# US 6,727,155 B1 · Method for spin etching sidewall spacers by acid vapor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,155 B1
- Document ID: US6727155B1
- Status: Granted
- Kind: B1
- Application number: 10/323,349
- Filed: 2002-12-18
- Granted: 2004-04-27
- Earliest claimed: 2002-12-18
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Jiunn-Der Yang; Chaucer Chnug; Yuan-Chang Huang
- Web page: https://patentgrep.com/patent/US6727155B1

## CPC

- H10P 50/283: {by chemical means}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method forming sidewall spacers on a semiconductor substrate without using the conventional plasma etching method is disclosed. In the method, a semiconductor substrate that has a gate structure formed on a top surface is first provided, followed by the deposition of a dielectric material layer on top of the semiconductor substrate. The substrate is then rotated to a rotational speed of at least 50 rpm, and an acid vapor is flown onto the substrate until the sidewall spacers are formed. The dielectric material layer for forming the sidewall spacers may be SiO2, SiON or Si3N4. The acid vapor utilized may be formed from an acid of HF, H3PO4, H2SO4 or HCl. In a preferred embodiment, the semiconductor substrate may be rotated to a rotational speed between about 100 rpm and about 150 rpm for a time period between about 10 sec. and about 20 sec.

## Claims

### Claim 1

A method for forming sidewall spacers on a semiconductor substrate comprising the steps of:
providing a semiconductor substrate having a gate structure formed on top;
depositing a dielectric material layer on top of said semiconductor substrate;
rotating said semiconductor substrate to a rotational speed of at least 50 rpm; and
flowing an acid vapor onto said semiconductor substrate until said sidewall spacers are formed.

### Claim 2 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1 further comprising the step of mounting the semiconductor substrate on a wafer chuck situated in a spin etcher.

### Claim 3 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1, wherein said dielectric material layer being formed of a material selected from the group consisting of SiO2, SiON and Si3N4, SiCON, SiCo and SiC.

### Claim 4 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1, wherein said semiconductor substrate is a silicon wafer.

### Claim 5 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1, wherein said gate structure is formed for a photoelectronic device.

### Claim 6 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1 further comprising the step, subsequent to said depositing step, of annealing said semiconductor substrate at a temperature of at least 700° C. for a time period of at least 10 min.

### Claim 7 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1 further comprising the step of annealing said semiconductor substrate at a temperature between about 700° C. and about 800° C. for a time period between about 10 min. and about 20 min. after said depositing step.

### Claim 8 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1 further comprising the step of flowing an acid vapor formed of an acid selected from the group consisting of HF, H3PO4, H2SO4, and HCl onto said semiconductor substrate.

### Claim 9 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1 further comprising the step of rotating said semiconductor substrate to a rotational speed between about 50 rpm and about 200 rpm.

### Claim 10 (depends on 1)

A method for forming sidewall spacers on a semiconductor substrate according to claim 1 further comprising the step of rotating said semiconductor substrate to a rotational speed between about 100 rpm and about 150 rpm for a time period between about 10 sec. and about 20 sec.

### Claim 11

A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate comprising the steps of:
providing a silicon substrate with a gate structure formed on top;
depositing a dielectric material layer on top of said silicon substrate;
annealing said dielectric material layer at a temperature of at least 700° C. for a time period of at least 10 min;
rotating said silicon substrate to a rotational speed of at least 50 rpm; and
flowing an acid vapor onto said silicon substrate and etching said dielectric material layer into dielectric spacers.

### Claim 12 (depends on 11)

A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate according to claim 11 further comprising the step of depositing said dielectric material layer from a material selected from the group consisting of SiO2, SiON and Si3N4.

### Claim 13 (depends on 11)

A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate according to claim 11 further comprising the step of mounting said silicon substrate on a wafer chuck situated in a spin etcher.

### Claim 14 (depends on 11)

A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate according to claim 11 further comprising the step of forming said gate structure for a photoelectronic device.

### Claim 15 (depends on 11)

A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate according to claim 11 further comprising the step of annealing said dielectric material layer at a temperature between about 700° C. and about 800° C. for a time period between about 10 min. and about 20 min.

### Claim 16 (depends on 11)

A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate according to claim 11 further comprising the step of flowing an acid vapor formed of an acid selected from the group consisting of HF, H3PO4, H2SO4 and HCl onto said semiconductor substrate.

### Claim 17 (depends on 11)

A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate according to claim 11 further comprising the step of rotating said semiconductor substrate to a rotational speed between about 50 rpm and about 200 rpm.

### Claim 18 (depends on 11)

A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate according to claim 11 further comprising the step of rotating said semiconductor substrate to a rotational speed between about 100 rpm and about 150 rpm for a time period between about 10 sec. and about 20 sec.