Conductive polyester/polycarbonate blends, methods for preparation thereof, and articles derived therefrom
AssigneeGeneral Electric Company
InventorsBimal R. Patel, Estelle Cheret
Life of this patent
Estimating the term…
Abstract
A conductive thermoplastic composition includes a polycarbonate, a polyester, a conductive filler, an impact modifier, a transesterification quench, and glass fibers. The composition exhibits high strength and stiffness and is especially suitable for molding rigid, electrostatically painted automobile parts.
Claims23
A conductive thermoplastic composition, comprising, based on the total weight of the composition:
- 10 to 50 weight percent polycarbonate,
- 20 to 60 weight percent polyester;
- 0.005 to 5 parts by weight transesterification quencher per 100 parts by weight of polyester;
- 1 to 20 weight percent impact modifier;
- 0.2 to 20 weight percent conductive filler;
- and
- 10 to 40 weight percent glass fibers;
- wherein the composition comprises a first continuous phase comprising polyester, and wherein at least 50% of the conductive filler is disposed in the continuous phase comprising polyester.
5 more elements
A conductive thermoplastic composition, comprising, based on the total weight of the composition:
- 15 to 30 weight percent polycarbonate,
- 35 to 45 weight percent polyester;
- 0.01 to 0.04 parts by weight transesterification quencher per 100 parts by weight of polyester;
- 6 to 10 weight percent impact modifier;
- 4 to 6 weight percent conductive carbon black;
- and
- 15 to 30 weight percent glass fibers;
- wherein the composition comprises a first continuous phase comprising polyester, and wherein at least 50% of the conductive filler is disposed in the continuous phase comprising polyester.
5 more elements
A method of preparing a conductive thermoplastic composition, comprising:
- blending 10 to 50 weight percent polycarbonate;
- 20 to 60 weight percent polyester;
- 0.005 to 5 parts by weight transesterification quencher per 100 parts by weight of polyester;
- 1 to 20 weight percent impact modifier;
- and 0.2 to 20 weight percent conductive filler to form a first blend;
- and
- adding 10 to 40 weight percent glass fibers to the first blend total form the conductive thermoplastic composition;
- wherein all weight percentages are based on the weight of the total composition, and wherein the conductive filler is provided to the first blend as a conductive filler concentrate comprising 5 to 30 parts by weight of conductive filler and 70 to 95 parts by weight of polyester.