Sulfoaluminous clinker without iron and without free lime, its process of preparation and its use in white binders
AssigneeCiments Francais
InventorsBruno Classen, Pierre Colombet
Life of this patent
Estimating the term…
Abstract
The lightly colored sulfoaluminous clinker contains: more than 55% by weight of calcium sulfoaluminate phase (C4A3S), more than 10% by weight of belite phase (C2S), less than 10% by weight of anhydrite (C{overscore (S)}), and contains practically no ferrite phase, nor a gehlenite phase (C2AS), nor free lime. It is prepared by a process of roasting carried out at temperatures comprised between about 1250° C. and 1350° C. It can be used for a wide range of applications by combining it with a source of calcium sulfate and/or Portland cement, to obtain binders having specific properties (color, setup time, mechanical strength, expansion or contraction . . . ).
Claims17
Sulfoaluminous clinker containing:
- more than 55% by weight of calcium sulfoaluminate phase (C4A3{overscore (S)})
- from 10 to 20% by weight of belite phase (C2S)
- less than 10% by weight of anhydrite (C{overscore (S)})
- less than 5% by weight of gehlenite phase (C2AS),
- a free lime content less than about 0.2% by weight, and an iron content (expressed as Fe2O3) less than about 0.3% by weight.
Dependencies are inferred from the claim text.