# US 6,727,157 B2 · Method for forming a shallow trench isolation using air gap

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,157 B2
- Document ID: US6727157B2
- Status: Granted
- Kind: B2
- Application number: 10/657,082
- Filed: 2003-09-09
- Published: 2004-03-11
- Granted: 2004-04-27
- Earliest claimed: 2002-09-09
- Assignees: Anam Semiconductor Inc.
- Inventors: Young Hun Seo
- Web page: https://patentgrep.com/patent/US6727157B2

## CPC

- H10W 10/20: Air gaps
- H10W 10/0142: {the dielectric materials being chemical transformed from non-dielectric materials}
- H10W 10/0143: {comprising concurrently refilling multiple trenches having different shapes or dimensions}
- H10W 10/021: {of air gaps}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In fabricating a shallow trench isolation (STI), a silicon oxide layer, a silicon nitride layer and a moat pattern is sequentially deposited on a silicon substrate. Next, the silicon nitride layer and the silicon oxide layer is etched using the moat pattern as a mask to thereby partially expose the silicon substrate and then the moat pattern is removed. Ion implanting process is performed into the silicon substrate using the silicon nitride layer as a mask, adjusting a dose of an implanted ion and an implant energy, to thereby form an isolation region. And then, the isolation region to form a porous silicon and to form an air gap in the porous silicon is anodized, wherein a porosity of the porous silicon is determined by the dose of the implanted ion. Next, the porous silicon is oxidized through an oxidation process. Finally, the silicon nitride layer is removed.

## Claims

### Claim 1

A method for fabricating a shallow trench isolation, comprising the steps of:
sequentially depositing a silicon oxide layer, a silicon nitride layer and a moat pattern on a silicon substrate;
etching the silicon nitride layer and the silicon oxide layer using the moat pattern as a mask to thereby partially expose the silicon substrate and then removing the moat pattern;
performing ion implanting process into the silicon substrate using the silicon nitride layer as a mask, adjusting a dose of an implanted ion and an implant energy, to thereby form an isolation region;
anodizing the isolation region to form a porous silicon and to form an air gap in the porous silicon, wherein a porosity of the porous silicon is determined by the dose of the implanted ion;
oxidizing the porous silicon through an oxidation process; and
removing the silicon nitride layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the etching step includes the steps of etching the silicon nitride layer with a slope or inserting an additional sidewall nitride layer process into the STI process to form a space smaller than the moat pattern.

### Claim 3 (depends on 1)

The method of claim 1, wherein the ion implanting process is iteratively performed using different ion implant conditions to thereby form the isolation region having a stepwise ion concentration.

### Claim 4 (depends on 1)

The method of claim 1, wherein the ion implanting process is performed with N-type material.

### Claim 5 (depends on 1)

The method of claim 1, wherein the ion implanting process is performed with P-type material.

### Claim 6 (depends on 1)

The method of claim 1, wherein a porosity and a thickness of the porous silicon is controlled by adjusting a reaction time in anodic oxidation.

### Claim 7 (depends on 1)

The method of claim 1, wherein a porosity and a thickness of the porous silicon is controlled by adjusting a current density in anodic oxidation.

### Claim 8 (depends on 1)

The method of claim 1, wherein a porosity and a thickness of the porous silicon is controlled by adjusting hydrofluoric (HF) concentration in anodic oxidation.