Etching of semiconductor wafer edges
AssigneeRWE Schott Solar, Inc.
InventorsMichael J. Kardauskas, Bernhard P. Piwczyk
Life of this patent
Estimating the term…
Abstract
A novel method of etching a plurality of semiconductor wafers is provided which comprises assembling said plurality of wafers in a stack, and subjecting said stack of wafers to dry etching using a relatively high density plasma which is produced at atmospheric pressure. The plasma is focused magnetically and said stack is rotated so as to expose successive edge portions of said wafers to said plasma.
Claims28
Method of etching the edges of a plurality of like semiconductor wafers of rectangular configuration for the purpose of removing micro-cracks at said edges, said method comprising assembling said plurality of wafers face-to-face in contact with each other so as to form a coin stack with the wafers having their edges in mutual alignment, providing a reaction chamber containing a plasma generator characterized by at least a pair of hollow gas discharge electrodes that are disposed adjacent one another and arranged so that gas streams discharged therefrom will converge on one another, forming a reactive plasma comprising reactive halogen ions by discharging converging gas streams from said electrodes and energizing said electrodes so as to create an electric discharge between said converging gas streams while the pressure within said chamber is at the level of atmospheric pressure, said reactive plasma comprising a first zone above and spaced from the region of said electrodes and said electric discharge that is characterized by a temperature in the order of 500° C. and a second zone below said first zone and proximate the region of said electrodes and said electric discharge that is characterized by a temperature substantially greater than the temperature of said first zone, positioning said coin stack in said chamber above said electrodes so that said wafers extend vertically and first edges of said wafers face down and extend to the level of said first zone but short of the level of said second zone, continuously moving said coin stack so that said first edges move in and out of said first zone repetitively and continuously with the time duration of each transit of said first edges in said first zone being limited so that said first edges are etched incrementally by reaction with said halogen ions, terminating movement of said coin stack, removing said coin stack from said chamber, reorienting said coin stack and repositioning said coin stack in said chamber above said electrodes so that said wafers still extend vertically but other edges of said wafers face down, continuously moving said coin stack so that said other edges move in and out of said first zone repetitively and continuously with the time duration of said other edges in said first zone being limited so that said other edges are etched incrementally by reaction with said halogen ions, and then terminating movement of said coin stack and removing said coin stack from said chamber.
Method of etching edges of a plurality of planar silicon semiconductor wafers having opposite faces and edge portions that are characterized by micro-cracks, said method comprising assembling said plurality of wafers into a plurality of coin stacks with the wafers in each stack being assembled face-to-face in contact with one another and with their edges in mutual alignment, supporting said stacks in a circular array on a carousel in an etching chamber with said coin stacks oriented so that said opposite faces extend vertically and selected edge portions of said wafers face downward, creating a reactive plasma containing halogen ions in a selected region of said chamber below said carousel and said coin stack while said chamber is at substantially atmospheric pressure by introducing first and second converging gas streams into said chamber and creating an electric discharge between said gas streams in the presence of a halogen-containing compound, and rotating said carousel in said chamber in proximity to said region so that said selected edge portions of the wafers in each stack repetitively move into and out of said plasma with said selected edge portions being in said plasma for only a limited time during each transit through said plasma, whereby said selected edge portions undergo etching by contacting said plasma on an intermittent basis.
Method of edge etching a plurality of semiconductor wafers wherein each wafer has four side edges with portions of wafers at said edges having micro-cacks, said method comprising the following steps:
- (a) assembling said plurality of wafers in face-to-face contact with each other so as to form a coin stack with the edges of each wafer aligned with the edges of adjacent wafers;
- (b) positioning said coin stack so that said wafers extend vertically and the wafer edges along a first side of said coin stack are facing down;
- (c) repetitively and continuously moving said first side of said coin stack into and out of contact with a reactive plasma stream containing halogen ions that is produced at atmospheric pressure by passing an electric current through at least two converging gas streams discharged by separate electrode nozzles located below said coin stack, whereby to etch away wafer edge portions along said first side having micro-cracks, each contact with said reactive plasma stream being for a period of time in the order of milliseconds;
- (d) repositioning said coin stack so that the wafers still extend vertically but the wafer edges along a second side of said coin stack are facing down;
- (e) repetitively and continuously moving said second side of said coin stack into and out of contact with a reactive plasma stream containing halogen ions that is produced at atmospheric pressure by passing an electric current through at least two converging gas streams discharged by separate electrode nozzles located below said coin stack, whereby to etch away wafer edge portions along said second side having micro-cracks, each contact with said reactive plasma stream being for a period of time in the order of milliseconds;
- (f) repositioning said coin stack so that the wafers still extend vertically but the wafer edges along a third side of said coin stack are facing down;
- (g) repetitively moving said third side of said coin stack into and out of contact with a reactive plasma stream containing halogen ions that is produced at atmospheric pressure by passing an electric current through at least two converging gas streams discharged by separate electrode nozzles located below said coin stack, whereby to etch away wafer edge portions along said third side, each contact with said reactive plasma stream being for a period of time in the order of milliseconds;
- (h) repositioning said coin stack so that the wafers still extend vertically but the wafer edges along a fourth side of said coin stack are facing down;
- and
- (i) repetitively moving said fourth side of said coin stack into and out of contact with a reactive plasma stream containing halogen ions that is produced at atmospheric pressure by passing an electric current through at least two converging gas streams discharged by separate electrode nozzles located below said coin stack, whereby to etch away wafer edge portions along said fourth side, said contact with said reactive plasma stream being for a period of time in the order of milliseconds.
