# US 6,726,086 B2 · Liquid phase diffusion bonding to a superalloy component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,086 B2
- Document ID: US6726086B2
- Status: Granted
- Kind: B2
- Application number: 10/056,141
- Filed: 2002-01-24
- Published: 2003-07-24
- Granted: 2004-04-27
- Earliest claimed: 2002-01-24
- Assignees: Siemens Westinghouse Power Corporation
- Inventors: Vinod Mohan Philip
- Web page: https://patentgrep.com/patent/US6726086B2

## CPC

- B23P 6/007: {using only additive methods, e.g. build-up welding}
- B23K 20/023: {Thermo-compression bonding}
- B23K 35/0244: {Powders, particles or spheres; Preforms made therefrom}
- B23K 35/304: {with Cr as the next major constituent}
- B23P 6/002: {Repairing turbine components, e.g. moving or stationary blades, rotors, (B23P6/045 takes precedence)}
- C22F 1/10: of nickel or cobalt or alloys based thereon
- B23K 35/025: {Pastes, creams or slurries}
- B23K 2101/001: {Turbines}
- C21D 9/50: for welded joints
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

A method for the manufacturing or repair of a superalloy gas turbine component including a liquid phase diffusion bonding process wherein the brazing heat treatment used for the diffusion bonding of a powder material to the component is accomplished by a heat cycle that is performed on the component for another purpose. A manufacturing solution heat treatment, a pre-weld heat treatment, a post-weld heat treatment, or a rejuvenating heat treatment may be used as the brazing heat treatment. The composition of the powder material is selected so that a desired set of material properties is achieved when the powder material is subjected to the dual-purpose heat cycle. In one embodiment, a 50/50 mixture of AM775 and IN939 powder is diffusion brazed to an IN939 superalloy component using a heat treatment which also functions as the post-casting solution heat treatment for the IN939 component.

## Claims

### Claim 1

A method comprising:
casting an alloy material to form a component;
performing a solution heat treatment on the component;
subjecting the component to an operating environment;
applying an alloy powder mixture to the component; and
bonding the alloy powder mixture to the component by liquid phase diffusion bonding using a brazing heat treatment that incorporates the solution heat treatment, the alloy powder mixture selected to achieve a desired material property when exposed to the brazing heat treatment, and further comprising:
selecting the alloy material to be IN 939;
selecting the alloy powder mixture to be a 50/50 ratio by weight percent of IN 939 and AM 775 alloys;
performing the solution heat treatment as heating the component to 2,120° F. for four hours followed by cooling to below 1,000° F. in twenty minutes or less; and
performing the brazing heat treatment cycle as heating the component to 2,120° F. for four hours, cooling the component to 2,050° F. and holding for four hours, followed by cooling from 2,050° F. to below 1,000° F. in twenty minutes or less.

### Claim 2

A method comprising:
casting an alloy material to form a component;
performing a solution heat treatment on the component;
subjecting the component to an operating environment;
applying an alloy powder mixture to the component; and
bonding the alloy powder mixture to the component by liquid phase diffusion bonding using a brazing heat treatment that incorporates the solution heat treatment, the alloy powder mixture selected to achieve a desired material property when exposed to the brazing heat treatment, and further comprising performing a welding process on the component after the step of bonding, wherein the brazing heat treatment functions as a pre-weld heat treatment for the welding process.

### Claim 3

A method comprising:
casting an alloy material to form a component;
performing a solution heat treatment on the component;
subjecting the component to an operating environment;
applying an alloy powder mixture to the component; and
bonding the alloy powder mixture to the component by liquid phase diffusion bonding using a brazing heat treatment that incorporates the solution heat treatment, the alloy powder mixture selected to achieve a desired material property when exposed to the brazing heat treatment, and further comprising performing a welding process on the component before the step of bonding, wherein the brazing heat cycle functions as a post-weld heat treatment for the welding process.

