# US 6,726,785 B2 · Aluminum alloy sheet material and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,785 B2
- Document ID: US6726785B2
- Status: Granted
- Kind: B2
- Application number: 10/151,062
- Filed: 2002-05-16
- Published: 2003-01-09
- Granted: 2004-04-27
- Earliest claimed: 2001-05-17
- Assignees: Furukawa Electric Co., Ltd.; Honda Giken Kogyo Kabushiki Kaisha
- Inventors: Koji Oyama; Yoichiro Bekki; Noboru Hayashi; Morio Kuroki
- Web page: https://patentgrep.com/patent/US6726785B2

## CPC

- C22C 21/02: with silicon as the next major constituent
- C22F 1/043: of alloys with silicon as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

An aluminum alloy sheet material, containing 2.6% by mass or more and less than 3.5% by mass (% by mass is simply denoted by % hereinafter) of Si, 0.05 to 0.5% of Mg, 0.5% or more and less than 1.2% of Cu, 0.6 to 1.5% of Mn, 0.5 to 1.6% of Zn, and 0.3 to 2.0% of Fe, and containing, if necessary, at least one of 0.01 to 0.2% of Cr, 0.01 to 0.2% of Zr, 0.01 to 0.2% of V, and 0.01 to 0.2% of Ti, with the balance of Al and unavoidable impurities. A method of producing the aluminum alloy sheet material, which method contains carrying out specific workings.

## Claims

### Claim 1

An aluminum alloy sheet material, consisting of 2.6% by mass or more and less than 3.5% by mass (% by mass is simply denoted by % hereinafter) of Si, 0.05 to 0.5% of Mg, 0.5% or more and less than 1.2% of Cu, 0.6 to 1.5% of Mn, 0.5 to 1.6% of Zn, and 0.3 to 2.0% of Fe, with the balance of Al and unavoidable impurities, and wherein the 0.2% proof stress is 100 MPa or less.

### Claim 2 (depends on 1)

The aluminum alloy sheet material according to claim 1, further containing a component originating from scraps of an aluminum alloy in at least a part of the sheet material.

### Claim 3 (depends on 1)

The aluminum alloy sheet material according to claim 1, wherein concentrations of Si, Mn and Fe, when they are represented by A%, B% and C%, respectively, satisfy conditions as shown by the following formula:
(0.015×A+0.15×B+0.03×C)≦0.445, and
wherein a density of precipitates with an average diameter of 100 μm or more is 2 precipitates/cm2 or less.

### Claim 4 (depends on 1)

The aluminum alloy sheet material according to claim 1, wherein tensile strength and 0.2% proof stress, when they are represented by T (MPa) and Y (MPa), respectively, satisfy conditions as shown by the following formula:
T2/Y≧350.

### Claim 5 (depends on 1)

The aluminum alloy sheet material according to claim 1, wherein 0.2% proof stress after baking of a coating is higher by 30 MPa or more than 0.2% proof stress before baking.

### Claim 6

An aluminum alloy sheet material, comprising 2.6% by mass or more and less than 3.5% by mass of Si, 0.05 to 0.5% of Mg, 0.5% or more and less than 1.2% of Cu, 0.6 to 1.5% of Mn, 0.5 to 1.6% of Zn, and 0.3 to 2.0% of Fe, and comprising at least one selected from the group consisting of 0.01 to 0.2% of Cr, 0.01 to 0.2% of Zr, 0.01 to 0.2% of V, and 0.01 to 0.2% of Ti, with the balance of Al and unavoidable impurities, and wherein said aluminum alloy sheet material has been heat treated to have a 0.2% proof stress is 100 Mpa or less.

### Claim 7 (depends on 6)

The aluminum alloy sheet material according to claim 6, further containing a component originating from scraps of an aluminum alloy in at least a part of the sheet material.

### Claim 8 (depends on 6)

The aluminum alloy sheet material according to claim 6, wherein concentrations of Si, Mn, Fe, Cr, Zr and Ti, when they are represented by A%, B%, C%, D%, E% and F%, respectively, satisfy conditions as shown by the following formula:
{0.015×A+0.15×B+0.03×C+0.60×(D+E)+0.50×F}≦0.445, and
wherein a density of precipitates with an average diameter of 100 μm or more is 2 precipitates/cm2 or less.

### Claim 9 (depends on 6)

The aluminum alloy sheet material according to claim 6, wherein tensile strength and 0.2% proof stress, when they are represented by T (MPa) and Y (MPa), respectively, satisfy conditions as shown by the following formula:
T2/Y≧350.

