# US 6,727,163 B2 · Method for sawing wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,163 B2
- Document ID: US6727163B2
- Status: Granted
- Kind: B2
- Application number: 10/366,299
- Filed: 2003-02-12
- Published: 2003-08-28
- Granted: 2004-04-27
- Earliest claimed: 2002-02-25
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Dae Young Kim; Geun Ho Song
- Web page: https://patentgrep.com/patent/US6727163B2

## CPC

- H10P 72/74: {using temporarily an auxiliary support}
- H10P 54/00: Cutting or separating of wafers, substrates or parts of devices
- H10P 72/7402: {Wafer tapes, e.g. grinding or dicing support tapes}
- H10P 72/0442: {Apparatus for placing on an insulating substrate, e.g. tape}
- H10P 72/7416: {used during dicing or grinding}
- H10P 72/7422: {used to protect an active side of a device or wafer}
- Y10S 438/976: Temporary protective layer
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for sawing a wafer having a large number of semiconductor devices, e.g., image sensor devices is provided. In one embodiment, a protective layer covers micro-lenses of the image sensor devices to protect the lenses from being damaged or polluted by, for example, silicon dust during wafer sawing. The silicon dust remaining in a gap between the devices is removed together with an adhesive tape on the backside surface of the wafer. Accordingly, the silicon dust cannot affect the micro-lenses during the wafer sawing process or subsequent die-attach, so that image defects caused by the silicon dust can be reduced and the yield of the image sensor devices is increased.

## Claims

### Claim 1

A method for sawing a wafer, the method comprising:
providing a wafer having a plurality of image sensor devices on an active surface thereof, each device having a plurality of micro-lenses formed thereon;
forming a protective layer on the active surface of the wafer, the protective layer covering the micro-lenses;
attaching a first adhesive tape to a backside surface of the wafer;
dicing the wafer into individual image sensor devices;
attaching a second adhesive tape to the protective layer; and
stripping the first adhesive tape from the backside surface of the wafer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
attaching a third adhesive tape to the backside surface of the wafer;
stripping the second adhesive tape from the active surface of the wafer; and
removing the protective layer from the active surface of the wafer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the protective layer is formed of resin material.

### Claim 4 (depends on 3)

The method of claim 3, wherein the resin material comprises a novolak-based resist.

### Claim 5 (depends on 1)

The method of claim 1, wherein removing the protective layer comprises using an organic solvent.

### Claim 6 (depends on 5)

The method of claim 5, wherein the organic solvent is selected from the group consisting of isopropyl alcohol, methanol and ethanol.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
attaching a device that separates the first tape from the second tape to the first adhesive tape before the attaching the second adhesive tape.

### Claim 8 (depends on 7)

The method of claim 7, wherein the device surrounds a periphery of the wafer.

### Claim 9 (depends on 7)

The method of claim 7, wherein the device is a ring frame.

### Claim 10 (depends on 1)

The method of claim 1, wherein each of the first, second and third adhesive tapes is a normal-type tape having an adhesive strength of 120±30 g/20 mm.

### Claim 11 (depends on 1)

The method of claim 1, wherein each of the first, second and third adhesive tapes is an ultraviolet tape having an adhesive strength of 300˜500 g/20 mm.

### Claim 12 (depends on 1)

The method of claim 1, wherein the protective layer is selectively formed such that scribe lines of the wafer are exposed.

### Claim 13 (depends on 1)

The method of claim 1, wherein the image sensor device is a charge-coupled device.

### Claim 14

A method for sawing a wafer, the method comprising:
forming a protective layer on an active surface of a wafer having a plurality of semiconductor devices;
attaching a first adhesive tape to a backside surface of the wafer;
dicing the wafer into individual semiconductor devices;
attaching a second adhesive tape to the protective layer; and
stripping the first adhesive tape from the backside surface of the wafer.

### Claim 15 (depends on 14)

The method of claim 14, further comprising:
attaching a third adhesive tape to the backside surface of the wafer;
stripping the second adhesive tape from the active surface of the wafer; and
removing the protective layer from the active surface of the wafer.

### Claim 16 (depends on 14)

The method of claim 14, further comprising:
attaching a device that separates the first tape and the second tape to the first adhesive tape before attaching the second adhesive tape.