# US 6,722,012 B1 · Minting process for producing a two color coin or medal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,722,012 B1
- Document ID: US6722012B1
- Status: Granted
- Kind: B1
- Application number: 09/638,988
- Filed: 2000-08-15
- Granted: 2004-04-20
- Earliest claimed: 2000-08-15
- Assignees: Imprensa Nacional Casa da Moeda, SA
- Inventors: Antonio Jose do Rosario Coelho Texeira; Paulo Antonio Martins; Paulo Jorge Leitao
- Web page: https://patentgrep.com/patent/US6722012B1

## CPC

- A44C 21/00: Coins (coins specially adapted to operate coin-freed mechanisms G07F1/06); Emergency money; Beer or gambling coins or tokens, or the like
- B44B 5/008: {in layered material; connecting a plurality of layers by embossing}
- B44B 5/009: {by multi-step processes}
- Y10T 29/49915: Overedge assembling of seated part
- A44C: PERSONAL ADORNMENTS, e.g. JEWELLERY; COINS
- B44B: MACHINES, APPARATUS OR TOOLS FOR ARTISTIC WORK, e.g. FOR SCULPTURING, GUILLOCHING, CARVING, BRANDING, INLAYING (processes for producing decorative effects B44C; embossing leather C14B)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention deals with a technology for minting coins and medals. The technology is based on the utilization of metal blanks with similar diameters, one being very thin (hereafter named as the foil), joined together by mechanical means during the impartion of the surface details by the minting dies. The technology requires the design and manufacture of a special geometry in the edge of the thicker disk in order to make possible assembly of the metal blanks. The proposed technology is based on a multi-stage manufacturing process consisting of three cold metal forming operations (preforming, rimming and coining) and one intermediate annealing treatment. The first metal forming operation ensures the preforming of the thicker disk blank, hereafter named as the disk. The second metal forming stage is the rimming operation in which the preformed disk is bent along its diameter in order to generate a suitable profile for subsequent assembly with the foil. The third metal forming stage is a coining operation in which the metal blanks (disk and foil) are assembled together, by locking the foil into the rimmed edge of the disk, during the imprint of the surface details. The annealing treatment is to be performed before the coining operation. The goal is to restore the initial ductility of the disk prior to the final coining stage.

## Claims

### Claim 1

A minting process for producing a two color coin or medal from a blank metal foil having a first color and a metal base having a thickness greater than the metal foil and a second color, the process comprising the steps of:
preforming the metal base to create an intermediate metal base geometry with a peripheral raised surface partition surrounding a lower surface area;
rimming the raised surface partition to form a suitable rim profile for subsequent assembly with the metal foil,
annealing the metal base following the rimming step; and
joining the blank metal foil onto the thicker metal base by:
positioning the blank metal foil proximate to the lower surface area,
imprinting an image on the foil subsequent to the positioning step, and
bending the rimmed profile for engagement with the foil.

### Claim 2 (depends on 1)

The process of claim 1 wherein said metal foil has a thickness in the range of 0.1 mm to less than 0.3 mm.

### Claim 3 (depends on 1)

The minting process of claim 1 wherein the imprinting and bending steps are performed simultaneously in a coining operation.

### Claim 4 (depends on 1, 3)

The minting process of claim 1 or 3 wherein the positioning step includes spacing a perimeter of the foil from the rim by a distance of about 0.3 mm.

### Claim 5 (depends on 1, 3)

The minting process of claim 1 or 3 wherein the positioning step includes spacing a perimeter of the foil from the rim by a distance within the range of 1% to 3% of the diameter of the blank metal foil.

### Claim 6 (depends on 1, 3)

The minting process of claim 1 or 3 wherein the rimming step includes forming a sharp fillet at the base of the rim.

### Claim 7 (depends on 1, 3)

The minting process of claim 1 or 3 wherein the annealing step is performed until the metal base recovers its initial ductility.

### Claim 8

A minting process for producing a two color coin or medal from a blank metal foil having a first color and a known perimeter size, and a metal base having a second color, a known ductility and a thickness greater than the foil thickness, the process comprising the steps of:
preforming the metal base to create an intermediate metal base geometry with a peripheral raised surface partition surrounding a lower surface area;
rimming the raised surface partition to form a suitable rim profile, including a sharp fillet at the base of the rim, for subsequent assembly with the metal foil,
annealing the metal base following the rimming step until the metal base recovers its initial ductility; and
joining the blank metal foil onto the thicker metal base by:
positioning the blank metal foil proximate to the lower surface area of the metal base with the perimeter of the foil being spaced from the rim by a distance within the range of 1% to 3% of the diameter of the blank metal foil, and
coining the foil and base simultaneously to imprint an image on the foil and to bend the rimmed profile for engagement with the foil.