# US 6,664,037 B2 · Silver halide emulsion and method for chemical sensitization thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,664,037 B2
- Document ID: US6664037B2
- Status: Granted
- Kind: B2
- Application number: 10/167,386
- Filed: 2002-06-12
- Published: 2003-05-01
- Granted: 2003-12-16
- Earliest claimed: 2001-06-15
- Assignees: Fuji Photo Film Co., Ltd.
- Inventors: Masafumi Mizuno
- Web page: https://patentgrep.com/patent/US6664037B2

## CPC

- G03C 1/005: Silver halide emulsions; Preparation thereof; Physical treatment thereof; Incorporation of additives therein (catalytic amounts of silver halide in dry silver systems {or thermographic systems using noble metal compounds} G03C1/494)
- G03C 1/09: Noble metals or mercury; Salts or compounds thereof; Sulfur, selenium or tellurium, or compounds thereof, e.g. for chemical sensitising (G03C1/34, G03C1/35 take precedence)
- G03C 1/0051: {Tabular grain emulsions}
- G03C 2001/0056: {Disclocations}
- G03C 2001/03552: {Epitaxial junction grains; Protrusions or protruded grains}
- G03C 2001/0863: {Group VIII metal compound}
- G03C 2001/091: {Gold}
- G03C 2001/096: {Sulphur sensitiser}
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

Disclosed is a method for chemical sensitization of a silver halide emulsion comprising a sensitization step of subjecting the silver halide emulsion to chemical sensitization with a chalcogen compound or a chalcogen compound and a gold compound to produce silver chalcogenide or gold silver chalcogenide, wherein the chemical sensitization is performed under such conditions that at least a part of the silver chalcogenide or gold silver chalcogenide produced in the sensitization step can be amorphized. This method can provide a silver halide emulsion showing high sensitivity without increasing fog and degrading storability and such a silver halide emulsion.

## Claims

### Claim 1

A method for chemical sensitization of a silver halide emulsion comprising a sensitization step of subjecting the silver halide emulsion to chemical sensitization with a chalcogen compound or a combination of a chalcogen compound and a gold compound to produce silver chalcogenide or gold silver chalcogenide, wherein the chemical sensitization is performed under such conditions that at least a part of the silver chalcogenide or gold silver chalcogenide produced in the sensitization step can be amorphized.

### Claim 2 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein the chemical sensitization is performed in the presence of transition metal ions of at least one metal selected from the metals of Group IB, Group IIB, Group VIA, Group VIIA and Group VIII.

### Claim 3 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein the maximum X-ray diffraction peak intensity of silver chalcogenide or gold silver chalcogenide obtained for a standard model as defined in the following (a) (Intensity A) and the maximum X-ray diffraction peak intensity of silver chalcogenide or gold silver chalcogenide obtained by applying the chemical sensitization conditions of the chemical sensitization step to a simplified model as defined in the following (b) (Intensity B) satisfy the relational equation defined in the following (c):
(a) silver chalcogenide or gold silver chalcogenide produced by mixing 20 mL of 0.01 mol/L silver nitrate aqueous solution, 20 mL of 0.01 mol/L solution of the chalcogen compound in water or an alcohol and, when a gold compound is also used in the chemical sensitization, 0.01 mol/L solution of the gold compound in water or an alcohol in such an amount that the gold compound and the chalcogen compound should exist in the same molar ratio as that used for the chemical sensitization, said mixing being conducted at the temperature used for the chemical sensitization,
(b) silver chalcogenide or gold silver chalcogenide produced by mixing the chalcogen compound or a combination of the chalcogen compound and the gold compound with 20 mL of 0.01 mol/L silver nitrate aqueous solution under the same conditions as those of the chemical sensitization, except that the silver halide emulsion does not exist, the chalcogen compound is added as 0.01 mol/L solution in water or an alcohol and the other additives are added in such amounts that molar ratios of the additives with respect to the chalcogen compound should be the same as those used for the chemical sensitization,
(c) B/A≦½.

### Claim 4 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein an amorphizing agent is used in the sensitization step.

### Claim 5 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein a gold sensitizer is used in the sensitization step.

### Claim 6 (depends on 5)

The method for chemical sensitization of a silver halide emulsion according to claim 5, wherein the gold sensitizer has an organic ligand.

### Claim 7 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein reduction sensitization is also performed in the sensitization step.

### Claim 8 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein a sensitizing dye is added during the sensitization step or before or after the sensitization step.

### Claim 9 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein a nitrogen-containing heterocyclic compound is added during the sensitization step.

### Claim 10 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein the silver halide grains are tabular grains having an aspect ratio of 2 or more.

### Claim 11 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein the silver halide grains have dislocation lines.

### Claim 12 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein the silver halide grains have a portion formed by epitaxial growth.

### Claim 13 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein the silver halide grains contain a Group VIII metal or an inorganic or organic hexa-coordinate complex thereof.

### Claim 14 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein a compound of Group VIII metal is added as an amorphizing agent within 5 minutes before or after addition of the chalcogen compound in an amount of {fraction (1/16)} to 16 times the amount of the chalcogen compound.

### Claim 15 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein Pt compound is added as an amorphizing agent within 5 minutes before or after addition of the chalcogen compound in an amount of {fraction (1/16)} to 16 times the amount of the chalcogen compound.

### Claim 16 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein a compound of Group VIII metal is added as an amorphizing agent within 2 minutes before or after addition of the chalcogen compound in an amount of ¼ to 4 times the amount of the chalcogen compound.

### Claim 17 (depends on 1)

The method for chemical sensitization of a silver halide emulsion according to claim 1, wherein Pt compound is added as an amorphizing agent within 2 minutes before or after addition of the chalcogen compound in an amount of ¼ to 4 times the amount of the chalcogen compound.