# US 6,726,864 B2 · Simulated stone texture process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,864 B2
- Document ID: US6726864B2
- Status: Granted
- Kind: B2
- Application number: 10/037,189
- Filed: 2001-11-09
- Published: 2002-10-10
- Granted: 2004-04-27
- Earliest claimed: 2000-11-09
- Inventors: Moe Nasr; Kurt Kuriger
- Web page: https://patentgrep.com/patent/US6726864B2

## CPC

- B44C 3/046: {using a modelling surface, e.g. plate}
- B29C 41/06: about two or more axes
- B29C 41/22: Making multilayered or multicoloured articles
- B29C 41/46: Heating or cooling
- B44F 9/04: of stone surfaces, e.g. marble
- B29C 37/0032: {the coating being applied upon the mould surface before introducing the moulding compound, e.g. applying a gelcoat (B29C44/14 and B29C44/32 take precedence)}
- B29C 2035/1616: {using liquids}
- B29C 2035/1658: {using gas}
- B29C 2791/001: Shaping in several steps
- B29K 2105/0032: {Pigments, colouring agents or opacifiyng agents}
- B29K 2105/16: Fillers
- B44C: PRODUCING DECORATIVE EFFECTS (processes for applying liquids or other fluent materials to surfaces, in general B05D; shaping of plastics or substances in a plastic state B29C; printing processes to produce transfer pictures B41M3/12; thermographic duplication or marking methods B41M5/00); MOSAICS; TARSIA WORK (imitation of mosaic or tarsia work patterns B44F11/04); PAPERHANGING {(labels G09F; multi-step processes for making paper labels or tags B31D1/02)}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B44F: SPECIAL DESIGNS OR PICTURES
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Simulated stone texture products are obtained when specially selected materials are properly admixed and formed via rotational molding. These products are manufactured from suitable molds according to a prescribed process methodology using synthetic polymeric materials instead of stone materials. Prerequisite surface textures are produced that effectively simulate the corresponding actual stone products.

## Claims

### Claim 1

A method for manufacturing a simulated stone texture product from a plastic resin, said method comprising the steps of:
preheating in an oven a mold configured to form a suitable shape corresponding to said simulated stone product;
opening said preheated mold to provide access to its face;
coating said face of said mold with a latex glue material;
allowing said latex glue coating to set until said latex glue flashes off substantially all water contained therein, to yield a solid adhesive residue for retaining coloring pigments and texturing materials;
selecting materials to impart stone colors and textures being simulated;
applying said coloring and texturing materials to said mold face to become embedded with or integrated into said solid adhesive residue;
loading a base resin charge into said mold;
closing said charged mold;
molding said base resin charge in a temperature range of 500° F.-650° F.;
unloading said molded base resin charge from the mold;
cooling said molded base resin charge to sustain said shape of said molded product; and
removing said cooled base resin charge from a cooling jig.

### Claim 2 (depends on 1)

The method recited in claim 1, wherein said preheating step preheats said mold to an outside mold temperature in the range 500° F.-650° F.

### Claim 3 (depends on 1)

The method recited in claim 1, wherein said preheating step preheats said mold to an outside mold temperature in the range 550° F.-625° F.

### Claim 4 (depends on 1)

The method recited in claim 1, wherein said preheating step preheats said mold to an outside mold temperature of 575° F.

### Claim 5 (depends on 1)

The method recited in claim 1, wherein said mold is coated with said latex glue using an airless spray means to assure in situ retention of coloring pigments and texturing materials.

### Claim 6 (depends on 1)

The method recited in claim 1, wherein said step of applying said coloring and texturing materials to said mold face is performed using a dry shake method.

### Claim 7 (depends on 1)

The method recited in claim 1, wherein said coloring and texturing materials are in the range of 5-20% of the total weight of said base resin charge.

### Claim 8 (depends on 1)

The method recited in claim 1, wherein said base resin charge comprises linear low density polyethylene.

### Claim 9 (depends on 1)

The method recited in claim 1, wherein said molding of said base resin charge proceeds via rotational molding.

### Claim 10 (depends on 9)

The method recited in claim 9, wherein said rotational molding of said base resin charge proceeds for 18-22 minutes.

### Claim 11 (depends on 9)

The method recited in claim 9, wherein said rotational molding of said base resin charge proceeds with arm rotations set to 10-12 RPM major axis and 6-8 RPM minor axis.

### Claim 12 (depends on 1)

The method recited in claim 1, wherein said cooling of said molded base resin charge step comprises injecting cool air into said molded base resin charge.

### Claim 13 (depends on 12)

The method recited in claim 12, wherein said air cooling of said molded base resin charge step proceeds for 15-20 minutes.

