# US 6,726,863 B2 · Thermoplastic tube

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,863 B2
- Document ID: US6726863B2
- Status: Granted
- Kind: B2
- Application number: 09/940,626
- Filed: 2001-08-29
- Published: 2002-02-21
- Granted: 2004-04-27
- Earliest claimed: 1999-03-05
- Assignees: Wavin B.V.
- Inventors: Arjan Dirk van Lenthe; Jan Hendrik Prenger; Jan Visscher
- Web page: https://patentgrep.com/patent/US6726863B2

## CPC

- B29C 55/26: biaxial
- B29C 48/09: Articles with cross-sections having partially or fully enclosed cavities, e.g. pipes or channels
- B29C 48/902: {internally}
- B29C 48/903: {externally}
- B29C 48/908: {characterised by calibrator surface, e.g. structure or holes for lubrication, cooling or venting}
- B29C 48/91: Heating, e.g. for cross linking
- B29C 48/918: {characterized by differential heating or cooling}
- B29C 48/92: Measuring, controlling or regulating
- B29C 57/04: using mechanical means {(B29C57/025 takes precedence)}
- B29C 48/0018: {combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence)}
- B29C 48/10: flexible, e.g. blown foils
- B29C 48/13: Articles with a cross-section varying in the longitudinal direction, e.g. corrugated pipes
- B29C 48/355: Conveyors for extruded articles
- B29C 48/885: External treatment, e.g. by using air rings for cooling tubular films
- B29C 48/912: {of tubular films}
- B29C 48/919: {using a bath, e.g. extruding into an open bath to coagulate or cool the material}
- B29C 2948/92209: Temperature
- B29C 2948/92438: Conveying, transporting or storage of articles
- B29C 2948/9258: Velocity
- B29C 2948/926: Flow or feed rate
- B29C 2948/92647: Thickness
- B29C 2948/92809: Particular value claimed
- B29C 2948/92904: Die; Nozzle zone
- B29C 2948/92923: Calibration, after-treatment or cooling zone
- Y10T 29/49805: Shaping by direct application of fluent pressure
- Y10T 428/13: Hollow or container type article [e.g., tube, vase, etc.]
- Y10T 428/139: Open-ended, self-supporting conduit, cylinder, or tube-type article
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for producing a tube section from thermoplastic material, in which a tube section is extruded by means of an extruder which is provided with an extruder die having an inner core, which inner core defines an axial hollow space in the tube section, the tube section coming out of the extruder die downstream of the extruder die being internally cooled by means of an internal cooling member and externally cooled by means of an external cooling device. Immediately after the tube section leaves the extruder die, the internal cooling member brings about internal cooling of the tube. The external cooling device is positioned downstream of the internal cooling member, so that the external cooling of the tube section is brought about after the internal cooling.

## Claims

### Claim 1

An improved method for producing a biaxially oriented thermoplastic tube comprising the steps of:
extruding a tubular preform having a wall thickness from thermoplastic material using an extruder having an output, the extruder is provided with an extruder die having an inner core defining a hollow space in the preform;
subjecting the preform to a temperature conditioning, so that a tempered preform is obtained having an orientation temperature which is suitable for the thermoplastic material of said preform;
forcing the tempered preform over a mandrel comprising an expansion part, which brings about an expansion in the circumferential direction of the tempered preform forced over said mandrel in such a manner that said preform is transformed into a biaxially oriented tube with thermoplastic material which is oriented in axial direction and in circumferential direction of the tube, said preform having a preform advancement speed upstream of the mandrel which is set by means of a preform speed-control means which acts on the preform upstream of the mandrel, said tube having an adjustable tube advancement speed down stream of the mandrel which is set by means of a drawing device which acts on the tube downstream of the mandrel; and
cooling said biaxially oriented tube; and
periodically changing the wall thickness of the preform by varying the ratio of the preform advancement speed and the output of the extruder with in a wide range, wherein the tube advancement speed of the tube downstream of the mandrel is varied periodically in such a manner that the ratio of the tube advancement speed to the preform advancement speed is kept substantially constant.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the tube part with greater wall thickness is subjected to a socket forming operation.

### Claim 3 (depends on 1)

A method of claim 1, wherein the ratio of the advancement speed of the preform, which is determined by the preform speed-control means, to the output of the extruder is kept substantially constant at a first value for a first period, so that the preform then acquires a first wall thickness, and is set to one or more values which differ from the first value for a second period, which is considerably shorter than the first period.

### Claim 4 (depends on 1)

The method of claim 1, wherein the output of the extruder is varied periodically and the advancement speed of the preform, which is determined by the speed-control means, is kept substantially constant.

### Claim 5 (depends on 1)

The method of claim 1, wherein the output of the extruder is kept substantially constant and the advancement speed of the preform, which is determined by the speed-control means, is varied periodically.

### Claim 6 (depends on 1)

The method of claim 1, wherein the biaxially oriented tube downstream of the expansion part of the mandrel is cooled in such a manner that the cooled tube does not undergo any further axial stretching and the generation of the axial orientation is concentrated in a section between a speed-control means for the preform and a downstream end of the mandrel.