### Claim 4

A method comprising:
casting an alloy material to form a component;
applying an alloy powder mixture to the component; and
performing a solution heat treatment cycle on the component, the solution heat treatment cycle functioning as a brazing heat treatment for bonding the alloy powder mixture to the component by liquid phase diffusion bonding, the powder mixture selected to achieve a desired material property when subjected to the solution heat treatment cycle, and further comprising:
selecting the alloy material to be IN 939;
selecting the alloy powder mixture to be a 50/50 ratio by weigh percent of IN 939 and AM 775 alloys;
performing the solution heat treatment as heating the component to 2,120° F. for four hours, cooling the component to 2,050° F. and holding for four hours, followed by cooling from 2,050° F. to below 1,000° F. in twenty minutes or less.

### Claim 5

A method comprising:
casting an alloy material to form a component;
applying an alloy powder mixture to the component; and
performing a solution heat treatment cycle on the component, the solution heat treatment cycle functioning as a brazing heat treatment for bonding the alloy powder mixture to the component by liquid phase diffusion bonding, the powder mixture selected to achieve a desired material property when subjected to the solution heat treatment cycle, and further comprising:
exposing the component to a high temperature operating environment after the step of performing a solution heat treatment cycle;
applying a second alloy powder mixture to the component;
applying a brazing heat treatment cycle to the component to bond the second alloy powder mixture to the component by liquid phase diffusion bonding, the brazing heat cycle selected to incorporate the solution heat treatment cycle and the second powder mixture selected to achieve a desired material property when subjected to the brazing heat treatment cycle.

### Claim 6

A method comprising:
applying a first alloy powder mixture to a component formed of an alloy material;
bonding the first alloy powder mixture to the component by liquid phase diffusion bonding using a first brazing heat treatment that accomplishes bonding between the first alloy powder mixture and the component by liquid phase diffusion bonding and that also accomplishes a pre-weld stress relief in the component; and
performing a welding process on the component after the step of bonding.

### Claim 7 (depends on 6)

The method of claim 6, further comprising:
selecting the alloy material to be IN 939;
selecting the alloy powder mixture to be a 50/50 ratio by weigh percent of IN 939 and AM 775 alloys; and
performing the first brazing heat treatment as heating the component to 2,120° F. for four hours, cooling the component to 2,050° F. and holding for four hours, followed by cooling from 2,050° F. to below 1,000° F. in twenty minutes or less.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first brazing heat treatment is selected to incorporate a manufacturing solution heat treatment used to form the component.

### Claim 9 (depends on 6)

The method of claim 6, further comprising:
applying a second alloy powder mixture to the component; and
bonding the second alloy powder mixture to the component by liquid phase diffusion bonding using a second brazing heat treatment that accomplishes bonding between the second alloy powder mixture and the component by liquid phase diffusion bonding and that also accomplishes a post-weld stress relief in the component.

### Claim 10 (depends on 9)

The method of claim 9, wherein the second alloy powder mixture is selected to have essentially the same composition as the first alloy powder mixture and the second brazing heat treatment is selected to be essentially the same as the first brazing heat treatment.

### Claim 11

A method comprising:
performing a welding process on a component formed of an alloy material;
applying an alloy powder mixture to a portion of the component; and
bonding the alloy powder mixture to the component by liquid phase diffusion bonding using a brazing heat treatment that accomplishes liquid phase diffusion bonding between the alloy powder mixture and the component and that also accomplishes a post weld stress relief in the component.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
selecting the alloy material to be IN 939;
selecting the alloy powder mixture to be a 50/50 ratio by weigh percent of IN 939 and AM 775 alloys; and
performing the brazing heat treatment as heating the component to 2,120° F. for four hours, cooling the component to 2,050° F. and holding for four hours, followed by cooling from 2,050° F. to below 1,000° F. in twenty minutes or less.

### Claim 13 (depends on 11)

The method of claim 11, wherein the brazing heat treatment is selected to incorporate a manufacturing solution heat treatment used to form the component.