# US 6,726,787 B2 · Process for making a work piece having a major phase of α from a titanium alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,787 B2
- Document ID: US6726787B2
- Status: Granted
- Kind: B2
- Application number: 10/327,992
- Filed: 2002-12-26
- Published: 2003-05-22
- Granted: 2004-04-27
- Earliest claimed: 1999-01-07
- Assignees: Jiin-Huey Chern Lin; Chien-Ping Ju
- Inventors: Jiin-Huey Chern Lin; Chien-Ping Ju; Chih-Min Lee
- Web page: https://patentgrep.com/patent/US6726787B2

## CPC

- C22C 14/00: Alloys based on titanium
- A61L 27/06: Titanium or titanium alloys
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)

## Abstract

Quenching a work piece made of a titanium alloy having a temperature higher than 800° C. to a temperature lower than 500° C. at a cooling rate greater than 10° C./second between 800° C. and 500° C. is used to render the cooled work piece containing α″ phase as a major phase. The titanium alloy composition contains at least one isomorphous beta stabilizing element selected from Mo, Nb, Ta and W; and the balance Ti, wherein said composition has a Mo equivalent value from about 6 to about 9. The work piece is preferably a medical device.

## Claims

### Claim 1

A process for making a work piece having an α″ phase as a major phase from a titanium alloy composition comprising the following steps:
a) preparing a titanium alloy composition comprising at least one isomorphous beta stabilizing element selected from the group consisting of Mo, Nb, Ta and W; and the balance Ti, wherein said composition has a Mo equivalent value from about 6 to about 9;
b) fast cooling said composition having a temperature higher than 800° C. to a temperature lower than 500° C. at a cooling rate greater than 10° C./second between 800-500° C., so that the resulting cooled composition contains an α″ phase as a major phase.

### Claim 2 (depends on 1)

The process according to claim 1, wherein said titanium alloy composition in step a) is substantially free from an eutectoid beta stabilizing element selected from the group consisting of Fe, Mn, Cr, Co, and Ni.

### Claim 3 (depends on 1)

The process according to claim 1, wherein said titanium alloy composition in step a) is substantially free from Al.

### Claim 4 (depends on 1)

The process according to claim 1, wherein said titanium alloy composition in step a) is substantially free from V.

### Claim 5 (depends on 1)

The process according to claim 1, wherein said titanium alloy composition in step a) consists essentially of at least one isomorphous beta stabilizing element selected from the group consisting of Mo, Nb, Ta and W; and the balance Ti.

### Claim 6 (depends on 1)

The process according to claim 1, wherein said cooling rate in step b) is greater than 20° C./sec.

### Claim 7 (depends on 6)

The process according to claim 6, wherein said fast cooling comprises water quenching.

### Claim 8 (depends on 1)

The process according to claim 1, wherein said composition has a temperature of 800-1200° C. before said fast coolig in step b).

### Claim 9 (depends on 1)

The process according to claim 1, wherein said preparing in step a) comprises casting said titanium alloy composition to form a work piece having a temperature higher than 800° C., and said fast cooling in step b) comprises fast cooling said work piece having a temperature higher than 800° C.

### Claim 10 (depends on 1)

The process according to claim 1, wherein said preparing in step a) comprises metal working said titanium alloy composition to form a work piece, and heating the resulting work piece to a temperature higher than 800° C., and said fast cooling in step b) comprises fast cooling said work piece having a temperature higher than 800° C.

### Claim 11 (depends on 1)

The process according to claim 1, wherein said titanium alloy composition in step a) further comprises one or more incidental impurities selected from the group consisting of carbon, oxygen and nitrogen, wherein a total amount of said one or more incidental impurities is less than 1 wt %.

### Claim 12 (depends on 1)

The process according to claim 1, wherein said work piece having a major phase of α″ is a medical device.