Method for producing barium titanate based powders by oxalate process
AssigneeSamsung Electro-Mechanics Co., Ltd.
InventorsJai Joon Lee, Kang Heon Hur
Life of this patent
Estimating the term…
Loading patent…
AssigneeSamsung Electro-Mechanics Co., Ltd.
InventorsJai Joon Lee, Kang Heon Hur
Estimating the term…
The method is carried out in the following manner: An aqueous mixture solution containing barium chloride and titanium chloride is added into an aqueous oxalic acid solution, so that barium titanyl oxalate would be precipitated. Then the precipitates are aged, washed and filtered. The filtered barium titanyl oxalate precipitates are crushed, and dried. Then a thermal decomposition is carried out to obtain a agglomerated barium titanate powder, and this is crushed again to obtain the final barium titanate powder. In order to obtain barium titanate based powder such as Ba(Ti1−zZrz)O3, (Ba1−xCax)(Ti1−zZrz)O3, and (Ba1−x−yCaxSry)(Ti1−zZrz)O3, the desired elements (Ca, Sr, Zr and so on) are added to barium titanyl oxalate when crushed before thermal decomposition step. After thermal decomposition and crushing, the barium titanate based powder can be obtained.
A method for manufacturing a barium titanate powder by an oxalate process, comprising the steps of:
A method for manufacturing a perovskite-type barium titanate based powder by an oxalate process, comprising the steps of:
Dependencies are inferred from the claim text.