Abstract
A hot-melt ink for use with an ink jet printing apparatus is a liquid at about 100° C. to about 130° C. and solidifies to a two-phase solid having an elastic phase and a crystalline phase. The ink is formulated from a carrier, a first plasticizer, a linear block copolymer, a block copolymer plasticizer, a flow additive and a colorant. The block copolymer plasticizer, in combination with the linear block copolymer forms an elastic phase of the ink upon solidifying. The first plasticizer exhibits sufficiently low viscosity at elevated temperatures to permit ejection of the liquid ink from the printing apparatus. A method for producing indicia is also disclosed.
Claims6
A hot-melt ink for use with an ink jet printing apparatus, the ink being a liquid at about 1000° C. to about 130° C. and solidifying to a two-phase solid having an elastic phase and a crystalline phase, the ink consisting essentially of:
- stearic acid present in a concentration of about 45 percent to about 95 percent of the ink;
- an aromatic hydrocarbon resin first plasticizer present in a concentration of about 0.1 percent to about 25 percent of the ink;
- a tri-block copolymer present in a concentration of about 0.5 percent to about 5.0 percent of the ink;
- polyvinyl butyral in a concentration of about 0.5 percent to about 10 percent of the ink;
- a fluorinated polyolefin copolymer present in a concentration of about 0.5 percent to about 10 percent of the ink;
- and
- a colorant present in a concentration of about 2.0 percent to about 8.0 percent of the ink,
- wherein the polyvinyl butyral, in combination with tri-block copolymer forms an elastic phase of the ink upon solidifying, and wherein the aromatic hydrocarbon resin exhibits sufficiently low viscosity at elevated temperatures to permit ejection of the liquid ink from the printing apparatus.
A method for producing indicia on a substrate comprising the steps of:
- heating to liquid a non-aqueous, solid hot-melt ink formulation to a temperature of not more than 130° C. said ink formulation including stearic acid present in a concentration of about 45 percent to about 95 percent of the ink, an aromatic hydrocarbon resin first plasticizer present in a concentration of about 0.1 percent to about 25 percent of the ink, a tri-block copolymer present in a concentration of about 0.5 percent to about 5.0 percent of the ink, polyvinyl butyral in a concentration of about 0.5 percent to about 10 percent of the ink, a fluorinated polyolefin copolymer present in a concentration of about 0.5 percent to about 10 percent of the ink and a colorant present in a concentration of about 2.0 percent to about 8.0 percent of the ink, the polyvinyl butyral, in combination with tri-block copolymer forming an elastic phase of the ink upon solidifying, wherein the aromatic hydrocarbon resin exhibiting sufficiently low viscosity at elevated temperatures to permit ejection of the liquid ink from the printing apparatus;
- ejecting the liquid from a printing device;
- and
- allowing the liquid to solidify.