# US 6,726,530 B2 · End-point detection system for chemical mechanical polishing applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,530 B2
- Document ID: US6726530B2
- Status: Granted
- Kind: B2
- Application number: 10/052,769
- Filed: 2002-01-17
- Published: 2002-05-23
- Granted: 2004-04-27
- Earliest claimed: 2000-06-30
- Assignees: Lam Research Corporation
- Inventors: Katrina A. Mikhaylich; Mike Ravkin; Yehiel Gotkis
- Web page: https://patentgrep.com/patent/US6726530B2

## CPC

- B24B 37/013: Devices or means for detecting lapping completion
- B24B 21/04: for grinding plane surfaces
- B24B 49/14: taking regard of the temperature during grinding
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS

## Abstract

Chemical mechanical polishing systems and methods are disclosed. The system includes a polishing pad that is configured to move from a first point to a second point. A carrier is also included and is configured to hold a substrate to be polished over the polishing pad. The carrier is designed to apply the substrate to the polishing pad in a polish location that is between the first point and the second point. A first sensor is located at the first point and oriented so as to sense an IN temperature of the polishing pad, and a second sensor is located a the second point and oriented so as to sense an OUT temperature of the polishing pad. The sensing of the IN and OUT temperatures is configured to produce a temperature differential that allows monitoring the process state and the state of the wafer surface for purposes of switching the process steps while processing wafers by chemical mechanical planarization.

## Claims

### Claim 1

A method for monitoring a process state of a wafer surface during chemical mechanical polishing, comprising:
providing a polishing pad belt that is configured to move linearly;
applying a wafer to the polishing pad belt at a polishing location so as to remove a first layer of material from the wafer;
sensing a first temperature of the polishing pad belt at an IN location that is linearly before the polishing location;
sensing a second temperature of the polishing pad belt at an OUT location that is linearly after the polishing location;
calculating a temperature differential between the second temperature and the first temperature; and
monitoring a change in the temperature differential, the change being indicative of a removal of the first layer from the wafer.

### Claim 2 (depends on 1)

A method for monitoring a process state of a wafer surface during chemical mechanical polishing as recited in claim 1, further comprising:
generating a temperature differential table, the temperature differential table including a plurality of temperature differentials wherein each temperature differential is associated with a material type to be polished from the wafer.

### Claim 3 (depends on 2)

A method for monitoring a process state of a wafer surface during chemical mechanical polishing as recited in claim 2, wherein the change in temperature differential further indicates a change in the removal of the first layer being of first type of material to another layer being of a second type of material.

### Claim 4 (depends on 3)

A method for monitoring a process state of a wafer surface during chemical mechanical polishing as recited in claim 3, wherein the first type of material is a metallization material and the second type of material is a barrier material.

### Claim 5 (depends on 3)

A method for monitoring a process state of a wafer surface during chemical mechanical polishing as recited in claim 3, wherein the first type of material is a diffusion barrier material and the second type of material is an dielectric material.

### Claim 6 (depends on 1)

A method for monitoring a process state of a wafer surface during chemical mechanical polishing as recited in claim 1, wherein the sensing includes infrared temperature sensing.

### Claim 7 (depends on 1)

A method for monitoring a process state of a wafer surface during chemical mechanical polishing as recited in claim 1, further comprising:
sensing a plurality of additional pairs of locations, each of the additional pairs of locations including a first point that is before the polishing location and a second point that is after the polishing location.

### Claim 8 (depends on 7)

A method for monitoring a process state of a wafer surface during chemical mechanical polishing as recited in claim 7, wherein each of the additional pairs of locations are configured to provide end-point detection over an associated plurality of zones of the wafer.

### Claim 9

A method for monitoring a process state of a wafer surface for purposes of switching to another wafer preparation phase or finishing a chemical mechanical planarization process, comprising:
providing a polishing pad that is configured to move linearly;
applying a wafer to the polishing pad at a polishing location so as to remove a layer of material from the wafer;
sensing a first temperature of the polishing pad at a first location that is before the polishing location;
sensing a second temperature of the polishing pad at a second location that is after the polishing location; and
calculating a temperature differential between the second temperature and the first temperature.

### Claim 10 (depends on 9)

A method for monitoring a process state of a wafer surface for purposes of switching to another wafer preparation phase or finishing a chemical mechanical planarization process as recited in claim 9, further comprising:
monitoring a change in the temperature differential, the change being indicative of a removal of the layer from the wafer.

### Claim 11 (depends on 10)

A method for monitoring a process state of a wafer surface for purposes of switching to another wafer preparation phase or finishing a chemical mechanical planarization process as recited in claim 10, wherein the change in temperature differential further indicates a change in the removal of the layer being of first type of material to another layer being of a second type of material.

### Claim 12

An end-point detection method, comprising:
providing a polishing pad;
applying a wafer to the polishing pad at a polishing location so as to remove a first layer of material from the wafer;
sensing a first temperature of the polishing pad at an IN location that is before the polishing location;
sensing a second temperature of the polishing pad at an OUT location that is after the polishing location;
calculating a temperature differential between the second temperature and the first temperature; and
monitoring a change in the temperature differential, the change being indicative of a removal of the first layer from the wafer.

### Claim 13 (depends on 12)

An end-point detection method as recited in claim 12, wherein the pad is one of a belt pad, a table pad, a rotary pad, and an orbital pad.