# US 6,727,131 B2 · System and method for addressing junction capacitances in semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,131 B2
- Document ID: US6727131B2
- Status: Granted
- Kind: B2
- Application number: 10/279,650
- Filed: 2002-10-24
- Published: 2003-05-01
- Granted: 2004-04-27
- Earliest claimed: 2001-10-26
- Assignees: Texas Instruments Incorporated
- Inventors: Zhiqiang Wu; Kaiping Liu
- Web page: https://patentgrep.com/patent/US6727131B2

## CPC

- H10P 30/21: {of electrically active species}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of forming a semiconductor device is provided that comprises forming a gate conductor proximate to and insulated from an outer surface of a semiconductor substrate. The gate conductor defines a channel region disposed inwardly from the gate conductor. Source and drain regions are formed in the semiconductor substrate, each disposed adjacent one edge of the channel region. The semiconductor substrate and the source and drain regions have an associated bottom wall junction capacitance. A transient enhanced diffusion anneal is used to affect ion concentration profiles associated with the source and drain regions, resulting in an increased balance in the ion concentration profiles of the source and drain regions and an ion concentration associated with the semiconductor substrate, which results in reduction of the bottom wall junction capacitance.

## Claims

### Claim 1

A method of forming a semiconductor device, comprising:
forming a gate conductor proximate to and insulated from an outer surface of a semiconductor substrate, the gate conductor defining a channel region disposed inwardly from the gate conductor;
forming source and drain regions in the semiconductor substrate, the source and drain regions each being disposed adjacent one edge of the channel region, the semiconductor substrate and the source and drain regions having a bottom wall junction capacitance associated therewith; and
effecting a transient enhanced diffusion anneal of the source and drain regions causing ion concentration profiles associated with the source and drain regions to be affected resulting in an increased balance in the ion concentration profiles of the source and drain regions and an ion concentration profile associated with the semiconductor substrate such that a reduction in the bottom wall junction capacitance is achieve; and
effecting a rapid thermal anneal on the source and drain regions after the transient enhanced diffusion anneal in order to enhance the increased balance in the ion concentration profiles of the source and drain regions and the ion concentration profile associated with the semiconductor substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the transient enhanced diffusion anneal is executed in a temperature range of approximately 550° C. to 800° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the transient enhanced diffusion anneal has a time duration of approximately 10 minutes to 120 minutes.

### Claim 4 (depends on 1)

The method of claim 1, further comprising introducing an ionic implant into the substrate such that the ion concentration profiles associated with the source and drain regions are affected in order to facilitate achievement of the increased balance.

### Claim 5 (depends on 4)

The method of claim 4, wherein the introducing of the ionic implant comprises introducing ionic impurities comprising phosphorous into the semiconductor substrate having an associated energy level in a range of approximately 10 to 60 KeV and an associated dosage level in a range of approximately 1E13 to 2E15 ions/cm2.

### Claim 6 (depends on 4)

The method of claim 4, wherein the introducing of the ionic implant comprises introducing ionic impurities comprising boron into the substrate having an associated energy level in a range of approximately 3 KeV to 20 KeV and an associated dosage level in a range of approximately 1E13 to 2E15 ions/cm2.

### Claim 7 (depends on 1)

The method of claim 1, wherein the rapid thermal anneal is executed in a temperature range of approximately 900° C. to 1100° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the rapid thermal anneal has a time duration of approximately 1 second to 30 seconds.

### Claim 9

A transistor formed in a semiconductor layer comprising:
a gate conductor formed proximate to and insulated from an outer surface of the semiconductor layer, the gate conductor defining a channel region disposed inwardly from the gate conductor; and
a source and a drain region, each disposed adjacent one edge of the channel region and each having an ion concentration profile associated therewith, wherein the source and drain region receive a rapid thermal anneal after the transient diffusion anneal in order to enhance the increased balance in the ion concentration profiles of the source and drain regions and the ion concentration profile associated with the semiconductor layer.

### Claim 10 (depends on 9)

The transistor of claim 9, wherein the transient enhanced diffusion anneal is executed in a temperature range of approximately 550° C. to 800° C.

### Claim 11 (depends on 9)

The transistor of claim 9, wherein the transient enhanced diffusion anneal has a time duration of approximately 10 minutes to 120 minutes.

### Claim 12 (depends on 9)

The transistor of claim 9, wherein an ionic implant is introduced into the semiconductor layer such that the ion concentration profiles associated with the source and drain regions are affected in order to facilitate achievement of the increased balance.

### Claim 13 (depends on 12)

The transistor of claim 12, wherein the introducing of the ionic implant comprises introducing ionic impurities comprising phosphorous into the semiconductor layer having an associated energy level in a range of approximately 10 to 60 KeV and an associated dosage level in a range of approximately 1E13 to 2E15 ions/cm2.

### Claim 14 (depends on 12)

The transistor of claim 12, wherein the introducing of the ionic implant comprises introducing ionic impurities comprising boron into the semiconductor layer having an associated energy level in a range of approximately 3 KeV to 20 KeV and an associated dosage level in a range of approximately 1E13 to 2E15 ions/cm2.

### Claim 15 (depends on 9)

The transistor of claim 9, wherein the rapid thermal anneal is executed in a temperature range of approximately 900° C. to 1100° C.

### Claim 16 (depends on 9)

The transistor of claim 9, wherein the rapid thermal anneal has a time duration of approximately 1 second to 30 seconds.

### Claim 17

A method of forming a semiconductor device, comprising:
forming a gate conductor proximate to and insulated from an outer surface of a semiconductor substrate, the gate conductor defining a channel region disposed inwardly from the gate conductor;
forming source and drain regions in the semiconductor substrate, the source and drain regions each being disposed adjacent one edge of the channel region, the semiconductor substrate and the source and drain regions having a bottom wall junction capacitance associated therewith;
introducing an ionic implant comprising boron into the semiconductor substrate having an associated energy level in a range of approximately 3 to 20 KeV and an associated dosage level in a range of approximately 1E13 to 2E15 ions/cm2 such that ion concentration profiles associated with the source and drain regions is affected;
effecting a transient enhanced diffusion anneal in a temperature range of approximately 550° C. to 800° C. for a duration of approximately 10 minutes to 120 minutes of the source and drain regions causing the ion concentration profiles associated with the source and drain regions to be affected resulting in an increased balance in the ion concentration profiles of the source and drain regions and an ion concentration profile associated with the semiconductor substrate such that a reduction in the bottom wall junction capacitance is achieved; and
effecting a rapid thermal anneal after the transient enhanced anneal on the source and drain regions in a temperature range of approximately 900° C. to 1100° C. for a duration of approximately 1 to 30 seconds, the rapid thermal anneal enhancing the increased balance in the ion concentration profiles of the source and drain regions and the ion concentration profile associated with the semiconductor substrate.