# US 6,726,085 B2 · Method and apparatus for producing a refined grain structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,726,085 B2
- Document ID: US6726085B2
- Status: Granted
- Kind: B2
- Application number: 10/145,009
- Filed: 2002-05-14
- Published: 2003-11-27
- Granted: 2004-04-27
- Earliest claimed: 2002-05-14
- Assignees: The Boeing Company
- Inventors: Edward Litwinski; Steven G. Keener
- Web page: https://patentgrep.com/patent/US6726085B2

## CPC

- B23K 20/1275: {involving metallurgical change}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The apparatus for operating on a workpiece includes a die defining first and second apertures and an interior therebetween. The first aperture and the interior of the die are structured to receive the workpiece. The interior of the die can be structured to shape the workpiece into a predetermined configuration. The apparatus includes at least one rotatable pin extending at least partially into the interior of the die. The pin is structured to at least partially stir the workpiece as the workpiece moves through the interior of the die to thereby refine the grain structure of the workpiece.

## Claims

### Claim 1

A method of operating on a workpiece, comprising:
moving a workpiece through a die; and
concurrently with said moving step, mixing the workpiece with at least one rotating pin to thereby refine the grain structure of the workpiece.

### Claim 2 (depends on 1)

A method according to claim 1 wherein said mixing step comprises:
individually rotating a plurality of pins in corresponding first directions; and
collectively rotating the plurality of pins in a second direction.

### Claim 3 (depends on 2)

A method according to claim 2 wherein the corresponding first directions are the same as the second direction.

### Claim 4 (depends on 2)

A method according to claim 2 wherein the corresponding first directions are opposite to the second direction.

### Claim 5 (depends on 2)

A method according to claim 2 wherein said first rotating step comprises individually rotating at least two of the plurality of friction stir pins in opposite directions.

### Claim 6 (depends on 1)

A method according to claim 1 further comprising precipitation hardening the workpiece prior to said moving step.

### Claim 7 (depends on 1)

A method according to claim 1 further comprising solution heat treating the workpiece at a predetermined temperature schedule after said mixing step.

### Claim 8 (depends on 7)

A method according to claim 7 further comprising precipitation heat treating the workpiece by aging at a second predetermined temperature schedule after said solution heat treating step.

### Claim 9 (depends on 1)

A method according to claim 1 further comprising heating the workpiece concurrently with said mixing step.

### Claim 10 (depends on 1)

A method according to claim 1 further comprising heating at least one of the pin or the die concurrently with said mixing step.

### Claim 11 (depends on 10)

A method according to claim 10 wherein said heating step comprises heating the at least one of the pin or the die to a temperature between about 600° F. and about 1000° F.

### Claim 12 (depends on 1)

A method according to claim 1 further comprising cooling the die concurrently with said mixing step.