of DC power, RF power, pressure, and wafer bias.

### Claim 7 (depends on 1)

The method as recited in claim 1 wherein the wafer bias is adjusted so that silicon is not sputtered from the substrate to a source generating the metal plasma.

### Claim 8 (depends on 1)

The method as recited in claim 1 wherein the metal plasma comprises Titanium and the flux is about 6*1015 atoms*cm−2*sec−1.

### Claim 9 (depends on 1)

The method as recited in claim 1 wherein the metal plasma comprises Cobalt and the flux is about 1*1015 atoms*cm−2*sec−1.

### Claim 10 (depends on 1)

The method as recited in claim 1 wherein the annealing the concentration of metal in the subsurface region of the partially formed semiconductor device is an in-situ annealing step occurring simultaneously with the step of the exposing the substrate with a metal plasma.

### Claim 11 (depends on 10)

The method as recited in claim 10 wherein the salicided contact formed is NiSi and the in-situ annealing step comprises heating the wafer to a temperature in the range of 250° C. to 650° C.

### Claim 12 (depends on 10)

The method as recited in claim 10 wherein the salicided contact formed is CoSi2 and the in-situ annealing step comprises heating the wafer to a temperature in the range of 500° C. to 850° C.

### Claim 13 (depends on 10)

The method as recited in claim 10 wherein the salicided contact formed is TiSi2 and the in-situ annealing step comprises heating the wafer to a temperature in the range of 750° C. to 950° C.

### Claim 14

A method of forming a semiconductor device having salicided contacts the method comprising:
implanting a concentration of metal in a subsurface region of a substrate of a partially formed semiconductor device by exposing the substrate to a metal plasma; and
forming salicided contacts in-situ by simultaneously annealing the concentration of metal as the metal is implanted in the subsurface region of the substrate of the partially formed semiconductor device.

### Claim 15 (depends on 14)

The method as recited in claim 14 wherein the annealing of the concentration of metal simultaneously with implanting the concentration of metal comprises heating a chuck holding a wafer containing the semiconductor device.

### Claim 16 (depends on 1)

The method as recited in claim 1 wherein the wafer bias is adjusted so that the implanted concentration of metal extends below the depth of substrate surface nonuniformities.

### Claim 17 (depends on 1)

The method as recited in claim 1 wherein the implanted concentration of metal is approximately 1 nm in thickness.

### Claim 18 (depends on 1)

The method as recited in claim 1 wherein the implanted concentration of metal extends to a depth of at least 1 nm below the surface of the substrate.

### Claim 19 (depends on 1)

The method as recited in claim 1 wherein the wafer bias is adjusted to be approximately 5 watts.

### Claim 20 (depends on 14)

The method as recited in claim 14 wherein the wafer bias is adjusted so that the implanted concentration of metal extends below the depth of substrate surface nonuniformities.

### Claim 21 (depends on 14)

The method as recited in claim 14 wherein the implanted concentration of metal extends to a depth of at least 1 nm below the surface of the substrate.

### Claim 22 (depends on 14)

The method as recited in claim 14 wherein the metal plasma has a DC power level in the range of 1 to 10 kw, an RF power level of about 1 to 10 kw, and a wafer bias of 0 to 20 watts.