# US 6,727,159 B2 · Method of forming a shallow trench isolation in a semiconductor substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,159 B2
- Document ID: US6727159B2
- Status: Granted
- Kind: B2
- Application number: 10/163,239
- Filed: 2002-06-04
- Published: 2003-07-31
- Granted: 2004-04-27
- Earliest claimed: 2002-01-28
- Assignees: Nanya Technology Corporation
- Inventors: Yi-Nan Chen; Hsien-Wen Liu; Kaan-Lu Tzou
- Web page: https://patentgrep.com/patent/US6727159B2

## CPC

- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6506: {Formation of intermediate materials}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming a shallow trench isolation in a semiconductor substrate. First, a hard mask consisting of a pad nitride and a pad oxide is formed on the semiconductor substrate. The semiconductor substrate is anisotrpically etched to form a trench while the hard mask is used as the etching mask. A thermal oxide film is grown on the trench. Then, a nitride liner is formed on the thermal oxide film. Next, a silicon rich oxide layer is conformally deposited on the nitride liner by high density plasma chemical vapor deposition without a bias voltage applied to the semiconductor substrate. Then, a silicon oxide is deposited to fill the trench by high density plasma chemical vapor deposition while a bias voltage is applied to the semiconductor substrate.

## Claims

### Claim 1

A method of forming a shallow trench isolation in a semiconductor substrate, comprising the steps of:
(a) forming a hard mask consisting of a pad nitride and a pad oxide on the semiconductor substrate;
(b) etching the semiconductor substrate to form a trench while the hard mask is used as the etching mask;
(c) forming a thermal oxide film on the trench;
(d) forming a nitride liner on the thermal oxide film;
(e) conformally depositing a silicon rich oxide layer on the nitride liner by high density plasma chemical vapor deposition without a bias voltage applied to the semiconductor substrate; and
(f) forming a silicon oxide to fill the trench by high density plasma chemical vapor deposition while a bias voltage is applied to the semiconductor substrate.

### Claim 2 (depends on 1)

The method of forming a shallow trench isolation in a semiconductor substrate as claimed in claim 1, wherein the deposition gas in step (e) includes a mixture gas of silane and oxygen having a flow ratio of about 1:1.

### Claim 3 (depends on 1)

The method of forming a shallow trench isolation in a semiconductor substrate as claimed in claim 1, wherein the deposition gas in step (f) includes a mixture gas of silane and oxygen having a flow ratio of about 1:1 to 1:2.

### Claim 4 (depends on 1)

The method of forming a shallow trench isolation in a semiconductor substrate as claimed in claim 1, wherein the silicon rich oxide layer has a hydrofluoric acid selectivity of about 1 relative to the silicon oxide layer.

### Claim 5 (depends on 1)

The method of forming a shallow trench isolation in a semiconductor substrate as claimed in claim 1, wherein the silicon rich oxide layer has a hydrofluoric acid selectivity less than 1 relative to the silicon oxide layer.

### Claim 6 (depends on 1)

The method of forming a shallow trench isolation in a semiconductor substrate as claimed in claim 1, further comprising the steps of:
planarizing the silicon rich oxide layer and the silicon oxide layer by chemical mechanical polishing while the hard mask is used as the polishing stop layer; and
removing residual oxide above the hard mask by hydrofluoric acid.

### Claim 7 (depends on 1)

The method of forming a shallow trench isolation in a semiconductor substrate as claimed in claim 1, wherein the nitride liner is a silicon nitride film formed by chemical vapor deposition.