### Claim 10 (depends on 6)

The aluminum alloy sheet material according to claim 6, wherein 0.2% proof stress after baking of a coating is higher by 30 MPa or more than 0.2% proof stress before baking.

### Claim 11

An aluminum alloy sheet material, consisting essentially of 2.6% by mass or more and less than 3.5% by mass of Si, 0.05 to 0.5% of Mg, 0.5% or more and less than 1.2% of Cu, 0.6 to 1.5% of Mn, 0.5 to 1.6% of Zn, 0.3 to 2.0% of Fe, and at least one selected from the group consisting of 0.01 to 0.2% of Cr, 0.01 to 0.2% of Zr, 0.01 to 0.2% of V, and 0.01 to 0.2% of Ti, with the balance of Al and unavoidable impurities,
wherein concentrations of Si, Mn, Fe, Cr, Zr and Ti, when they are represented by A%, B%, C%, D%, E% and F%, respectively, satisfy conditions as shown by the following formula:
{0.015×A+0.15×B+0.03×C+0.60×(D+E)+0.50×F}≦0.445, and
wherein a density of precipitates with an average diameter of 100 μm or more is 2 precipitates/cm2 or less,
wherein 0.2% proof stress is 100 MPa or less, and
wherein the aluminum alloy sheet material is for use in automobiles.

### Claim 12 (depends on 11)

The aluminum alloy sheet material according to claim 11, further containing a component originating from scraps of an aluminum alloy in at least a part of the sheet material.

### Claim 13 (depends on 11)

The aluminum alloy sheet material according to claim 11, wherein 0.2% proof stress after baking of a coating is higher by 30 MPa or more than 0.2% proof stress before baking.

### Claim 14 (depends on 11)

The aluminum alloy sheet material according to claim 11, wherein the scraps of an aluminum alloy are scraps of aluminum castings.

### Claim 15 (depends on 11)

An automobile material, which is prepared from the aluminum sheet materials according to claim 11.

### Claim 16 (depends on 11)

The sheet material of claim 11, wherein the forming height by stretch forming is 12 mm or more and less than 14 mm.

### Claim 17

An aluminum alloy sheet material, comprising 2.6% by mass or more and less than 3.5% by mass of Si, 0.05 to 0.5% of Mg, 0.5% or more and less than 1.2% of Cu, 0.6 to 1.5% of Mn, 0.5 to 1.6% of Zn, and 0.3 to 2.0% of Fe, with the balance of Al and unavoidable impurities,
wherein concentrations of Si, Mn and Fe, when they are represented by A%, B% and C%, respectively, satisfy conditions as shown by the following formula:
(0.015×A+0.15×B+0.03×C)≦0.445,
wherein a density of precipitates with an average diameter of 100 μm or more is 2 precipitates/cm2 or less,
wherein 0.2% proof stress is 100 MPa or less, and
wherein the aluminum alloy sheet material is for use in automobiles.

### Claim 18 (depends on 17)

A The aluminum alloy sheet material according to claim 17, wherein tensile strength and 0.2% proof stress, when they are represented by T (MPa) and Y (MPa), respectively, satisfy conditions as shown by the following formula:
T2/Y≧350.

### Claim 19 (depends on 17)

The sheet material of claim 17, wherein the forming height by stretch forming is 12 mm or more and less than 14 mm.

### Claim 20

An aluminum alloy sheet material, consisting of 2.6% by mass or more and less than 3.5% by mass (% by mass is simply denoted by % hereinafter) of Si, 0.05 to 0.5% of Mg, 0.5% or more and less than 1.2% of Cu, 0.6 to 1.5% of Mn, 0.5 to 1.6% of Zn, and 0.3 to 2.0% of Fe, with the balance of Al and unavoidable impurities,
wherein the 0.2% proof stress is 100 MPa or less;
wherein concentrations of Si, Mn and Fe, when they are represented by A%, B% and C%, respectively, satisfy conditions as shown by the following formula:
(0.015×A+0.15×B+0.03×C)≦0.445, and
wherein a density of precipitates with an average diameter of 100 μm or more is 2 precipitates/cm2 or less;
wherein tensile strength and 0.2% proof stress, when they are represented by T (MPa) and Y (MPa), respectively, satisfy conditions as shown by the following formula:
T2/Y≧350; and
wherein a forming height by stretch forming is 14 to 15 mm.