# US 6,586,297 B1 · Method for integrating a metastable base into a high-performance HBT and related structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,586,297 B1
- Document ID: US6586297B1
- Status: Granted
- Kind: B1
- Application number: 10/160,979
- Filed: 2002-06-01
- Granted: 2003-07-01
- Earliest claimed: 2002-06-01
- Assignees: Newport Fab, LLC
- Inventors: Greg D. U'Ren; Klaus F. Schuegraf
- Web page: https://patentgrep.com/patent/US6586297B1

## CPC

- H10D 10/021: {of heterojunction BJTs [HBT]}
- H10D 10/891: {comprising lattice-mismatched active layers, e.g. SiGe strained-layer transistors}
- H10D 84/0109: {the at least one component covered by H10D12/00 or H10D30/00 being a MOS device}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

According to one exemplary embodiment, a heterojunction bipolar transistor is fabricated by forming a metastable epitaxial silicon-germaniuim base on a collector. The metastable epitaxial silicon-gernaniuim base, for example, may have a concentration of germanium greater than 20.0 atomic percent of germanium. The heterojunction bipolar transistor, for example, may be an NPN silicon-germanium heterojunction bipolar transistor. According to this exemplary embodiment, the heterojunction bipolar transistor is further fabricated by fabricating an emitter over the metastable epitaxial silicongermanium base. The heterojunction bipolar transistor is further fabricated by doping the emitter with a first dopant. The first dopant, for example, may be arsenic. The heterojunction bipolar transistor is further fabricated by heating the metastable epitaxial silicon-germanium base in a spike anneal process so as to maintain the metastable epitaxial silicon-germanium base as a strained crystalline structure after the spike anneal process and so as to diffusion the first dopant to form emitter-base junction.

## Claims

### Claim 1

A method for fabricating a heterojunction bipolar transistor, said method comprising steps of:
forming a metastable epitaxial silicon-germanium base on a collector;
fabricating an emitter over said metastable epitaxial silicon-germanium base;
doping said emitter with a first dopant;
heating said metastable epitaxial silicon-germanium base in a spike anneal process so as to maintain said metastable epitaxial silicon-germanium base as a strained crystalline structure after said spike anneal process and so as to diffuse said first dopant to form an emitter-base junction.

### Claim 2 (depends on 1)

The method of claim 1 wherein said epitaxial silicon-germanium base comprises a concentration of germanium greater than 20.0 atomic percent of germanium.

### Claim 3 (depends on 1)

The method of claim 1 wherein the thickness of said metastable epitaxial silicon-germanium base is greater than a critical thickness.

### Claim 4 (depends on 1)

The method of claim 1 wherein said epitaxial silicon-germanium base comprises a concentration of germanium greater than 30.0 atomic percent of germanium.

### Claim 5 (depends on 1)

The method of claim 1 wherein the width of said emitter is approximately 0.2 microns.

### Claim 6 (depends on 1)

The method of claim 1 wherein the width of said emitter is approximately 0.9 microns.

### Claim 7 (depends on 1)

The method of claim 1 wherein said first dopant is arsenic.

### Claim 8 (depends on 1)

The method of claim 1 wherein said epitaxial silicon-germanium base comprises a concentration of germanium approximately equal to 40.0 atomic percent of germanium.

### Claim 9 (depends on 1)

The method of claim 1 wherein said emitter comprises polycrystalline silicon.

### Claim 10 (depends on 1)

The method of claim 1 wherein said heterojunction bipolar transistor is an NPN silicon-germanium heterojunction bipolar transistor.

### Claim 11

A method for fabricating a heterojunction bipolar transistor, said method comprising steps of:
forming a silicon-germnanium base on a substrate;
implanting a dopant in an extrinsic region of said silicon-germnanium base;
heating said silicon-germnanium base in a spike annealryocess so as to reduce damage to said silicon-germaniumn base resulting from said implanting step.

### Claim 12 (depends on 11)

The heterojunction bipolar transistor of claim 11 wherein said heterojunction bipolar transistor is an NPN silicon-germnanium heterojunction bipolar transistor.

### Claim 13 (depends on 11)

The heterojunction bipolar transistor of claim 11 wherein said dopant is boron.