### Claim 7 (depends on 1)

The method of claim 1, wherein the biaxially oriented tube downstream of the expansion part of the mandrel is cooled in such a manner that the cooled tube does not undergo any further axial stretching and the generation of the axial orientation is concentrated in a section between a plurality of preform speed-control means for the preform which are arranged upstream of the mandrel.

### Claim 8 (depends on 1)

A method according to claim 1, in which the preform downstream of the extruder die is subjected to calibration of the external diameter of the preform, so that the preform acquires a uniform external diameter and a preform section with a greater wall thickness has a smaller internal diameter than the adjoining parts of the preform with a smaller wall thickness.

### Claim 9 (depends on 1)

The method of claim 1, wherein the preform downstream of the extruder die is subjected to calibration of the internal diameter of the preform, so that the preform acquires a uniform internal diameter and a preform part with a greater wall thickness has a greater external diameter than the adjoining parts of the preform with a smaller wall thickness.

### Claim 10 (depends on 1)

The method of claim 1, wherein the preform is tempered such that a preform part with a larger wall thickness on average is at a higher temperature, measured at a location immediately upstream of the expansion mandrel, than an immediately adjoining downstream preform part with a smaller wall thickness which is already on the mandrel.

### Claim 11 (depends on 1)

The method of claim 1, wherein a series of a plurality of parts with a larger wall thickness which are located relatively close together is created in the preform, followed by a considerably longer preform section with a uniform, smaller wall thickness.

### Claim 12 (depends on 1)

The method of claim 1, wherein the biaxially oriented tube, in a section between the downstream end of the mandrel and the drawing device, is subjected to calibration of the external diameter of the tube.

### Claim 13 (depends on 1)

The method of claim 1, wherein the biaxially oriented tube downstream of the drawing device is divided at or next to a tube part with a larger wall thickness, so that tube sections are obtained which at one or both axial ends have an end part with a greater wall thickness than the remainder of the tube section, which has a uniform, smaller wall thickness.

### Claim 14

An improved method for producing a biaxial oriented thermoplastic tube comprising the steps of
extruding a tubular preform having a wall thickness from thermoplastic material using an extruder having an output, the extruder is provided with an extruder die having an inner core defining a hollow space in the preform;
subjecting the preform to a temperature conditioning, so that a tempered preform is obtained having an orientation temperature which is suitable for the thermoplastic material of said preform;
forcing the tempered preform over a mandrel comprising an expansion part, which brings about an expansion in the circumferential direction of the tempered preform forced over said mandrel in such a manner that said preform is transformed into a biaxially oriented tube with thermoplastic material which is oriented in axial direction and in circumferential direction of the tube, said preform having a preform advancement speed upstream of the mandrel which is set by means of a preform speed-control means which acts on the preform upstream of the mandrel, said tube having an adjustable tube advancement speed down stream of the mandrel which is set by means of a drawing device which acts on the tube downstream of the mandrel; and
cooling said biaxially oriented tube; and
periodically changing the wall thickness of the preform by varying the ratio of the preform advancement speed and the output of the extruder with in a wide range, wherein the ratio of the preform advancement speed to the output of the extruder is kept substantially constant at a first value for a first period, so that the preform acquires a first wall thickness, and is the set to one or more values which differ from the first value for a second period, which is considerably shorter than the first period, and in which, in a period during which a part of the preform with a wall thickness which is greater than the first wall thickness is being forced over the mandrel or for part of this period, the ratio of the tube advancement speed to the preform advancement speed is greater in a period during which a part of the preform with the first wall thickness is being forced over the mandrel, in such a manner that a tube part with the greater wall thickness acquires a greater axial stretching than a tube part with the first wall thickness.

### Claim 15

An improved method for producing a biaxial oriented thermoplastic tube comprising the steps of
extruding a tubular preform having a wall thickness from thermoplastic material using an extruder having an output, the extruder is provided with an extruder die having an inner core defining a hollow space in the preform;
subjecting the preform to a temperature conditioning, so that a tempered preform is obtained having an orientation temperature which is suitable for the thermoplastic material of said preform;
forcing the tempered preform over a mandrel comprising an expansion part, which brings about an expansion in the circumferential direction of the tempered preform forced over said mandrel in such a manner that said preform is transformed into a biaxially oriented tube with thermoplastic material which is oriented in axial direction and in circumferential direction of the tube, said preform having a preform advancement speed upstream of the mandrel which is set by means of a preform speed-control means which acts on the preform upstream of the mandrel, said tube having an adjustable tube advancement speed down stream of the mandrel which is set by means of a drawing device which acts on the tube downstream of the mandrel; and
cooling said biaxially oriented tube; and
periodically changing the wall thickness of the preform by varying the ratio of the preform advancement speed to the output of the extruder with in a wide range, wherein the preform is tempered such that a preform part with a larger wall thickness on average is at a higher temperature, measured at a location immediately upstream of the expansion mandrel, than an immediately adjoining downstream preform part with a smaller wall thickness which is already on the mandrel.