# US 6,727,110 B2 · Silica-based optical device fabrication

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,727,110 B2
- Document ID: US6727110B2
- Status: Granted
- Kind: B2
- Application number: 09/986,250
- Filed: 2001-11-08
- Published: 2002-05-30
- Granted: 2004-04-27
- Earliest claimed: 2000-11-29
- Assignees: Redfern Integrated Optics Pty LTD
- Inventors: Michael Bazylenko
- Web page: https://patentgrep.com/patent/US6727110B2

## CPC

- G02B 6/132: by deposition of thin films
- C23C 16/402: {Silicon dioxide}
- C23C 16/5096: {Flat-bed apparatus}
- C23C 28/00: Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method and apparatus for fabricating silica-based waveguide devices on a substrate using a low temperature PECVD process using a TEOS source material for depositing waveguide layers containing silica, the apparatus being arranged, in use, in a manner such that a liquid source material containing silicon is used during the PECVD.

## Claims

### Claim 1

A method of fabricating a silica-based waveguide photonic device, the method comprising the step of depositing waveguide layers containing silica using PECVD, wherein a liquid source material containing silicon is used during the PECVD deposition process, the source material not comprising SiCl4, silane, or a derivative of silane, and at least one as-deposited layer having low optical losses in the infra-red region is produced.

### Claim 2 (depends on 1)

A method as claimed in claim 1 wherein said waveguide layers are deposited using a low temperature deposition process.

### Claim 3 (depends on 2)

A method as claimed in claim 2 wherein the deposition process temperature is below 500 degrees Celsius.

### Claim 4 (depends on 1)

A method as claimed in claim 1, wherein the PECVD is carried out in the absence of nitrogen and nitrogen-containing source materials.

### Claim 5 (depends on 1)

A method as claimed in claim 1, wherein said waveguide device is formed without high temperature thermal annealing of said waveguide layers.

### Claim 6 (depends on 1)

A method as claimed in claim 1, wherein said waveguide device is formed without being annealing at temperatures of 800 degrees Celsius or higher.

### Claim 7 (depends on 1)

A method as claimed in claim 1, wherein the PECVD is carried out in an ambient comprising a mixture of oxygen and vapour from the liquid source material.

### Claim 8 (depends on 1)

A method as claimed in claim 1, wherein the liquid source material comprises tetraethoxysilane.

### Claim 9 (depends on 1)

A method as claimed in claim 1, wherein the method further comprises a step of controlling a refractive index contrast between the deposited waveguide layers by incorporating a dopant material during the PECVD.

### Claim 10 (depends on 9)

A method as claimed in claim 9, wherein the dopant material is provided in a gaseous or liquid form.

### Claim 11 (depends on 9)

A method as claimed in claim 9, wherein the dopant material comprises tetramethylgermaniun.

### Claim 12 (depends on 1)

A method as claimed in claim 1, wherein the method further comprises a step of controlling at least one optical property of at least one of the waveguide layers by controlling ion bombardment of the deposited waveguide layer during the PECVD process.

### Claim 13 (depends on 12)

A method as claimed in claim 12, wherein the ion bombardment is controlled by controlling a spacing between electrodes used during the PECVD.

### Claim 14 (depends on 12)

A method as claimed in claim 12, wherein the ion bombardment is controlled by controlling a frequency of RF power applied to electrodes used during the PECVD process.

### Claim 15 (depends on 12)

A method as claimed in claim 12, wherein the step of controlling at least one optical property comprises: simultaneously applying a lower frequency component of RF power and an upper frequency of RF power to electrodes used during the PECVD, each component having a different frequency; and controlling ion bombardment by controlling the power of the lower frequency component so as to control the or each optical property.

### Claim 16 (depends on 12)

A method as claimed in claim 12, wherein the or each optical property which is controlled through the ion bombardment is selected from a group comprising a refractive index of the waveguide layer and a stress-induced birefringence in the waveguide layer.

### Claim 17 (depends on 1)

A method as claimed in claim 1, further comprising a step of using ion bombardment during the PECVD to control a level of stress in each waveguide layer.

### Claim 18 (depends on 1)

A method as claimed in claim 1, further comprising a step of using ion bombardment during the PECVD to minimise curvature of a wafer onto which the waveguide layer is being deposited.

### Claim 19 (depends on 1)

A method as claimed in claim 1, wherein a frequency of RF power used in the PECVD or a deposition rate of the PECVD is controlled to achieve a homogeneous material with low porosity and low optical scattering characteristics.

### Claim 20 (depends on 1)

A method as claimed in claim 1, wherein a frequency of RF power used in a PECVD or a deposition rate of the PECVD is controlled to achieve a product which has a low hydroscopicity, and is environmentally-stable.

### Claim 21

A method of fabricating a silica-based waveguide photonic device, the method comprising the step of depositing waveguide layers containing silica using PECVD, wherein a liquid source material containing silicon is used during the PECVD deposition process, the liquid source material comprising tetraethoxysilane, and at least one as-deposited layer having low optical losses in the infra-red region is produced.

### Claim 22 (depends on 21)

A method as claimed in claim 21, wherein the step of depositing waveguide layers further comprises using a process temperature which is below 500° C.

### Claim 23 (depends on 21)

A method as claimed in claim 21, wherein said waveguide is formed without being annealed at temperatures of 800° C. or higher.