# US 6,726,956 B1 · Ceramic-coated fiberglass member and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,956 B1
- Document ID: US6726956B1
- Status: Granted
- Kind: B1
- Application number: 10/032,192
- Filed: 2001-12-20
- Granted: 2004-04-27
- Earliest claimed: 2001-12-20
- Inventors: Russell John Meeks; Rodney Jay Wagner; Lona Marie Jensen
- Web page: https://patentgrep.com/patent/US6726956B1

## CPC

- F16L 9/10: of glass or ceramics, e.g. clay, clay tile, porcelain (F16L9/16 - F16L9/22 take precedence)
- F16L 9/105: {of glass}
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL

## Abstract

A ceramic-coated fiberglass member and method for manufacturing the same that withstands flames or high temperatures for a substantial period of time. A fiberglass pipe is washed and dried. The pipe is sanded axially along the lengthwise direction of the pipe to expose pores on the pipes. A first ceramic base coating is applied evenly on the pipe. Then, the first ceramic base coating is burnished into the pores. Next, the first ceramic base coating is dried so that substantially no moisture is left in the first ceramic base coating. The first ceramic base coating is axially burnished along the lengthwise direction of the pipe. Then, a second ceramic base coating is applied on the first ceramic base coating. The pipe is dried with first and second ceramic base coatings thereon. The pipe is burnished axially with first and second ceramic base coatings. Subsequently, a first ceramic top coating is applied evenly on the second ceramic base coating. The first ceramic top coating is dried so that substantially no moisture is left in the first ceramic top coating. The first ceramic top coating is burnished axially along the lengthwise direction of the pipe. A second ceramic top coating is applied evenly on the first ceramic top coating. The present invention ceramic-coated fiberglass pipe can withstand 900 degrees F. for over an hour, exceeding the requirement of U.S. Coast Guard (400 degrees F. of open flame for ten minutes) by more than twice.

## Claims

### Claim 1

A method of manufacturing a ceramic-coated fiberglass pipe, comprising:
washing and drying a fiberglass pipe;
sanding the pipe axially along the lengthwise direction to expose pores on the pipes;
applying a first ceramic base coating evenly on the pipe;
axially burnishing the first ceramic base coating into the pore;
drying the first ceramic base coating such that substantially no moisture is left in the first ceramic base coating;
axially burnishing the first ceramic base coating along the lengthwise direction of the pipe;
applying a second ceramic base coating on the first ceramic base coating; and
drying the pipe with first and second ceramic;base coatings coated thereon.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first ceramic base coating comprises a slurry including silica, porcelain clay, and water.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first or second ceramic base coating is formed to a thickness of approximately 0.010 inch thick.

### Claim 4 (depends on 1)

The method of claim 1, wherein the second ceramic base coating material is formed of the same material as the first ceramic top coating material.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
axially burnishing the pipe with first and second ceramic base coatings;
applying a first ceramic top coating evenly on the second ceramic base coating; and
drying the first ceramic top coating such that substantially no moisture is left in the first ceramic top coating.

### Claim 6 (depends on 5)

The method of claim 5, further comprising:
axially burnishing the first ceramic top coating along the direction of the pipe; and
applying a second ceramic top coating evenly on the first ceramic top coating.

### Claim 7 (depends on 6)

The method of claim 6, wherein the first or second ceramic top coating is formed to a thickness of approximately 0.010 inch thick.

### Claim 8 (depends on 6)

The method of claim 6, wherein the first ceramic top coating comprises a slurry including silica, porcelain clay, and water.

### Claim 9 (depends on 6)

The method of claim 6, wherein the second ceramic top coating comprises the same material as first ceramic top coating.

### Claim 10 (depends on 6)

The method of claim 6, wherein the first and second ceramic top coatings or base coatings are formed to a combined thickness of approximately 0.020 inch.

### Claim 11 (depends on 6)

The method of claim 6, wherein the first and second ceramic base coatings and the first and second ceramic top coatings are formed to a combined thickness of approximately 0.040 inch.

### Claim 12 (depends on 1)

The method of claim 1, wherein the pipe is a fiberglass reinforced epoxy thermosetting-resin pipe.

### Claim 13 (depends on 1)

The method of claim 1, wherein the drying the pipe is performed for approximately eight (8) hours in 70 degree Fahrenheit or above with not more than 50% humidity.