# US 6,726,768 B2 · Method of crystallizing amorphous silicon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,768 B2
- Document ID: US6726768B2
- Status: Granted
- Kind: B2
- Application number: 10/134,480
- Filed: 2002-04-30
- Published: 2002-11-14
- Granted: 2004-04-27
- Earliest claimed: 2001-05-11
- Assignees: LG. Philips LCD Co., Ltd.
- Inventors: Jin-Mo Yoon
- Web page: https://patentgrep.com/patent/US6726768B2

## CPC

- H10P 14/381: {Beam shaping, e.g. using a mask}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3812: {Shape of mask}
- H10P 14/382: {Scanning of a beam}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A mask and its application in sequential lateral solidification (SLS) crystallization of amorphous silicon. The mask includes a light absorptive portion that blocks a laser beam and a plurality of tier-shaped light-transmitting portions that pass a laser beam. Each light-transmitting portion has a plurality of adjacent rectangular sub-portions. Adjacent rectangular sub-portions form a step. In operation, the mask moves transversely relative to a amorphous silicon film while a laser performs SLS crystallization. The light portions control grain growth such that high quality polycrystalline silicon is formed.

## Claims

### Claim 1

A sequential lateral solidification (SLS) mask comprising:
a light absorptive portion for blocking a laser beam; and
a plurality of tier-shaped light-transmitting portions for passing a laser beam.

### Claim 2 (depends on 1)

The sequential lateral solidification (SLS) mask of claim 1, wherein each tier-shaped light-transmitting portion includes a plurality of rectangular sub-portions that are adjacent each other.

### Claim 3 (depends on 2)

The sequential lateral solidification (SLS) mask of claim 2, wherein the width of each rectangular sub-portion is greater than one micrometer.

### Claim 4 (depends on 3)

The sequential lateral solidification (SLS) mask of claim 3, wherein the width of each rectangular sub-portion is equal to or less than twice the maximum length of the lateral grain growth that is to be grown by the sequential lateral solidification (SLS) mask.

### Claim 5 (depends on 2)

The mask of claim 2, wherein the width of each rectangular sub-portion is equal to or greater than twice the maximum length of the lateral grain growth that is to be grown by the sequential lateral solidification (SLS) mask.

### Claim 6 (depends on 1)

The mask of claim 1, wherein adjacent rectangular sub-portions form a step.

### Claim 7 (depends on 6)

The mask of claim 6, wherein the step is greater than the maximum length of the lateral grain growth that is to be grown by the sequential lateral solidification (SLS) mask.

### Claim 8 (depends on 6)

The mask of claim 6, wherein the step between the adjacent rectangular sub-portions is less than the maximum length of the lateral grain growth that is to be grown by the sequential lateral solidification (SLS) mask.

### Claim 9 (depends on 1)

The mask of claim 1, wherein a length of each rectangular sub-portion ranges is greater than two hundred micrometers.

### Claim 10

A method of crystallizing an amorphous silicon film, comprising;
locating a substrate having an amorphous silicon film in a sequential lateral solidification (SLS) apparatus;
irradiating the amorphous silicon film using a laser beam that passes through a mask, wherein the mask includes a light absorptive portion and a plurality of tier-shaped light-transmitting portions, wherein each light-transmitting portion has a plurality of rectangular sub-portions, wherein a width of each rectangular sub-portion is greater than one micrometer and less than ten micrometers, wherein a length of each rectangular sub-portion is greater than 200 micrometers, wherein the laser beam portion that passes through said light-transmitting portions melts the amorphous silicon film in first crystallized regions into liquid silicon, wherein each of said first crystallized regions includes a plurality of silicon sub-portions, each having a first grain region, a second grain region, and a middle section, and wherein silicon grains form in the first and second grain regions by growing laterally from an interface between liquid silicon and solid silicon;
transversely moving the mask relative to the amorphous silicon film; and
performing a second crystallization on second crystallized regions such that silicon grains in the second grain regions continue to grow.

### Claim 11 (depends on 10)

The method of claim 10, further comprising transversely moving the mask relative to the amorphous silicon film a plurality of times so as to continue growing the silicon grains in the second grain regions until the amorphous silicon film is crystallized in the transverse direction.

### Claim 12 (depends on 11)

The method of claim 11, further comprising moving the mask in a longitudinal direction after the amorphous silicon film is crystallized in the transverse direction.

### Claim 13 (depends on 12)

The method of claim 12, further comprising conducting a second transverse directional crystallization after moving the mask in the longitudinal direction.

### Claim 14 (depends on 13)

The method of claim 13, wherein a step is formed by adjacent tier-shaped light-transmitting portions.

### Claim 15 (depends on 14)

The method of claim 14, wherein the step is greater than the maximum length of lateral grain growth of the silicon grains.

### Claim 16 (depends on 14)

The method of claim 14, wherein the step is less than the maximum length of lateral growth of the grain.

### Claim 17 (depends on 10)

The method of claim 10, wherein the width of each rectangular sub-portion is less then or equal to twice the maximum length of lateral grain growth.

### Claim 18 (depends on 17)

The method of claim 17, wherein the middle section of the each silicon sub-portion is a collision region wherein silicon grains collide.

### Claim 19 (depends on 10)

The method of claim 10, wherein the width of each rectangular sub-portion is greater than or equal to twice the maximum length of lateral grain growth.

### Claim 20 (depends on 19)

The method of claim 19, wherein laser beam irradiation forms polycrystalline silicon particles in the middle section of each first crystallized region.
