- Number: US 6,726,988 B2
- Document ID: US6726988B2
- Status: Granted
- Kind: B2
- Application number: 10/108,380
- Filed: 2002-03-29
- Published: 2002-11-21
- Granted: 2004-04-27
- Earliest claimed: 2001-04-05
- Assignees: TDK Corporation
- Inventors: Hitoshi Hirayama; Masao Nakayama
- Web page: https://patentgrep.com/patent/US6726988B2

## CPC

- G11B 5/73937: {Substrates having an organic polymer comprising a ring structure}
- Y10T 428/31681: Next to polyester, polyamide or polyimide [e.g., alkyd, glue, or nylon, etc.]
- Y10T 428/31725: Of polyamide
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A magnetic recording medium comprises a non-magnetic substrate and a metal thin film magnetic layer formed by an oblique evaporating method on the substrate, the non-magnetic substrate being an aromatic polyamide film. The film has a thickness of 3.0 μm to 6.0 μm, has a Young's modulus in the transverse direction of 16000 MPa to 18000 MPa, and has a thermal contraction coefficient (in the transverse direction; 180° C. for 30 minutes) of 0.7% to 1.3%. With this structure, it has been found that the thermal deformation (cupping) after the thin film is formed can be prevented to improve head touch and the electromagnetic conversion properties.

## Claims

### Claim 1

A magnetic recording medium comprising:
a non-magnetic substrate;
a metal thin film magnetic layer formed on the substrate by an oblique vapor evaporating method;
a plasma-polymerized carbon layer on the magnetic layer;
a lubricant on the carbon layer; and
a back coat layer with a thickness of 0.3 μm to 0.7 μm on a side opposite to the magnetic layer of the substrate,
wherein the non-magnetic substrate is an aromatic polyamide film,
wherein the film has a Young's modulus in the transverse direction of 16000 MPa to 18000 MPa, and has a thermal contraction coefficient of 0.7% to 1.3%, and
wherein the lubricant is represented by R1-A-R2, where R1 is CF3(CF2)n—, CF3(CF2)n(CH2)m—, CH3(CH2)1—, or H; A is COOCH(C1H21+1)CH2COO, and R2 is CF3(CF2)n—, CF3(CF2)n(CH2)m—, CH3(CH2)1—, or H; provided that R1 noteq R2, n=7 to 17, m=1 to 3, and l=7 to 30.

### Claim 2 (depends on 1)

A magnetic recording medium according to claim 1, wherein the non-magnetic substrate has a thickness of 3.0 μm to 6.0 μm.