# US 6,726,216 B2 · Piston ring with oxide-nitride composite layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,216 B2
- Document ID: US6726216B2
- Status: Granted
- Kind: B2
- Application number: 10/158,836
- Filed: 2002-06-03
- Published: 2002-12-05
- Granted: 2004-04-27
- Earliest claimed: 2001-06-01
- Assignees: Federal-Mogul Friedberg GmbH
- Inventors: Ehrenfried Horn; Rudolf Widmann; Steffen Hoppe
- Web page: https://patentgrep.com/patent/US6726216B2

## CPC

- F16J 9/26: characterised by the use of particular materials
- F16J: PISTONS {(specially adapted for dampers F16F9/32)}; CYLINDERS; SEALINGS

## Abstract

A piston ring for use in a cylinder of an internal combustion engine, which ring is nitride-hardened at least on the sliding surface between piston ring and cylinder wall. The nitride layer is composed of a precipitated layer and a compound layer, wherein the piston ring consists of a low-alloyed iron-base material and an oxide layer is deposited on the compound layer.

## Claims

### Claim 1

A nitride hardened piston ring for use in a cylinder of an internal combustion engine, which piston ring has a surface that is in sliding contact relationship with a wall of said cylinder during operation, wherein the piston ring comprises
low alloy iron based material;
a region of increased nitride content whereby the piston ring is nitride-hardened, wherein said region of increased nitride content comprises a precipitated layer and a compound layer,
wherein the compound layer comprises a multi-phase compound layer; and wherein the precipitated layer comprises ferrite and further comprises dissolved nitrogen or carbon and which are in the precipitated layer in the form of Fe4N member selected from the group consisting of Fe4N, CrN and CrCN;
an oxide layer which is deposited on the said surface of said piston ring and which is deposited over the compound layer, and which oxide layer, during operation is in sliding contact with said cylinder
wherein the oxide layer has a thickness of 1-4 μm and wherein the oxide layer comprises at least one iron oxide in which the iron has a valence of 2 or 3 and the iron oxide is in the form of hematite and magnetite.

### Claim 2 (depends on 1)

The piston ring of claim 1, wherein the compound layer is a multiphase compound layer, selected from the group consisting of Fe2-3N, Fe2-3NC, Fe4N, Fe4NC, CrN and CrCN.

### Claim 3 (depends on 1)

The piston ring of claim 1, wherein the nitration-hardened layer is generated with a gas-normal pressure technique.

### Claim 4 (depends on 2)

The piston ring of claim 2, wherein the nitration-hardened layer is generated with a gas-normal pressure technique.