Method of edge etching a plurality of planar semiconductor wafers so as to remove edge portions thereof that are characterized by micro-cracks, said method comprising assembling said plurality of wafers in a plurality of coin stacks with the wafers in each stack being in face to face contact in edge alignment with one another, supporting said stacks on a carousel in an etching chamber, with said carousel having a vertical axis of rotation and said coin stacks disposed in a circular array centered on and spaced from said axis of rotation and with said wafers oriented so that they extend vertically and certain of their edge portions face downwardly, generating a reactive plasma zone in a selected region of said chamber below said carousel and said coin stacks while maintaining the pressure within said chamber at the level of substantially atmospheric pressure, continuously rotating said carousel so that each stack in turn passes through said region with said selected edge portions of the wafers in said each stack repetitively contacting said plasma in said plasma zone for a limited time in the order of milliseconds, whereby to etch said edge portions to eliminate said micro-cracks, terminating rotation of said carousel after said microcracks have been eliminated, and removing said coin stacks from contact with said plasma after said micro-cracks have been eliminated.
Method of edge etching semiconductor wafers for the purpose of removing edge portions thereof that have micro-cracks, said method comprising assembling a plurality of coin stacks of said wafers, with each coin stack comprising a plurality of said wafers disposed in face-to-face contact and in edge alignment with one another, positioning said plurality of coin stacks in a circle about a vertical axis of rotation with said stacks arranged so that the wafers extend vertically and so that selected edges of the wafers in each stack face downward, generating a reactive plasma in a reaction chamber by creating an electric discharge through first and second mutually converging gas streams at substantially atmospheric pressure in the presence of a halogen-containing compound, said plasma having a first relatively high temperature zone adjacent to and above said electric discharge and a second relatively low temperature zone immediately above said first relatively high temperature zone, rotating said array of coin stacks about said axis of rotation at a level above the level of said converging gas streams so that said selected edges of the wafers in said each coin stack are transported repeatedly and continuously into and out of said second relatively low temperature zone above the level of said first relatively high temperature zone, whereby portions of each wafer may be etched away incrementally at said selected edges by reaction with said plasma, terminating rotation of said array of coin stacks after said micro-cracks have been removed by etching away portions of said wafers at said selected edges, and thereafter terminating exposure of said wafers to said plasma.
Method of edge etching a plurality of rectangular semiconductor wafers having first, second, third and fourth side edges defining a rectangular edge configuration for the purpose of removing edge portions thereof that have microcracks, said method comprising assembling said plurality of wafers face-to-face in contact with each other so as to form a coin stack with their edges in mutual alignment, creating a reactive plasma in a reaction chamber at substantially atmospheric pressure by creating an electric discharge through at least two upwardly directed converging gas streams, and positioning said coin stack in said chamber above the level of the region of said electric discharge with said wafers extending vertically and said first side edges facing down, continuously moving said coin stack horizontally in a circular path so that substantially said first side edges of said wafers are repetitively exposed to and are contacted by said plasma above said region of electric discharge for a limited time duration during each cycle of movement thereof along said circular path, whereby said portions of said wafers along said first side edges are etched away incrementally by said plasma, removing said coin stack from said chamber, repositioning said coin stack in said chamber above the level of the region of said electric discharge with said wafers extending vertically but said second side edges facing down, continuously moving said coin stack horizontally in a circular path so that substantially only said second side edges of said wafers are repetitively exposed to and are contacted by said plasma above said region of electric discharge for a limited time duration during each cycle of movement thereof along said circular path, whereby portions of said wafers along said second side edges are etched away incrementally by said plasma, and repeating the foregoing process so that said third and fourth side edges in turn a,-e repetitively exposed to and are contacted by said plasma above said region of electric discharge for a limited time duration, whereby portions of said wafers along said third and fourth side edges are etched away incrementally by said plasma.
Method of edge etching planar semiconductor wafers for the purpose of removing edge portions thereof that have micro-cracks, said method comprising assembling a plurality of coin stacks of said wafers, with each coin stack comprising a plurality of said wafers disposed in face-to-face contact and in edge alignment with one another, mounting said coin stacks on a carousel so that said coin stacks form a circular array and with said coin stacks oriented so that said each wafer extends in a vertical plane, and continuously and repetitively rotating said carousel above a reactive halogen ion-containing plasma stream produced and maintained at atmospheric pressure by an electric discharge between converging gas streams so that each stack in turn moves into and out of etching relation with said plasma stream with selected edge portions of the wafers in each stack being etched incrementally during each revolution of said carousel, stopping rotation of said carousel after etch removal of said edge portions, and removing said coin stacks from said carousel.
