Method and structure for determining a concentration profile of an impurity within a semiconductor layer
AssigneeCypress Semiconductor Corporation
InventorsSundar Narayanan, Krishnaswamy Ramkumar
Life of this patent
Estimating the term…
Loading patent…
AssigneeCypress Semiconductor Corporation
InventorsSundar Narayanan, Krishnaswamy Ramkumar
Estimating the term…
A method and a structure are provided for measuring a concentration of an impurity within a layer arranged upon a semiconductor substrate. The method may include exposing the layer and semiconductor substrate to oxidizing conditions and determining a difference in total dielectric thickness above the substrate from before to after exposing the layer and substrate. The difference may be correlated to a concentration of the impurity. In some cases, the method may include designating a plurality of measurement locations on the layer such that a concentration profile of the impurity within the layer may be determined. In some embodiments, exposing the layer and substrate may include forming an oxidized interface between the layer and the semiconductor substrate. Preferably, the oxidized interface is thicker underneath portions of the layer with a lower concentration of the impurity than underneath portions of the layer with a higher concentration of the impurity.
A method for measuring concentration of an known impurity within a dielectric layer arranged upon a semiconductor substrate, comprising:
A method for determining a concentration profile of a known component within a layer arranged upon a semiconductor substrate, comprising:
A semiconductor topography, comprising an oxidized interface between a semiconductor substrate and a layer comprising an impurity, wherein a thickness of the oxidized interface is dependent upon a concentration of the impurity within a respective portion of the layer.
Dependencies are inferred from the claim text.