# US 6,727,160 B1 · Method of forming a shallow trench isolation structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,160 B1
- Document ID: US6727160B1
- Status: Granted
- Kind: B1
- Application number: 10/270,348
- Filed: 2002-10-15
- Published: 2004-04-15
- Granted: 2004-04-27
- Earliest claimed: 2002-10-15
- Assignees: Silicon Integrated Systems Corp.
- Inventors: Chian-Kai Huang; Fung-Hsu Cheng; Jui-Ping Li
- Web page: https://patentgrep.com/patent/US6727160B1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming a STI structure. First, a substrate having a trench is provided. Next, a conformable silicon oxide layer is grown on the surface of the trench by wet oxidation using single wafer process to serve as a liner oxide layer. Thereafter, the substrate and the silicon oxide layer is in-situ annealed. Finally, an insulating layer is completely filled into the trench.

## Claims

### Claim 1

A method of forming a shallow trench isolation structure, comprising the steps of:
providing a substrate having a trench;
growing a conformable silicon oxide layer on the surface of the trench by wet oxidation using single wafer process to serve as a liner oxide layer; wherein the wet oxidation is performed using hydrogen and oxygen as reaction gases and wherein the flow rates of the hydrogen and oxygen are about 10˜16 slm and 5˜8 slm, respectively
in-situ annealing the substrate and the silicon oxide layer; and
filling an insulating layer into the trench.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the silicon oxide layer thickness of about 150˜250 Å.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the silicon oxide layer is grown at about 1100˜1200° C.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the annealing is performed in an atmosphere of nitrogen or nitrous oxide.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the annealing is performed for 20˜60 sec.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the annealing is performed at about 1100˜1200° C.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the insulating layer is high density plasma oxide.

### Claim 8

A method of forming a shallow trench isolation structure, comprising the steps of:
providing a substrate covered by a mask layer;
etching the mask layer to form a least one opening to expose the substrate;
etching the substrate under the opening to form a trench in the substrate;
growing a conformable silicon oxide layer on the surface of the trench at a predetermined temperature by wet oxidation using single wafer process to serve as a liner oxide layer; wherein the wet oxidation is performed using hydrogen and oxygen as reaction gases and wherein the flow rates of the hydrogen and oxygen are about 10˜16 slm and 5˜8 slm, respectively
in-situ annealing the substrate and the silicon oxide layer at the predetermined temperature;
forming an insulating layer over the mask layer and filling in the trench;
removing the insulating layer over the mask layer; and
removing the mask layer.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein the silicon oxide layer has a thickness of about 150˜250 Å.

### Claim 10 (depends on 8)

The method as claimed in claim 8, wherein the predetermined temperature is at about 1100˜1200° C.

### Claim 11 (depends on 8)

The method as claimed in claim 8, wherein the annealing is performed in an atmosphere of nitrogen or nitrous oxide.

### Claim 12 (depends on 8)

The method as claimed in claim 8, wherein the annealing is performed for 20˜60 sec.

### Claim 13 (depends on 8)

The method as claimed in claim 8, wherein the insulating layer is high density plasma oxide.

### Claim 14 (depends on 8)

The method as claimed in claim 8, wherein the insulating layer over the mask layer is removed by chemical mechanic polishing.