# US 6,726,955 B1 · Method of controlling the crystal structure of polycrystalline silicon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,955 B1
- Document ID: US6726955B1
- Status: Granted
- Kind: B1
- Application number: 09/605,518
- Filed: 2000-06-27
- Granted: 2004-04-27
- Earliest claimed: 2000-06-27
- Assignees: Applied Materials, Inc.
- Inventors: Shulin Wang; Steven A. Chen; Lee Luo; Errol Sanchez
- Web page: https://patentgrep.com/patent/US6726955B1

## CPC

- C23C 16/24: Deposition of silicon only
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3466: {Crystal orientation}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming a polycrystalline silicon film comprising: providing a process gas mix comprising a silicon source gas and a dilution gas mix wherein the dilution gas mix comprises H2 and an inert gas; and forming a polycrystalline silicon film from said silicon source gas.

## Claims

### Claim 1

A method of depositing a polycrystalline silicon film having a random grain silicon comprising:
providing a substrate on a wafer support in a chamber;
heating said substrate to a temperature greater than 650° C.;
flowing a silicon source gas into said chamber;
following a dilution gas mix into said chamber wherein the dilution gas mix comprises H2 and an inert gas in such a concentration ratio that a polycrystalline silicon film having random grains is formed during deposition; and
depositing said random grain polycrystalline silicon film on said substrate by thermally decomposing said silicon source gas in said chamber while flowing said silicon source gas and said dilution gas mix into said chamber and heating said substrate to said temperature.

### Claim 2 (depends on 1)

The method of claim 1 wherein said inert gas is selected from the group consisting of nitrogen (N2), helium (He) and Argon (Ar).

### Claim 3 (depends on 1)

The method of claim 1 wherein H2 comprises less than 20% of said dilution gas mix by volume.

### Claim 4 (depends on 1)

The method of claim 1 wherein H2 comprises more than 8% of said dilution gas mix.

### Claim 5 (depends on 1)

The method of claim 1 wherein H2 comprises between 10-15% of said dilution gas mix.

### Claim 6 (depends on 1)

The method of claim 1 wherein said dilution gas mix has an H2/inert gas volume concentration ratio such that said polycrystalline silicon film is deposited with a random grain structure with an average grain size between 50-500 Å.

### Claim 7 (depends on 1)

The method of claim 1 wherein said polycrystalline silicon is dominated by the <111> crystalline orientation.

### Claim 8 (depends on 1)

The method of claim 1 wherein said silicon source gas is silans (SiH4).

### Claim 9

A method of depositing a random grain polycrystalline silicon film comprising:
placing a substrate on a support in a chamber;
heating said support to a temperature between 700-740° C.;
generating a pressure between 150-350 torr in said chamber; flowing a silicon source gas into said chamber;
flowing a dilution gas mix wherein said dilution gas mix comprises H2 and N2 in such a concentration ratio that a polycrystalline silicon film having random grains is formed during deposition; and
depositing said random grain polycrystalline silicon film on said substrate by thermally decomposing said silicon source gas in said chamber while flowing said silicon source gas and said dilution gas mix into said chamber and heating said support to said temperature and generating said pressure.

### Claim 10 (depends on 9)

The method of claim 9 wherein H2 comprises less than 20% of said dilution gas mix.

### Claim 11 (depends on 9)

The method of claim 9 wherein H2 comprises more than 8% of said dilution gas mix.

### Claim 12 (depends on 9)

The method of claim 9 wherein H2 comprises between 10-15% of said dilution gas mix.

### Claim 13 (depends on 9)

The method of claim 9 wherein said dilution gas mix has an H2/N2 concentration ratio such that said polycrystalline silicon film is deposited with a random grain structure with an average grain size between 50-500 Å.

### Claim 14 (depends on 9)

The method of claim 9 wherein said polycrystalline silicon is dominated by the <111> crystalline orientation.

### Claim 15 (depends on 9)

The method of claim 9 wherein said silicon source gas is silane (SiH4).

### Claim 16 (depends on 9)

The method of claim 9 wherein said dilution gas has a flow rate of between 10-30 slm into said chamber while said silane gas has a flow rate of between 50-150 sccm.

### Claim 17 (depends on 9)

The method of claim 9 wherein said dilution gas has a flow rate of between 12-20 slm into said chamber while said silane gas has a flow rate of between 70-100 sccm.

