Loading metal particles into cell membrane vesicles and metal particular use for imaging and therapy
OwnerJames F. Hainfeldinventor
Life of this patent
Estimating the term…
Abstract
Delivery of metal particles to living tissue, then applying external energy that interacts with the metal particles, is found to selectively increase the energy deposition and interaction surrounding the metal particles. The method is useful to improve treatment of various conditions, since targeted cells may be selectively altered or killed. Metal particles are also loaded into cells or membrane vesicles by placing metal seed particles into the cells or vesicles, then chemically depositing additional metal on the metal seed particles. The metal particles are useful to improve imaging and therapies by their interaction with externally applied energy.
Claims43
A method for loading metal particles into erythrocyte membrane vesicles, comprising the steps, in the following order:
- a) providing erythrocytes in a solution containing metal nucleating particles which have a catalytic surface suitable for metal ion deposition;
- b) treating the erythrocytes to produce an opening in the surface membrane of the erythrocytes to allow passive loading of the metal nucleating particles, thereby producing erythrocyte membrane vesicles which contain the metal nucleating particles;
- c) treating the erythrocyte membrane vesicles to reduce the size of the opening produced in step b) to allow retention of the metal nucleating particles within the erythrocyte membrane vesicles;
- d) washing the erythrocyte membrane vesicles to remove extracellular metal nucleating particles;
- and
- e) treating the erythrocyte membrane vesicles to catalytically deposit metal by diffusing metal ions in combination with a reducing agent through openings of step c), whereby the reducing agent acts to catalytically reduce the metal ion to form an insoluble metal which is immobilized internally around the nucleating small metal particles within the erythrocyte membrane vesicles thereby producing metal particles which occupy more than 10% of the erythrocyte membrane vesicle internal volume.
A method for loading metal particles into erythrocyte membrane vesicles, comprising:
- a) providing erythrocytes;
- b) washing the erythrocytes in physiologically buffered solution;
- c) lysing the washed erythrocytes hypotonically in a solution containing from 20 to 200 μMolar metal nucleating particles which have a catalytic surface suitable for metal ion deposition, thereby producing erythrocyte membrane vesicles which contain the metal nucleating particles;
- d) incubating the erythrocyte membrane vesicles of step c) at 37° C. for between 5 and 15 minutes;
- e) washing the incubated erythrocyte membrane vesicles of step d) with physiologically buffered solution, to remove extracellular metal nucleating particles;
- and
- f) treating the washed erythrocyte membrane vesicles of step e) to catalytically deposit metal by diffusing metal ions in combination with a reducing agent into the erythrocyte membrane vesicles of step c) whereby the reducing agent acts to catalytically reduce the metal ion to form an insoluble metal which is immobilized internally around the nucleating small metal particles within the erythrocyte membrane vesicles to produce metal particles which occupy more than 10% of the erythrocyte membrane vesicle internal volume.
A method for loading metal particles into erythrocyte membrane vesicles, comprising:
- a) providing erythrocytes;
- b) washing the erythrocytes in physiologically buffered solution;
- c) lysing the washed erythrocytes in a physiologically buffered solution containing a detergent, and from 20 to 200 μMolar metal nucleating particles which have a catalytic surface suitable for metal ion deposition, thereby producing erythrocyte membrane vesicles which contain metal nucleating particles;
- d) washing the erythrocyte membrane vesicles produced in step c) with physiologically buffered solution, to remove extracellular metal nucleating particles;
- and
- e) treating the washed erythrocyte membrane vesicles of step d) to catalytically deposit metal by diffusing metal ions in combination with a reducing agent into the erythrocyte membrane vesicles of step c) whereby the reducing agent acts to catalytically reduce the metal ion to form an insoluble metal which is immobilized internally around the nucleating small metal particles within the erythrocyte membrane vesicles to produce metal particles which occupy more than 10% of the erythrocyte membrane vesicle internal volume.
A method for loading metal particles into erythrocyte membrane fragment vesicles, comprising:
- a) providing erythrocytes;
- b) washing the erythrocyte in physiologically buffered solution;
- c) lysing the washed erythrocytes hypotonically in a solution containing from 20 to 200 μMolar metal nucleating particles which have a catalytic surface suitable for metal ion deposition, thereby producing erythrocyte membrane vesicles which contain the metal nucleating particles;
- d) homogenizing the erythrocyte membrane vesicles of step c) to produce small erythrocyte membrane vesicles from 0.02 μm to 4 μm in diameter;
- e) incubating the small erythrocyte membrane vesicles of step d) to 37° C. for between 5 and 15 minutes;
- f) washing the incubated erythrocyte membrane fragment vesicles of step e) with physiologically buffered solution, to remove extracellular metal nucleating particles;
- and
- g) treating the washed small erythrocyte membrane vesicles of step f) to catalytically deposit metal by diffusing metal ions in combination with a reducing agent into the erythrocyte membrane vesicles of step c) whereby the reducing agent acts to catalytically reduce the metal ion to form an insoluble metal which is immobilized internally around the nucleating small metal particles within the small erythrocyte membrane vesicles to produce metal particles which occupy more than 10% of the erythrocyte membrane vesicle internal volume.
A method for loading metal particles into erythrocyte membrane vesicles, comprising:
- a) providing erythrocytes;
- b) washing the erythrocytes in physiologically buffered solution;
- c) lysing the washed erythrocytes in a physiologically buffered solution containing a detergent, and from 20 to 200 μMolar metal nucleating particles which have a catalytic surface suitable for metal ion deposition, thereby producing erythrocyte membrane vesicles which contain metal nucleating particles;
- d) homogenizing the erythrocyte membrane vesicles of step c) to produce small erythrocyte membrane vesicles from 0.02 μm to 4 μm in diameter, which contain metal nucleating particles;
- e) washing the small erythrocyte membrane vesicles of step d) with physiologically buffered'solution, to remove extracellular metal nucleating particles;
- and
- f) treating the washed small erythrocyte membrane vesicles of step e) to catalytically deposit metal by diffusing metal ions in combination with a reducing agent into the erythrocyte membrane vesicles of step c) whereby the reducing agent acts to catalytically reduce the metal ion to form an insoluble metal which is immobilized internally around the nucleating small metal particles within the small erythrocyte membrane vesicles to produce metal particles which occupy more than 10% of the erythrocyte membrane vesicle internal volume.
Dependencies are inferred from the claim text.