# US 6,726,807 B1 · Multi-phase calcium silicate hydrates, methods for their preparation, and improved paper and pigment products produced therewith

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,807 B1
- Document ID: US6726807B1
- Status: Granted
- Kind: B1
- Application number: 09/649,413
- Filed: 2000-08-26
- Granted: 2004-04-27
- Earliest claimed: 1999-08-26
- Assignees: G.R. International, Inc. (A Washington Corporation)
- Inventors: Vijay K. Mathur
- Web page: https://patentgrep.com/patent/US6726807B1

## CPC

- D21H 21/285: {insoluble}
- D21H 17/68: siliceous, e.g. clays
- D21H 19/40: siliceous, e.g. clays
- D21H 19/54: Starch
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

A method for the hydrothermal preparation of calcium silicate hydrates. Multi-phase calcium silicate hydrates, having unique physical and chemical properties, are prepared by hydrothermal reaction of specified ratios of CaO and SiO2, normally starting from slurries of slaked lime and from fluxed calcined diatomaceous earth, each of which is at about the atmospheric boiling point before being mixed and charged to a reactor, and pressurized. The hydrothermal reaction is carried out while maintaining the initial dilution for a preselected reaction time at a preselected reaction temperature. The calcium silicate hydrates produced have high water absorption and light scattering power, and have optical and physical properties making them highly desirable as a filler substitute in papermaking.

## Claims

### Claim 1

A method for improving opacity of paper, said paper manufactured by drying a furnish mixture of an aqueous pulp slurry and at least one preselected filler, said method comprising incorporating into said furnish mixture a preselected filler comprising a multiple phase calcium silicate hydrate comprising a major component comprised of foshagite, and a minor component of xenotlite, said multiple phase mixture
(a) having an x-ray diffraction pattern substantially as set forth in Table 1c of the specification, and
(b) a fibrous crystalline structure comprising (i) foshagite having (A) a diameter of less than about 0.2 microns, and (B) a length greater than about 1 micron, and (ii) xenotlite particles having (A) a diameter of less than about 0.3 microns, and (B) a length of greater than about 1 micron.

### Claim 2 (depends on 1)

The method as set forth in claim 1, wherein said multiple phases calcium silicate hydrate comprises a plurality of stable secondary particles, said stable secondary particles comprising an interlocking structure of primary fibrous crystals.

### Claim 3 (depends on 2)

The method as set forth in claim 2, wherein said stable secondary particles comprise a porous haystack like structure of median diameter from about 10 to about 40 microns.

### Claim 4 (depends on 1)

The method as set froth in claim 1, wherein in said multiple phase calcium silicate hydrate has a water absorption characteristic of at least 400 percent by weight.

### Claim 5 (depends on 1)

The method as set forth in claim 1, wherein said multiple phase calcium silicate hydrate has a water absorption characteristic of at least 800 percent by weight.

### Claim 6 (depends on 1)

The method as set forth in claim 1, wherein said multiple phase calcium silicate hydrate has a water absorption characteristic of from about 500 percent to about 1000 percent by weight.

### Claim 7 (depends on 1)

The method as set forth in claim 1, wherein the percentage of foshagite is at least seventy (70) percent.

### Claim 8 (depends on 1)

The method as set forth in claim 1, wherein the percentage of foshagite is at least eighty (80) percent.

### Claim 9 (depends on 1)

The method as set forth in claim 1, wherein the percentage of foshagite is at least ninety (90) percent.

### Claim 10 (depends on 1)

The method as set forth in claim 1, wherein said foshagite has a diameter from about 0.1 to about 0.2 microns.

### Claim 11 (depends on 1)

The method as set forth in claim 1, wherein said foshagite has a length from about 1 micron to about 5 microns.

### Claim 12 (depends on 1)

The method as set forth in claim 1, wherein said xenotlite particles have a diameter from about 0.1 to about 0.3 microns.

### Claim 13 (depends on 1)

The method as set forth in claim 1, wherein said xenotlite particles have a length of from about 1 microns to about 3 microns.

### Claim 14 (depends on 1, 3)

The method as set forth in claim 1, or in claim 3, wherein said multiple phase calcium silicate hydrate comprises a hydrothermal reaction product of an aqueous suspension of lime and a siliceous material in a CaO to SiO2 mole ratio of between 1.2 to 1 and about 1.7 to 1.

### Claim 15 (depends on 1, 3)

The method as set forth in claim 1 or in claim 3, wherein said multiple phase calcium silicate hydrate comprises a hydrothermal reaction product of an aqueous suspension of lime and a siliceous material in a CaO to SiO2 mole ratio of about 1.35 to 1.

### Claim 16 (depends on 1, 3)

The method as set forth in claim 1 or in claim 3, wherein said paper has a Gurley porosity, and wherein addition of said multiple phase calcium silicate hydrate to said furnish simultaneously increases said Gurley porosity and said opacity.

