# US 6,727,151 B2 · Method to fabricate elevated source/drain structures in MOS transistors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,151 B2
- Document ID: US6727151B2
- Status: Granted
- Kind: B2
- Application number: 10/213,562
- Filed: 2002-08-07
- Published: 2004-02-12
- Granted: 2004-04-27
- Earliest claimed: 2002-08-07
- Assignees: Chartered Semiconductor Manufacturing Ltd.
- Inventors: Yung Fu Chong; Randall Cher Liang Cha; Alex See
- Web page: https://patentgrep.com/patent/US6727151B2

## CPC

- H10D 30/0225: {using an initial gate mask complementary to the prospective gate location, e.g. using dummy source and drain electrodes}
- H10D 30/0212: {using self-aligned silicidation}
- H10D 30/0278: {forming single crystalline channels on wafers after forming insulating device isolations}
- H10D 30/608: {having non-planar bodies, e.g. having recessed gate electrodes}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/015: {removing at least parts of gate spacers, e.g. disposable spacers}
- H10D 64/018: {Spacers formed inside holes at the prospective gate locations, e.g. holes left by removing dummy gates}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10D 64/259: {Source or drain electrodes being self-aligned with the gate electrode and having bottom surfaces higher than the interface between the channel and the gate dielectric}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for forming a MOSFET having an elevated source/drain structure is described. A sacrificial oxide layer is provided on a substrate. A polish stop layer is deposited overlying the sacrificial oxide layer. An oxide layer is deposited overlying the polish stop layer. An opening is formed through the oxide layer and the polish stop layer to the sacrificial oxide layer. First polysilicon spacers are formed on sidewalls of the opening wherein the first polysilicon spacers form an elevated source/drain structure. Second polysilicon spacers are formed on the first polysilicon spacers. The oxide layer and sacrificial oxide layer exposed within the opening are removed. An epitaxial silicon layer is grown within the opening. A gate dielectric layer is formed within the opening overlying the second polysilicon spacers and the epitaxial silicon layer. A gate material layer is deposited within the opening. The gate material layer, first polysilicon spacers and second polysilicon spacers are polished back to the polish stop layer thereby completing formation of a MOSFET having an elevated source/drain structure in the fabrication of an integrated circuit device.

## Claims

### Claim 1

A method of forming a MOSFET having an elevated source/drain structure in the fabrication of an integrated circuit device comprising:
providing a sacrificial oxide layer on a substrate;
depositing a polish stop layer overlying said sacrificial oxide layer;
depositing an oxide layer overlying said polish stop layer;
forming an opening through said oxide layer and said polish stop layer to said sacrificial oxide layer;
forming first polysilicon spacers on sidewalls of said opening wherein said first polysilicon spacers form said elevated source/drain structure;
forming second polysilicon spacers on said first polysilicon spacers;
removing said oxide layer and said sacrificial oxide layer exposed within said opening;
growing an epitaxial silicon layer within said opening;
forming a gate dielectric layer within said opening overlying said second polysilicon spacers and said epitaxial silicon layer;
depositing a gate material layer within said opening; and
polishing back said gate material layer, said first polysilicon spacers and said second polysilicon spacers to said polish stop layer thereby completing formation of said MOSFET having an elevated source/drain structure in the fabrication of said integrated circuit device.

### Claim 2 (depends on 1)

The method according to claim 1 wherein said polish stop layer comprises silicon nitride having a thickness of between about 100 and 1000 Angstroms.

### Claim 3 (depends on 1)

The method according to claim 1 wherein said step of forming said first polysilicon spacers comprises:
depositing a first polysilicon layer overlying said oxide layer and said sacrificial oxide layer within said opening; and
etching back said first polysilicon layer to leave said first polysilicon spacers only on sidewalls of said opening.

### Claim 4 (depends on 3)

The method according to claim 3 wherein said first polysilicon layer is doped after said depositing step and prior to said etching back step.

### Claim 5 (depends on 3)

The method according to claim 3 wherein said first polysilicon layer is in-situ doped.

### Claim 6 (depends on 1)

The method according to claim 1 wherein said step of forming said second polysilicon spacers comprises:
depositing a second polysilicon layer overlying said oxide layer and said sacrificial oxide layer and said first polysilicon spacers within said opening; and
etching back said second polysilicon layer to leave said second polysilicon spacers only on sidewalls of said first polysilicon spacers.

### Claim 7 (depends on 6)

The method according to claim 6 wherein said second polysilicon layer is doped after said depositing step and prior to said etching back step.

### Claim 8 (depends on 6)

The method according to claim 6 wherein said second polysilicon layer is in-situ doped.

### Claim 9 (depends on 6)

The method according to claim 6 wherein said second polysilicon spacers form lightly doped source/drain extensions.

### Claim 10 (depends on 1)

The method according to claim 1 wherein said epitaxial silicon layer is grown to a thickness of between about 10 and 500 Angstroms.

### Claim 11 (depends on 1)

The method according to claim 1 wherein during said step of growing said epitaxial silicon layer, said first and second polysilicon spacers also increase in size.

### Claim 12 (depends on 1)

The method according to claim 1 further comprising doping said epitaxial silicon layer for threshold voltage control.

### Claim 13 (depends on 1)

The method according to claim 1 wherein said gate material layer is selected from the group consisting of: polysilicon and metals.

### Claim 14 (depends on 1)

The method according to claim 1 wherein said polishing back step comprises chemical mechanical polishing.