### Claim 18 (depends on 9)

The method of claim 9 wherein said dilution gas mix and said silicon source gas are fed into said chamber at a concentration and temperature to deposit a said polycrystalline silicon film at a rate between 1000-5000 Å per minute.

### Claim 19

A method of depositing a random grain polycrystalline silicon film comprising:
placing a substrate into a chamber having aluminum sidewalls and an aluminum nitride substrate support having a resistive heater contained therein;
heating said substrate to a temperature greater than 650° C.; flowing a silicon source gas into said chamber;
flowing a dilution gas mix into said chamber wherein said dilution gas mix comprises H2 and N2 in such a concentration ratio that a polycrystalline silicon film having random grains is formed during deposition; and
depositing said random grain polycrystalline silicon film on said substrate by thermally decomposing said silicon source gas in said chamber while providing said process gas mix into said chamber and while heating said substrate to said temperature.

### Claim 20 (depends on 19)

The method of claim 19 further comprising providing a flow of N2 gas into said chamber from below said substrate support wherein said process gas mix flow and said flow of N2 is the total gas flow into said chamber.

### Claim 21 (depends on 20)

The method of claim 20 wherein H2 comprises less than 20% of said total gas flow into said chamber.

### Claim 22 (depends on 20)

The method of claim 20 wherein H2 comprises more than 8% of said total gas flow into said chamber.

### Claim 23 (depends on 20)

The method of claim 20 wherein H2 comprises between 10-15% of said total gas flow into said chamber.

### Claim 24

A method of depositing a doped random grain polycrystalline silicon gate electrode comprising:
placing a substrate into a chamber;
heating said substrate to a temperature greater than 650° C.;
flowing a silicon source gas into said chamber wherein said dilution gas mix comprises H2 and an inert gas in such a concentration ratio that a polycrystalline silicon film having random grains is formed during deposition;
depositing said random grain polycrystalline silicon film on said substrate by thermally decomposing said silicon source gas in said chamber while flowing said silicon source gas and said dilution gas mix into said chamber and while heating said substrate; and
implanting dopants into said random grain polycrystalline silicon film.

### Claim 25

A method of forming a composite tungsten/polycrystalline silicon film comprising:
placing a substrate into a chamber;
heating said substrate to a temperature greater than 650° C.;
flowing a silicon source gas into said chamber wherein said dilution gas mix comprises H2 and an inert gas in such a concentration ratio that a polycrystalline silicon film having random grains is formed during deposition;
depositing said random grain polycrystalline silicon film on said substrate by thermally decomposing said silicon source gas in said chamber while flowing said silicon source gas and said dilution gas mix into said chamber and while heating said substrate to said temperature; and
forming a tungsten or tungsten suicide film on said random grain polycrystalline silicon film utilizing a reactant gas mix comprising WF6.

### Claim 26

A method of depositing a random grain polycrystalline silicon film comprising:
placing a substrate on a support in a chamber;
heating said support to a temperature between 700-740° C.;
generating a pressure between 150-350 torr in said chamber;
flowing a silicon source gas into said chamber wherein said dilution gas mix comprises H2 and an inert gas in such a concentration ratio that a polycrystalline silicon film having random grains is formed during deposition; and
depositing said random grain polycrystalline silicon film on said substrate by thermally decomposing said silicon source gas in said chamber while flowing said silicon source gas and said dilution gas mix and while heating said support to said temperature and while generating said pressure.

### Claim 27

A method of depositing a random grain polycrystalline silicon film comprising:
placing a substrate on a support in a chamber;
heating said substrate;
generating a pressure between 150-350 torr in said chamber;
flowing a silicon source gas into said chamber wherein said dilution gas mix comprises H2 and an inert gas in such a concentration ratio that a polycrystalline silicon film having random grains is formed during deposition; and
depositing said random grain polycrystalline silicon film on said substrate by thermally decomposing said silicon source gas in said chamber while flowing said silicon source gas and said dilution gas mix and while generating said pressure.

### Claim 28

A method of depositing a random grain polycrystalline silicon film comprising:
placing a substrate on a support in a chamber;
heating said support to a temperature between 700-740° C.;
flowing a silicon source gas into said chamber wherein said dilution gas mix comprises H2 and an inert gas in such a concentration ratio that a polycrystalline silicon film having random grains is formed during deposition; and
depositing said random grain polycrystalline silicon film on said substrate by thermally decomposing said silicon source gas in said chamber flowing said silicon source gas and said dilution gas mix and while heating said support to said temperature.