# US 6,727,164 B2 · Method for fabricating a semiconducting nitride film, susceptor tray, and apparatus for fabricating a semiconducting nitride film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,164 B2
- Document ID: US6727164B2
- Status: Granted
- Kind: B2
- Application number: 10/060,802
- Filed: 2002-01-30
- Published: 2002-08-29
- Granted: 2004-04-27
- Earliest claimed: 2001-02-02
- Assignees: NGK Insulators, Ltd.
- Inventors: Tomohiko Shibata; Yukinori Nakamura; Mitsuhiro Tanaka; Keiichiro Asai
- Web page: https://patentgrep.com/patent/US6727164B2

## CPC

- C23C 16/4401: {Means for minimising impurities, e.g. dust, moisture or residual gas, in the reaction chamber}
- C23C 16/4583: {the substrate being supported substantially horizontally}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

In fabricating a semiconducting nitride film by a MOCVD method, a susceptor tray is employed. The susceptor tray is constructed of a base plate and an outer member detachable from the base plate. A substrate for the film to be formed upon is set in a recessed portion formed by disposing the outer member on the base plate.

## Claims

### Claim 1

A method for fabricating a semiconducting nitride film, comprising the steps of:
preparing a susceptor tray comprising an outer member and a base plate, said outer member being disposed on said base plate to form a recessed portion, wherein said outer member is detachable and has an annular shape;
setting a substrate in said recessed portion; and
fabricating said semiconducting nitride film on said substrate;
wherein substantially no space is provided between an inner peripheral portion of said outer member and an outer peripheral portion of said substrate in said recessed portion.

### Claim 2 (depends on 1)

The fabricating method of claim 1, wherein said outer member comprises an optically transparent material having an average optical absorption rate of 0.1 cm−1 or below within a wavelength range of 400-700 nm.

### Claim 3 (depends on 1)

The fabricating method of claim 1, wherein said semiconducting nitride film includes elemental Al.

### Claim 4 (depends on 3)

The fabricating method of claim 3, wherein the Al content of said semiconducting nitride film is 50 atomic percent or over.

### Claim 5 (depends on 4)

The fabricating method of claim 4, wherein said semiconducting nitride film comprises AlN.

### Claim 6 (depends on 3)

The fabricating method of claim 3, wherein said semiconducting nitride film is fabricated at 1100° C. or over by a CVD method.

### Claim 7 (depends on 1)

The fabricating method of claim 1, wherein said semiconducting nitride film is fabricated under a depressurized atmosphere by a CVD method.