### Claim 15

A method of forming a MOSFET having an elevated source/drain structure in the fabrication of an integrated circuit device comprising:
providing a sacrificial oxide layer on a substrate;
depositing a polish stop layer overlying said sacrificial oxide layer;
depositing an oxide layer overlying said polish stop layer;
forming an opening through said oxide layer and said polish stop layer to said sacrificial oxide layer;
forming first polysilicon spacers on sidewalls of said opening wherein said first polysilicon spacers form said elevated source/drain structure;
forming second polysilicon spacers on said first polysilicon spacers wherein a portion of said sacrificial oxide is exposed between said second polysilicon spacers within said opening;
removing said oxide layer and said sacrificial oxide layer exposed within said opening wherein said substrate is exposed within said opening;
growing an epitaxial silicon layer within said opening and doping said epitaxial silicon layer for threshold voltage control;
forming a gate dielectric layer within said opening overlying said second polysilicon spacers and said epitaxial silicon layer;
depositing a gate material layer within said opening; and
polishing back said gate material, said first polysilicon spacers and said second polysilicon spacers to said polish stop layer thereby completing formation of said MOSFET having an elevated source/drain structure in the fabrication of said integrated circuit device.

### Claim 16 (depends on 15)

The method according to claim 15 wherein said polish stop layer comprises silicon nitride having a thickness of between about 100 and 1000 Angstroms.

### Claim 17 (depends on 15)

The method according to claim 15 wherein said step of forming said first polysilicon spacers comprises:
depositing a first polysilicon layer overlying said oxide layer and said sacrificial oxide layer within said opening; and
etching back said first polysilicon layer to leave said first polysilicon spacers only on sidewalls of said opening.

### Claim 18 (depends on 17)

The method according to claim 17 wherein said first polysilicon layer is doped prior to said etching back step and wherein a doping method is selected from the group consisting of in-situ doping and ion implantation.

### Claim 19 (depends on 15)

The method according to claim 15 wherein said step of forming said second polysilicon spacers comprises:
depositing a second polysilicon layer overlying said oxide layer and said sacrificial oxide layer and said first polysilicon spacers within said opening; and
etching back said second polysilicon layer to leave said second polysilicon spacers only on sidewalls of said first polysilicon spacers.

### Claim 20 (depends on 19)

The method according to claim 19 wherein said second polysilicon layer is doped prior to said etching back step and wherein a doping method is selected from the group consisting of in-situ doping and ion implantation.

### Claim 21 (depends on 19)

The method according to claim 19 wherein said second polysilicon spacers form lightly doped source/drain extensions.

### Claim 22 (depends on 15)

The method according to claim 15 wherein said epitaxial silicon layer is grown to a thickness of between about 10 and 500 Angstroms.

### Claim 23 (depends on 15)

The method according to claim 15 wherein during said step of growing said epitaxial silicon layer, said first and second polysilicon spacers also increase in size.

### Claim 24 (depends on 15)

The method according to claim 15 wherein said gate material layer is selected from the group consisting of: polysilicon and metals.

### Claim 25 (depends on 15)

The method according to claim 15 wherein said polishing back step comprises chemical mechanical polishing.

### Claim 26

A method of forming a MOSFET having an elevated source/drain structure in the fabrication of an integrated circuit device comprising:
providing a sacrificial oxide layer on a substrate;
depositing a polish stop layer overlying said sacrificial oxide layer;
depositing an oxide layer overlying said polish stop layer;
forming an opening through said oxide layer and said polish stop layer to said sacrificial oxide layer;
depositing a first polysilicon layer overlying said oxide layer and said sacrificial oxide layer within said opening;
etching back said first polysilicon layer to leave first polysilicon spacers only on sidewalls of said opening;
depositing a second polysilicon layer overlying said oxide layer and said sacrificial oxide layer and said first polysilicon spacers within said opening;
etching back said second polysilicon layer to leave said second polysilicon spacers only on sidewalls of said first polysilicon spacers wherein a portion of said sacrificial oxide is exposed between said second polysilicon spacers within said opening and wherein said second polysilicon spacers form lightly doped source/drain extensions;
removing said oxide layer and said sacrificial oxide layer exposed within said opening wherein said substrate is exposed within said opening;
growing an epitaxial silicon layer within said opening wherein said first and second polysilicon spacers also increase in size;
doping said epitaxial silicon layer for threshold voltage control;
thereafter forming a gate dielectric layer within said opening overlying said second polysilicon spacers and said epitaxial silicon layer;
depositing a conducting layer within said opening; and
polishing back said conducting layer, said first polysilicon spacers and said second polysilicon spacers to said polish stop layer wherein said conducting layer forms a gate electrode and said first polysilicon spacers form said elevated source/drain regions thereby completing formation of said MOSFET having an elevated source/drain structure in the fabrication of said integrated circuit device.

### Claim 27 (depends on 26)

The method according to claim 26 wherein said polish stop layer comprises silicon nitride having a thickness of between about 100 and 1000 Angstroms.

### Claim 28 (depends on 26)

The method according to claim 26 wherein said first polysilicon layer is doped prior to said etching back said first polysilicon layer and wherein a doping method is selected from the group consisting of in-situ doping and ion implantation.

### Claim 29 (depends on 26)

The method according to claim 26 wherein said second polysilicon layer is doped prior to said etching back said second polysilicon layer and wherein a doping method is selected from the group consisting of in-situ doping and ion implantation.

### Claim 30 (depends on 26)

The method according to claim 26 wherein said epitaxial silicon layer is grown to a thickness of between about 10 and 500 Angstroms.

### Claim 31 (depends on 26)

The method according to claim 26 wherein said conducting layer is selected from the group consisting of: polysilicon and metals.

### Claim 32 (depends on 26)

The method according to claim 26 wherein said polishing back step comprises chemical mechanical polishing.