# US 6,726,784 B2 · α+β type titanium alloy, process for producing titanium alloy, process for coil rolling, and process for producing cold-rolled coil of titanium alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,784 B2
- Document ID: US6726784B2
- Status: Granted
- Kind: B2
- Application number: 10/243,793
- Filed: 2002-09-16
- Published: 2003-05-15
- Granted: 2004-04-27
- Earliest claimed: 1998-05-26
- Inventors: Hideto Oyama; Takayuki Kida; Kazumi Furutani; Masamitsu Fujii
- Web page: https://patentgrep.com/patent/US6726784B2

## CPC

- C22C 14/00: Alloys based on titanium
- C22F 1/183: {of titanium or alloys based thereon}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A high strength and ductility α+β type titanium alloy, comprising at least one is isomorphous β stabilizing element in a Mo equivalence of 2.0-4.5 mass %, at least one eutectic β stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15% mass, and has a β transformation temperature no lower than 940° C.

## Claims

### Claim 1

An α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %, at least one eutectic n-stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15 mass %, and has a β transformation temperature no lower than 940° C.

### Claim 2 (depends on 1)

The α+β titanium alloy according to claim 1, wherein an Al equivalence is more than 3 mass % and less than 6.5 mass %.

### Claim 3 (depends on 2)

The α+β titanium alloy according to claim 2, wherein those elements of Al equivalence are entirely Al.

### Claim 4 (depends on 1)

The α+β titanium alloy according to claim 1, which substantially contains Mo in an amount of 1.0-3.0 mass %, V in an amount of 1.0-2.0 mass %, Fe in an amount of 0.3-1.0 mass %, Al in an amount of 3.5-5.5 mass %, Si in an amount of 0.2-0.5 mass %, and C in an amount of 0.02-0.15 mass %, with the remainder being Ti and inevitable impurities.

### Claim 5

An α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %. at least one eutectic β-stabilizing element in an Fe equivalence of 0.3-2.0 mass %. Si in an amount of 0.1-1.5 mass %. and C in an amount of 0.01-0.15 mass %. wherein the alloy contains O as an additional element such that the amount of Mo-equivalence, the amount of Fe-equivalence, and the content of O satisfy the following inequality [1]:
7.0 mass %≦(Mo-equivalence+2.5×Fe-equivalence+40×O mass %)≦19 mass % [1].

### Claim 6 (depends on 5)

The α+β titanium alloy according to claim 5, wherein an Al equivalence is more than 3 mass % and less than 6.5 mass %.

### Claim 7 (depends on 5)

The α+β titanium alloy according to claim 5, which substantially contains Mo in an amount of 1.0-3.0 mass %, V in an amount of 1.0-2.0 mass %, Fe in an amount of 0.3-1.0 mass %, Al in an amount of 3.5-5.5 mass %, Si in an amount of 0.2-0.5 mass %, and C in an amount of 0.02-0.15 mass %, with the remainder being Ti and inevitable impurities.

### Claim 8

An α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %. at least one eutectic β-stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15 mass %, wherein the alloy further contains a platinum group element in an amount of 0.03-0.2 mass %.

### Claim 9 (depends on 8)

The α+β titanium alloy according to claim 8, wherein an Al equivalence is more than 3 mass % and less than 6.5 mass %.

### Claim 10 (depends on 8)

The α+β titanium alloy according to claim 8, which substantially contains Mo in an amount of 1.0-3.0 mass %, V in an amount of 1.0-2.0 mass %, Fe in an amount of 0.3-1.0 mass %, Al in an amount of 3.5-5.5 mass %, Si in an amount of 0.2-0.5 mass %, and C in an amount of 0.02-0.15 mass %, with the remainder being Ti and inevitable impurities.

### Claim 11

A process for rolling an α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %. at least one eutectic β-stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15 mass %, said process comprising:
annealing the titanium alloy at a temperature (T2) which satisfies the following inequality [3]
[β-transus−270° C.]≦T2≦(β-transus−50° C.) [3]:
and then rolling the annealed titanium alloy.

### Claim 12 (depends on 11)

The process for rolling to produce a coil according to claim 11, wherein rolling is carried out under a tension of 49-392 MPa such that the draft is no lower than 20%.

### Claim 13 (depends on 11)

The process for rolling to produce a coil according to claim 11, wherein rolling is repeated more than once, with annealing in the α+β region intervening between consecutive rolling steps.

### Claim 14

A process for annealing a cold-rolled coil of an α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %, at least one eutectic β-stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15 mass %, characterized in that the heating temperature for annealing is higher than the temperature at which work hardening due to cold-rolling is relieved and lower than the β transus but excludes the temperature range in which a alloy of brittle hexagonal crystals emerges, thereby improving the elongation in the transverse direction of the rolled strip of the titanium alloy.

### Claim 15 (depends on 2, 3, 4, 5, 6, 7, 8)

A process for hot-rolling the titanium alloy of any one of claims 2 to 8 said process comprising:
heating the titanium alloy at a temperature (T1) which satisfies the following inequality [2]:
[β-transus−20° C.−(770×C mass %)° C.]≦T1<β-transus [2];
and then rolling the heated titanium alloy.

### Claim 16 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

A process for annealing a cold-rolled coil of the titanium alloy of any one of claims 1 to 10, characterized in that the heating temperature for annealing is higher than the temperature at which work hardening due to cold-rolling is relieved and lower than the β transus but excludes the temperature range in which α alloy of brittle hexagonal crystals emerges, thereby improving the elongation in the transverse direction of the rolled strip of the titanium alloy.

### Claim 17 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

A process of annealing a coil cold-rolled strip of the titanium alloy of any one of claims 1 to 10, wherein annealing is carried out at the temperature (T3) which satisfies the following inequality [4]:
(β-transus−130° C.)≦T3≦(β-transus−15° C.) [4],
so as to give a coil rolled titanium alloy strip superior in bending properties.

### Claim 18 (depends on 4, 7)

A process of annealing a coil cold-rolled strip of the titanium alloy of claim 4, 7, or 9, wherein annealing is carried out at a temperature no lower than 850° C. and no higher than 963 ° C. so as to give a coil rolled titanium alloy strip superior in bending properties.