# US 6,726,535 B2 · Method for preventing localized Cu corrosion during CMP

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,535 B2
- Document ID: US6726535B2
- Status: Granted
- Kind: B2
- Application number: 10/132,442
- Filed: 2002-04-25
- Published: 2003-10-30
- Granted: 2004-04-27
- Earliest claimed: 2002-04-25
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Tsu Shih; Kuan-Ku Hung; Chen-Hua Yu
- Web page: https://patentgrep.com/patent/US6726535B2

## CPC

- H10W 20/062: {by smoothing of conductive parts, e.g. by planarisation}
- H10P 52/403: {of conductive or resistive materials}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for preventing or reducing corrosion of copper containing features included in a semiconductor wafer in a chemical mechanical polishing (CMP) process including providing a semiconductor wafer polishing surface including copper filled anisotropically etched features; polishing the semiconductor wafer polishing surface according to a first CMP process including applying at least one polishing slurry to contact the semiconductor wafer polishing surface for removing an uppermost layer of the semiconductor wafer polishing surface; and, alternately applying a copper corrosion inhibitor solution for a period of time and the at least one polishing slurry for a period of time to contact the semiconductor wafer polishing surface to comprise a polishing cycle said polishing cycle performed at least once during at least a second CMP process.

## Claims

### Claim 1

A method for preventing or reducing corrosion of copper containing features included in a semiconductor wafer in a chemical mechanical polishing (CMP) process comprising the steps of:
providing a semiconductor wafer polishing surface including copper filled anisotropically etched features;
polishing the semiconductor wafer polishing surface according to a first CMP process including applying at least one polishing slurry to contact the semiconductor wafer polishing surface for removing an uppermost layer of the semiconductor wafer polishing surface; and,
alternately applying a copper corrosion inhibitor solution for a period of time and the at least one polishing slurry for a period of time to contact the semiconductor wafer polishing surface to comprise a polishing cycle said polishing cycle performed at least once during at least a second CMP process.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of polishing the semiconductor wafer polishing surface according to a first CMP process includes polishing the uppermost layer to endpoint detection with respect to the uppermost layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the uppermost layer includes copper.

### Claim 4 (depends on 1)

The method of claim 1, wherein the copper corrosion inhibitor solution includes Benzotriazole (BTA) and derivatives thereof.

### Claim 5 (depends on 4)

The method of claim 4, wherein the copper corrosion inhibitor solution includes a mixture of BTA and deionized water.

### Claim 6 (depends on 5)

The method of claim 5, wherein the BTA is present in an amount from about 0.04 to about 4 weight percent.

### Claim 7 (depends on 1)

The method of claim 1, wherein the step of alternately applying includes applying the copper corrosion inhibitor solution from about 5 to about 20 seconds and applying the polishing slurry from about 30 to about 60 seconds.

### Claim 8 (depends on 1)

The method of claim 1, wherein the at least a second CMP process includes a third CMP process to remove a barrier/adhesion layer underlying the uppermost layer to planarize the semiconductor wafer polishing surface.

### Claim 9 (depends on 8)

The method of claim 8, wherein the barrier/adhesion layer comprises a metal nitride.

### Claim 10 (depends on 9)

The method of claim 9, wherein the metal nitride includes at least one of titanium nitride and tantalum nitride.

### Claim 11 (depends on 10)

The method of claim 10, wherein the polishing cycle is performed from about 1 to about 4 times.

### Claim 12

A method for preventing or reducing corrosion of copper containing features included in a semiconductor wafer during chemical mechanical polishing (CMP) comprising the steps of:
providing a semiconductor wafer polishing surface including copper filled anisotropically etched features;
polishing the semiconductor wafer polishing surface according to a first CMP process including applying a first polishing slurry for removing an uppermost copper layer of the semiconductor wafer polishing surface to endpoint detection with respect to the uppermost copper layer;
alternately applying to the semiconductor wafer polishing surface a first copper corrosion inhibitor solution for a period of time and the first polishing slurry for a period of time to comprise a copper layer overpolishing cycle said copper layer overpolishing cycle performed at least once during a second CMP process to substantially expose an underlying barrier/adhesion layer; and
alternately applying to the semiconductor wafer polishing surface a second polishing slurry for a period of time and the second copper corrosion inhibitor solution for a period of time to comprise a barrier/adhesion layer polishing cycle said polishing cycle performed at least once during a third CMP process to substantially expose an underlying insulating layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein at least one of the first and second copper corrosion inhibitor solutions include Benzotriazole (BTA) and derivatives thereof.

### Claim 14 (depends on 13)

The method of claim 13, wherein at least one of the first and second copper corrosion inhibitor solutions includes a mixture of BTA and deionized water.

### Claim 15 (depends on 14)

The method of claim 14, wherein the BTA is present in an amount from about 0.04 to about 4 weight percent.

### Claim 16 (depends on 12)

The method of claim 12, wherein the steps of alternately applying include independently applying the first copper corrosion inhibitor solution from about 5 to about 20 seconds and independently applying the first polishing slurry from about 30 to about 60 seconds.

### Claim 17 (depends on 12)

The method of claim 12, wherein the steps of alternately applying include independently applying the second copper corrosion inhibitor solution from about 5 to about 20 seconds and independently applying the second polishing slurry from about 30 to about 60 seconds.

### Claim 18 (depends on 12)

The method of claim 12, wherein the barrier/adhesion layer comprises a metal nitride.

### Claim 19 (depends on 18)

The method of claim 18, wherein the metal nitride includes at least one of titanium nitride and tantalum nitride.

### Claim 20 (depends on 12)

The method of claim 12, wherein the barrier/adhesion layer polishing cycle is performed from about 1 to about 4 times.