# US 6,726,378 B2 · Connecting method of different kind optical fibers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,378 B2
- Document ID: US6726378B2
- Status: Granted
- Kind: B2
- Application number: 10/160,560
- Filed: 2002-05-30
- Published: 2003-01-30
- Granted: 2004-04-27
- Earliest claimed: 2001-03-29
- Assignees: Furukawa Electric Co., Ltd.
- Inventors: Tetsuo Suzuki
- Web page: https://patentgrep.com/patent/US6726378B2

## CPC

- G02B 6/2551: {using thermal methods, e.g. fusion welding by arc discharge, laser beam, plasma torch}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

The connecting method of different kind optical fibers of the present invention is a connecting method able to improve the strength of connecting portions of the different kind optical fibers of different mode field diameters. In this connecting method, connecting ends of the different kind optical fibers removing their coating therefrom are mutually butted and fusion-spliced by gripping the coating in a step (S4). Next, the mode field diameters of different kind optical fiber connecting portions are conformed to each other by the heat treatment of a step (S5). This heat treatment is taken within a low dust space having a clean degree of 1000 or less in class. Thus, the heat treatment is taken under an environment in which foreign matters floated around the connecting portions of the different kind optical fibers are very small. Therefore, it is possible to restrain a crack from being caused by burning the foreign matters into the connecting portions. Accordingly, strength deterioration of the connecting portions of the different kind optical fibers caused by the crack can be prevented.

## Claims

### Claim 1

A method of fusion splicing two optical fibers having different mode field diameters comprising:
fusion splicing end faces of the optical fibers; and
heat-treating the fusion spliced portion optical fibers at a temperature sufficient to conform the mode field diameters,
wherein said heat-treating is performed under a clean degree of 1000 or less in class.

### Claim 2 (depends on 1)

The method of claim 1, further comprising cleaning just before the heat-treating.

### Claim 3 (depends on 1)

The method of claim 1 further comprising forming a protecting layer on the surface of the optical fibers while avoiding the heat treated area after said heat-treating; and,
etching a surface of the optical fibers including the heat-treated area of the optical fibers.

### Claim 4 (depends on 3)

The method of claim 3, wherein the optical fibers coated with coating layers, and said fusion splicing is performed after the coating layers of the optical fibers are removed, and a length interval of an etching processing area is equal to or greater than a length interval of the heat-treated area and smaller than an interval for removing the coating layers therefrom.

### Claim 5

A method of fusion splicing two optical fibers having different mode field diameters comprising:
exposing the optical fibers by removing the coating layers of the optical fibers;
fusion-splicing the exposed optical fibers;
heat-treating a fusion-spliced portion of the optical fibers to conform the mode field diameters;
forming a protective layer on both at least a portion of the exposed optical fibers and end face portions of the coating layer after said heat treating; and
etching a surface of the optical fibers including the heat-treated area of the optical fibers.

### Claim 6 (depends on 5)

The method of claim 5, further comprising cleaning just before the heat-treating.

### Claim 7 (depends on 5)

The method of claim 5, wherein an etched area includes the heat treated area, and non-etched areas remain in the exposed areas of the optical fibers.

### Claim 8

A method of fusion splicing two optical fibers having different mode field diameters comprising:
exposing the optical fibers by removing coating layers of the optical fibers;
fusion-splicing exposed optical fibers;
heat-treating a fusion-spliced portion of the optical fibers to conform the mode field diameters; and
forming a protective layer on at least a portion of the exposed optical fibers after said heat-treating;
wherein at least said heat-treating is performed under a clean degree of 1000 or less in class.

### Claim 9 (depends on 8)

The method of claim 8, wherein the protective layer is formed while avoiding the heat treated area.

### Claim 10 (depends on 8)

The method of claim 8, wherein the protective layer is formed on at least a portion of the exposed optical fibers and end face portions of the coating layer.

### Claim 11 (depends on 8)

The method of claim 8, further comprising etching a surface of the optical fibers including the heat-treated area of the optical fibers, wherein a length interval of an etching processing area is equal to or greater than a length interval of the heat-treated area and smaller than an interval for removing the coating layers therefrom.

### Claim 12 (depends on 8)

The method of claim 8, further comprising cleaning just before the heat-treating.