### Claim 14 (depends on 13)

The method recited in claim 13, wherein said cooling of said molded base resin charge step is further comprises injecting cool water into said molded base resin charge after said injection of cool air.

### Claim 15 (depends on 14)

The method recited in claim 14, wherein said water cooling of said molded base resin charge step proceeds for 1-2 minutes.

### Claim 16 (depends on 15)

The method recited in claim 15, wherein said cooling of said molded base resin charge step further comprises injecting subsequent cool air into said molded base resin charge after said injection of cool water.

### Claim 17 (depends on 16)

The method recited in claim 16, wherein said subsequent air cooling of said molded base resin charge step proceeds for 1-2 minutes.

### Claim 18 (depends on 1)

The method recited in claim 1, wherein said step of cooling said molded base resin charge includes a foam injection step for a said simulated stone product that requires shape retention and sound deadening properties.

### Claim 19 (depends on 1)

The method recited in claim 1, wherein said preheating step comprises heating said mold to an outside mold temperature in the range 350° F.-750° F.

### Claim 20

A method for manufacturing a simulated stone texture product from a plastic resin, said method comprising the steps of:
preheating in an oven a mold configured to form a suitable shape corresponding to said simulated stone product;
opening said preheated mold to provide access to its face;
coating said face of said mold with a latex glue material;
allowing said latex glue coating to set until said latex glue flashes off substantially all water contained therein, to yield a solid adhesive residue for retaining coloring pigments and texturing materials;
selecting materials to impart stone colors and textures being simulated;
applying said coloring and texturing materials to said mold face to become embedded with or integrated into said solid adhesive residue;
closing said mold;
loading a base resin charge into said mold;
molding said base resin charge in a temperature range of 500° F.-650° F.;
unloading said molded base resin charge from the mold;
cooling said molded base resin charge to sustain said shape of said molded product; and
removing said cooled base resin charge from a cooling jig.

### Claim 21 (depends on 20)

The method recited in claim 20, wherein said preheating step preheats said mold to an outside mold temperature in the range 500° F.-650° F.

### Claim 22 (depends on 20)

The method recited in claim 20, wherein said preheating step preheats said mold to an outside mold temperature in the range 550° F.-625° F.

### Claim 23 (depends on 20)

The method recited in claim 20, wherein said preheating step preheats said mold to an outside mold temperature of 575° F.

### Claim 24 (depends on 20)

The method recited in claim 20, wherein said mold is coated with said latex glue using an airless spray means to assure in situ retention of coloring pigments and texturing materials.

### Claim 25 (depends on 20)

The method recited in claim 20, wherein said step of applying said coloring and texturing materials to said mold face is performed using a fry shake method.

### Claim 26 (depends on 20)

The method recited in claim 20, wherein said coloring and texturing materials are in the range of 5-20% of the total weight of said base resin charge.

### Claim 27 (depends on 20)

The method recited in claim 20, wherein said base resin charge comprises linear low density polyethylene.

### Claim 28 (depends on 20)

The method recited in claim 20, wherein said molding of said base resin charge proceeds via rotational molding.

### Claim 29 (depends on 28)

The method recited in claim 28, wherein said rotational molding of said base resin charge proceeds for 18-22 minutes.

### Claim 30 (depends on 28)

The method recited in claim 28, wherein said rotational molding of said base resin charge proceeds with arm rotations set to 10-12 RPM major axis and 6-8 RPM minor axis.

### Claim 31 (depends on 20)

The method recited in claim 20, wherein said cooling of said molded base resin charge step comprises injecting cool air into said molded base resin charge.

### Claim 32 (depends on 22)

The method recited in claim 22, wherein said air cooling of said molded base resin charge step proceeds for 15-20 minutes.

### Claim 33 (depends on 32)

The method recited in claim 32, wherein said cooling of said molded base resin charge step is further comprises injecting cool water into said molded base resin charge after said injection of cool air.

### Claim 34 (depends on 33)

The method recited in claim 33, wherein said water cooling of said molded base resin charge step proceeds for 1-2 minutes.

### Claim 35 (depends on 34)

The method recited in claim 34, wherein said cooling of said molded base resin charge step further comprises injecting subsequent cool air into said molded base resin charge after said injection of cool water.

### Claim 36 (depends on 35)

The method recited in claim 35, wherein said subsequent air cooling of said molded base resin charge step proceeds for 1-2 minutes.

### Claim 37 (depends on 20)

The method recited in claim 20, wherein said step of cooling said molded base resin charge includes a foam injection step for a said simulated stone product that requires shape retention and sound deadening properties.

### Claim 38 (depends on 20)

The method recited in claim 20, wherein said preheating step comprises heating said mold to an outside mold temperature in the range 350° F.-750° F.