### Claim 17 (depends on 16)

The method as set forth in claim 16, wherein said paper has a bulk, and wherein addition of said multiple phase calcium silicate hydrate to said furnish simultaneously increases said bulk with said opacity.

### Claim 18 (depends on 16)

The method as set forth in claim 16, wherein said paper has a measurable smoothness, and wherein addition of said multiple phase calcium silicate hydrate to said furnish simultaneously increases (a) said measurable smoothness, (b)said bulk, (c) said opacity, and said porosity.

### Claim 19 (depends on 17)

The method as set forth in claim 17, wherein said paper has a measurable print show through, and wherein addition of said multiple phase calcium silicate hydrate to said furnish (a) decreases measurable print show throw, and (b) increases (i) said measurable smoothness, (ii) said bulk, and (iii) said opacity.

### Claim 20 (depends on 17)

The method as set forth in claim 17, wherein said paper has a measurable sheet stiffness, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases measurable sheet stiffness.

### Claim 21 (depends on 1)

The method as set forth in claim 1, wherein said paper has a brightness, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases said brightness.

### Claim 22 (depends on 1)

The method as set forth in claim 1, wherein said paper has a sheet scattering coefficient, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases said sheet scattering coefficient.

### Claim 23 (depends on 17)

The method as set forth in claim 17, wherein said paper has a sheet tensile index, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases said sheet tensile index.

### Claim 24

A method for improving opacity of paper, said paper manufactured by drying a furnish mixture of an aqueous pulp slurry and at least one preselected filler, said method comprising incorporating into said furnish mixture a preselected filler comprising a multiple phase calcium silicate hydrate comprising a major component comprised of foshagite, and a minor component of xenotlite, said multiple phase mixture
(a) having an x-ray diffraction pattern substantially as set forth in Table 1c of the specification, and
(b) a fibrous crystalline structure comprising (i) foshagite having (A) a diameter of less than about 0.2 microns, and (B) a length greater than about 1 micron, and (ii) xenotlite particles having (A) a diameter of less than about 0.3 microns, and (B) a length of greater than about 1 micron;
(c) a plurality of stable secondary particles, said stable secondary particles comprising an interlocking structure of primary fibrous crystals, wherein said stable secondary particles comprise a porous haystack like structure of median diameter from about 10 to about 40 microns.

### Claim 25 (depends on 24)

The method as set forth in claim 24, wherein
(a) said paper has a Gurley porosity, and wherein addition of said multiple phase calcium silicate hydrate to said furnish simultaneously increases said Gurley porosity and said opacity; and
(b) said paper has a bulk, and wherein addition of said multiple phase calcium silicate hydrate to said furnish simultaneously increases said bulk with said opacity;
(c) said paper has a measurable smoothness, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases said measurable smoothness; and
(d) said paper has a measurable print show through, and wherein addition of said multiple phase calcium silicate hydrate to said furnish decreases measurable print show through; and
(e) said paper has a measurable sheet stiffness, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases measurable sheet stiffness; and
(f) said paper has a brightness, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases said brightness; and
(g) said paper has a sheet scattering coefficient, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases said sheet scattering coefficient;
(h) said paper has a sheet tensile index, and wherein addition of said multiple phase calcium silicate hydrate to said furnish increases said sheet tensile index.

### Claim 26 (depends on 1, 25)

The method as set forth in claim 1 or in claim 25, wherein said calcium silicate hydrate has an ISO brightness from about 94 to about 97.

### Claim 27

A method for improving sheet stiffness of paper, said paper manufactured by drying a furnish mixture of an aqueous pulp slurry and preselected fillers, said method comprising incorporating into said furnish mixture a multiple phase calcium silicate hydrate comprising a major component comprised of riversideite, and a minor component of xenotlite, said multiple phase mixture having
(a) an x-ray diffraction pattern substantially as set forth in Table 2c of the specification, and
(b) an irregular globular structure having an outside diameter from about 10 to about 30 microns.

### Claim 28 (depends on 27)

The method as set forth in claim 27, wherein in said multiple phase calcium silicate hydrate has a water absorption characteristic of at least 250 percent.

### Claim 29 (depends on 27)

The method as set forth in claim 27, wherein said multiple phase calcium silicate hydrate has a water absorption characteristic of between 200 and 500 percent.

### Claim 30 (depends on 27)

The method as set forth in claim 27, wherein said paper has a measurable stiffness and a measurable bulk, and wherein in said measurable stiffness is simultaneously increased along with said bulk.

### Claim 31 (depends on 27)

The method as set forth in claim 27, wherein said paper has a measurable print show through, and wherein in measurable print show through is decreased while simultaneously increasing bulk and stiffness.