# US 6,727,135 B2 · All-in-one disposable/permanent spacer elevated source/drain, self-aligned silicide CMOS

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,135 B2
- Document ID: US6727135B2
- Status: Granted
- Kind: B2
- Application number: 10/464,339
- Filed: 2003-06-18
- Published: 2003-11-13
- Granted: 2004-04-27
- Earliest claimed: 2001-07-19
- Assignees: International Business Machines Corporation
- Inventors: Kam Leung Lee; Ronnen Andrew Roy
- Web page: https://patentgrep.com/patent/US6727135B2

## CPC

- H10D 64/015: {removing at least parts of gate spacers, e.g. disposable spacers}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 30/0275: {forming single crystalline semiconductor source or drain regions resulting in recessed gates, e.g. forming raised source or drain regions}
- H10D 30/608: {having non-planar bodies, e.g. having recessed gate electrodes}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10D 84/0133: {Manufacturing common source or drain regions between multiple IGFETs}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A complementary metal oxide semiconductor (CMOS) device having silicide contacts that are self-aligned to deep junction edges formed within a surface of a semiconductor substrate as well as a method of manufacturing the same are disclosed. Specifically, the CMOS device includes a plurality of patterned gate stack regions formed on a surface of a semiconductor substrate. Each plurality of patterned gate stack regions includes an L-shaped nitride spacer formed on exposed vertical sidewalls thereof, the L-shaped nitride spacer having a vertical element and a horizontal element, wherein the horizontal element is formed on a portion of the substrate that abuts each patterned gate stack region. Silicide contacts are located on other portions of the semiconductor substrate between adjacent patterned gate stack regions not containing the horizontal element of the L-shaped nitride spacer.

## Claims

### Claim 1

A method of forming a CMOS device comprising the steps of:
(a) providing a plurality of patterned gate stack regions on a surface of a semiconductor substrate, wherein each of said patterned gate stack regions includes exposed vertical sidewalls;
(b) forming a composite spacer on each exposed vertical sidewall, said composite spacer including a bilayer comprising a nitride layer and a Si-containing film, wherein said Si-containing film is thicker than said nitride layer and is formed on said nitride layer;
(c) forming deep source and drain regions in said surface of said semiconductor substrate;
d) removing said Si-containing film and forming shallow junctions in said semiconductor substrate in areas abutting each of said patterned gate stack regions;
(e) removing portions of said nitride layer so as to form an L-shaped nitride spacer on each vertical sidewall of said patterned gate stack regions and activating said source and drain regions; and
(t) forming silicide contacts in exposed regions of said semiconductor substrate not containing said L-shaped nitride spacer.

### Claim 2 (depends on 1)

The method of claim 1 wherein step (a) comprises deposition, lithography and etching.

### Claim 3 (depends on 1)

The method of claim 1 wherein said composite spacer is formed by sequentially depositing a conformal nitride layer and then said Si-containing film, and etching said Si-containing film.

### Claim 4 (depends on 3)

The method of claim 3 wherein said etching comprises an anisotropic spacer etch process.

### Claim 5 (depends on 1)

The method of claim 1 wherein said deep source and drain regions are formed by ion implantation.

### Claim 6 (depends on 5)

The method of claim 5 wherein said ion implantation is performed using an ion dose of about 1E15 cm−2 or greater and an implant energy of about 5 keV or greater.

### Claim 7 (depends on 6)

The method of claim 6 wherein said ion implantation is performed using an ion dose of about 2E15 cm−2 to about 2E16 cm−2 and an implant energy of from about 7 to about 50 keV.

### Claim 8 (depends on 1)

The method of claim 1 wherein said Si-containing film is removed by reactive-ion etching.

### Claim 9 (depends on 1)

The method of claim 1 wherein said Si-containing film is removed by a selective wet chemical etch process.

### Claim 10 (depends on 9)

The method of claim 9 wherein said selective wet chemical etch process includes the use of KOH.

### Claim 11 (depends on 1)

The method of claim 1 wherein said shallow junctions are formed by ion implantation.

### Claim 12 (depends on 11)

The method of claim 11 wherein said ion implantation is performed using an ion dose of about 2E15 cm−2 or less and an implant energy of about 20 keV or less.

### Claim 13 (depends on 12)

The method of claim 12 wherein said ion implantation is performed using an ion dose of from about 3E14 to about 1E15 cm−2 and an implant energy of from about 0.5 to about 5 keV.

### Claim 14 (depends on 1)

The method of claim 1 wherein said L-shaped nitride spacers are formed by a selective, wet chemical etch process.

### Claim 15 (depends on 14)

The method of claim 14 wherein said selective wet chemical etch process includes H3PO4 as an etchant.

### Claim 16 (depends on 1)

The method of claim 1 wherein halo implant regions and source/drain regions are formed between steps (e) and (f).

### Claim 17 (depends on 1)

The method of claim 1 wherein said silicide contacts are formed by a silicidation process.

### Claim 18 (depends on 17)

The method of claim 17 wherein said silicidation process comprises the steps of: forming a refractory metal on exposed surfaces of said semiconductor substrate, annealing said refractory metal so as to convert said refractory metal into a metal silicide, and optionally, removing any non-reactant refractory metal.

### Claim 19 (depends on 18)

The method of claim 18 wherein said annealing is performed at a temperature of about 350° C. or greater.

### Claim 20 (depends on 19)

The method of claim 19 wherein said annealing is performed at a temperature of about 450° C. or greater.

### Claim 21 (depends on 1)

The method of claim 1 wherein an epi Si layer is formed on exposed surfaces of said semiconductor substrate between steps (e) and (f).

### Claim 22 (depends on 21)

The method of claim 21 wherein said epi Si layer is formed by a selective epitaxial growing process.