Method of etching the edges of a plurality of like semiconductor wafers of rectangular configuration for the purpose of removing micro-cracks at said edges, said method comprising assembling said plurality of wafers face-to-face in contact with each other so as to form a coin stack with the wafers having their edges in mutual alignment, providing a reaction chamber containing a plasma generator characterized by at least a pair of hollow gas discharge electrodes that are disposed adjacent one another and arranged so that gas streams discharged therefrom will converge on one another, forming an upwardly flowing re plasma stream comprising reactive halogen ions by discharging converging gas streams from said electrodes and energizing said electrodes so as to create an electric discharge between said converging gas streams while the pressure within said chamber is at the level of atmospheric pressure, said upwardly flowing reactive plasma stream comprising a first zone above and spaced from the region of said electrodes and said electric discharge that is characterized by a temperature in the order of 500° C. and a second zone below said first zone and proximate the region of said electrodes and said electric discharge that is characterized by a temperature substantially greater than the temperature of said first zone, positioning said coin stack in said chamber above said electrodes so that said wafers extend vertically and first edges of said wafers face down and extend to the level of said first zone but short of the level of said second zone, continuously moving said coin stack so that said first edges move in and out of said first zone repetitively and continuously with the time duration of each transit of said first edges in said first zone being limited so that said first edges are etched incrementally by reaction with said halogen ions, terminating movement of said coin stack and removing said coin stack from said chamber after said first edges have been exposed to said plasma gas stream for a period of time sufficient to etch away substantially all microcracks from said first edge and to limit the etching substantially to edge portions of said wafers, reorienting said coin stack and repositioning said coin stack in said chamber above said electrodes so that said wafers still extend vertically but other edges of said wafers face down, continuously moving said coin stack so that said other edges move in and out of said first zone repetitively and continuously with the time duration of said other edges in said first zone being limited so that said other edges are etched incrementally by reaction with said halogen ions, and then terminating movement of said coin stack and removing said coin stack from said chamber after said other edges have been exposed to said plasma gas stream for a period of time sufficient to etch away substantially all microcracks from said other edges and to limit the etching substantially to edge portions of said wafers.
Method of edge etching a plurality of planar semiconductor wafers so as to remove edge portions thereof that are characterized by micro-cracks, said method comprising assembling said plurality of wafers in a plurality of coin stacks with the wafers in each stack being in face to face contact in edge alignment with one another, supporting said stacks on a carousel in an etching chamber, with said carousel having a vertical axis of rotation and said coin stacks disposed in a circular array centered on and spaced from said axis of rotation and with said wafers oriented so that they extend vertically and certain of their edge portions face downwardly, generating an upwardly flowing reactive plasma stream in a selected region of said chamber below said carousel and said coin stacks while maintaining the pressure within said chamber substantially at the level of atmospheric pressure, maintaining said plasma stream within said chamber at substantially atmospheric pressure, continuously rotating said carousel so that each stack in turn passes through said plasma stream with said selected edge portions of the wafers in said each stack repetitively contacting said plasma stream for a limited time in the order of milliseconds, whereby to etch said edge portions to eliminate said micro-cracks, terminating rotation of said carousel and removing said coin stacks from contact with said plasma stream after said micro-cracks have been eliminated and while the etching has been limited substantially to said edge portions.
Method of edge etching a plurality of rectangular polycrystalline semiconductor wafers having first, second, third and fourth side edges defining a rectangular edge configuration for the purpose of removing edge portions thereof that have micro-cacks, said method comprising assembling said plurality of wafers face-to-face in contact with each other so as to form a coin stack with their edges in mutual alignment, creating an upwardly flowing reactive plasma stream in a reaction chamber at substantially atmospheric pressure by creating an electric discharge through at least two upwardly directed converging gas streams, maintaining said reactive plasma stream while maintaining the pressure within said chamber at substantially atmospheric pressure, positioning said coin stack in said chamber above the level of the region of said electric discharge with said wafers extending vertically and said first side edges facing down, continuously moving said coin stack horizontally in a circular path so that substantially said first side edges of said wafers are repetitively exposed to and are contacted by said reactive plasma stream above said region of electric discharge for a limited time duration during each cycle of movement thereof along said circular path, whereby said portions of said first side edges are etched away incrementally by said plasma, removing said coin stack from said chamber after etch removal of micro-cracks from said first side edges, repositioning said coin stack in said chamber above the level of the region of said electric discharge with said wafers extending vertically but said second side edges facing down, continuously moving said coin stack horizontally in a circular path so that substantially only said second side edges of said wafers are repetitively exposed to and are contacted by said plasma stream above said region of electric discharge for a limited time duration during each cycle of movement thereof along said circular path, whereby portions of said wafers along said second side edges are etched away incrementally by said plasma stream, removing said coin stack from said chamber after etch removal of micro-cracks from said second side edges, and repeating the foregoing process so that said third and fourth side edges in turn are repetitively exposed to and are contacted by said plasma stream above said region of electric discharge for a limited time duration, whereby edge portions with micro-cracks along said third and fourth side edges are etched away incrementally by said plasma.
Dependencies are inferred from the claim text.