# US 6,726,781 B2 · High temperature permanent magnets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,781 B2
- Document ID: US6726781B2
- Status: Granted
- Kind: B2
- Application number: 10/241,895
- Filed: 2002-09-12
- Published: 2003-02-27
- Granted: 2004-04-27
- Earliest claimed: 1999-01-06
- Assignees: University of Dayton; Electron Energy Corporation
- Inventors: Marlin S. Walmer; Christina H. Chen; Shiqiang Liu; Michael H. Walmer; G. Edward Kuhl
- Web page: https://patentgrep.com/patent/US6726781B2

## CPC

- H01F 1/055: and magnetic transition metals, e.g. SmCo5
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A permanent magnet is provided which retains its magnetic properties and exhibits a linear extrinsic demagnetization curve at elevated temperatures up to 700° C. The magnet is represented by the general formula RE(CoWFeVCuXTY)Z, where RE is a rare earth metal selected from the group consisting of Sm, Gd, Pr, Nd, Dy, Ce, Ho, Er, La, Y, Tb, and mixtures thereof and T represents a transition metal(s) selected from the group consisting of Zr, Hf, Ti, Mn, Cr, Nb, Mo, W, V, Ni, Ta, and mixtures thereof.

## Claims

### Claim 1

A permanent magnet represented by the general formula RE(CowFevCuxTy)Z where RE is a rare earth element selected from the group consisting of Sm, Gd, Pr, Nd, Dy, Ce, Ho, Er, La, Y, Tb and mixtures thereof, and T is a transition metal selected from the group consisting of Zr, Hf, Ti, Mn, Cr, Nb, Mo, W, V, Ni, Ta, and mixtures thereof; said magnet exhibiting a substantially linear extrinsic demagnetization curve at a maximum operating temperature TM of between about 340° C. to about 700° C.

### Claim 2 (depends on 1)

The permanent magnet of claim 1 wherein z is between about 6.5 and about 8.0, w is between about 0.50 and about 0.85, v is between 0.0 and about 0.35, x is between about 0.05 and about 0.20, and y is between about 0.01 and about 0.05.

### Claim 3 (depends on 1)

The permanent magnet of claim 1 wherein the sum of w, v, x and y is 1 and z has a value between about 6.5 and about 8.0.

### Claim 4 (depends on 1)

The permanent magnet of claim 1 having a temperature coefficient of intrinsic coercivity of between 0.30%/° C. and −0.30%/° C.

### Claim 5 (depends on 1)

The permanent magnet of claim 1 wherein said substantially linear extrinsic demagnetization curve has a slope between 1.00 and 1.25.

### Claim 6 (depends on 1)

The permanent magnet of claim 1 comprising from between about 22.5% and about 35.0% by weight samarium, between about 42% and about 65% by weight cobalt, between 0.0% and about 25% by weight iron, between about 2.0% and about 17.0% by weight copper, and between about 1.0% and about 5.0% by weight zirconium.

### Claim 7 (depends on 1)

The permanent magnet of claim 1 comprising from between about 23.5% and about 28.0% by weight samarium, from between about 50% and about 60% by weight cobalt, from between about 4.0% and about 16% by weight iron, from between about 7.0% and about 12% by weight copper, and from between about 2.0% and about 4.0% by weight T.

### Claim 8 (depends on 1)

The permanent magnet of claim 1 having a temperature coefficient of residual induction Br of between +0.02%/° C. to −0.040%/° C.

### Claim 9 (depends on 1)

The permanent magnet of claim 1 comprising about 24.7% by weight Sm, about 57.8% by weight Co, about 7.0% by weight Fe, about 7.1% by weight Cu, and 3.4% by weight Zr+Nb.

### Claim 10 (depends on 1)

The permanent magnet of claim 1 comprising about 26% by weight Sm, about 59.5% by weight Co, about 3.3% by weight Fe, 7.6% Cu, and 3.6% by weight Zr+Nb.

### Claim 11 (depends on 1)

The permanent magnet of claim 1 comprising about 26% by weight Sm, about 61.0% by weight Co, about 1.0% by weight Fe, about 8.2% by weight Cu, and about 3.8% by weight Zr+Nb.

### Claim 12 (depends on 1)

The permanent magnet of claim 1 having a cell size of ≦100 nm.

### Claim 13

A permanent magnet represented by the general formula RE(CowFevCuxTy)Z, where RE is a rare earth element selected from the group consisting of Sm, Gd, Pr, Nd, Dy, Ce, Ho, Er, La, Y, Tb, and mixtures thereof, T is a transition metal selected from the group consisting of Zr, Hf, Ti, Mn, Cr, Nb, Mo, W, V, Ni, Ta, and mixtures thereof, z is between about 6.5 and about 8.0, w is between about 0.50 and about 0.85, v is between 0.0 and about 0.35, x is between about 0.05 and about 0.20, and y is between about 0.01 and about 0.05.

### Claim 14

A permanent magnet represented by the general formula RE(CowFevCuxTy)Z wherein the sum of w, v, x and y is 1; z has a value between about 6.5 and about 8.0, RE is a rare earth element selected from the group consisting of Sm, Gd, Pr, Nd, Dy, Ce, Ho, Er, La, Y, Tb, and mixtures thereof, and T is a transition metal selected from the group consisting of Zr, Hf, Ti, Mn, Cr, Nb, Mo, W, V, Ni, Ta and mixtures thereof.

### Claim 15

A class of permanent magnets represented by the general formula RE(CowFevCuxTy)Z, where RE is a rare earth element selected from the group consisting of Sm, Gd, Pr, Nd, Dy, Ce, Ho, Er, La, Y, Tb and mixtures thereof, and T is a transition metal selected from the group consisting of Zr, Hf, Ti, Mn, Cr, Nb, Mo, W, V, Ni, Ta, and mixtures thereof, wherein said magnets exhibit substantially linear extrinsic demagnetization curves at maximum operating temperatures up to 700° C.