# US 6,585,365 B1 · Paper coating for ink jet printing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 6,585,365 B1
- Document ID: US6585365B1
- Status: Granted
- Kind: B1
- Application number: 09/667,749
- Filed: 2000-09-21
- Granted: 2003-07-01
- Earliest claimed: 2000-01-18
- Assignees: Lexmark International, Inc.
- Inventors: David Starling MacMillan
- Web page: https://patentgrep.com/patent/US6585365B1

## CPC

- B41M 5/52: Macromolecular coatings
- B41M 5/0011: {Pre-treatment or treatment during printing of the recording material, e.g. heating, irradiating (after-treatment of prints B41M7/00; printers for treating or overcoating copy materials before, during or after printing B41J11/0015)}
- B41M 5/5245: {characterised by the use of polymers containing cationic or anionic groups, e.g. mordants}
- B41M 5/508: {Supports}
- B41M 5/5218: {characterised by inorganic additives, e.g. pigments, clays}
- B41M 5/5227: {characterised by organic non-macromolecular additives, e.g. UV-absorbers, plasticisers, surfactants}
- B41M 5/529: {characterised by the use of fluorine- or silicon-containing organic compounds}
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)

## Abstract

The invention provides an improved paper coating system for ink jet printing applications. The system includes an ink jet printer containing an ink jet pen and a paper coating device for coating a print media with an effective amount of coating composition prior to printing thereon. The coating composition preferably includes from about 0.25 to about 20% by weight of a first component selected from the group consisting of polyvalent metal salt and organic acid, a second component consisting of from about 1 to about 20% by weight amine polymer, from about 0.25 to about 2.0% by weight surfactant and from about 25 to about 96% by weight glycol-based solvent having a surface tension ranging from about 25 to below about 45 dynes/cm. Since the coating composition is free from ethylene glycol-based components, the composition is safer to use and less harmful to humans and the environment. The composition has also been found to provide improved ink drying with less bleeding or smearing of image.

## Claims

### Claim 1

A system for printing with an ink jet printer, the system comprising an ink jet printer containing an ink jet pen and a paper coating device for coating a print media with an effective amount of coating composition prior to printing thereon, the coating composition including from about 0.25 to about 20% by weight of a first component selected from the group consisting of polyvalent metal salt and organic acid, a second component consisting of from about 1 to about 20% by weight amine polymer, from about 0.25 to about 2.0% by weight surfactant and from about 25 to about 96% by weight glycol-based solvent having a surface tension ranging from about 25 to below about 45 dynes/cm.

### Claim 2 (depends on 1)

The printing system of claim 1 wherein the amine polymer comprises a cationic amine polymer.

### Claim 3 (depends on 2)

The printing system of claim 2 wherein the cationic amine polymer is a compound of the formula
wherein x is an integer ranging from about 15 to about 2000.

### Claim 4 (depends on 2)

The printing system of claim 2 wherein the cationic amine polymer is derived from dimethylamine and epichlorohydrin and has a number average molecular weight ranging from about 7,500 to about 10,000 MWN.

### Claim 5 (depends on 2)

The printing system of claim 2 wherein the surfactant comprises a polysiloxane surfactant.

### Claim 6 (depends on 5)

The printing system of claim 5 wherein the polysiloxane surfactant is a compound having the following general structure:
wherein: PE comprises —CH2CH2CH2O(EO)n(PO)oZ, Me is a methyl group, EO is an ethyleneoxy group, PO is a 1,2-propyleneoxy group, Z is H or a lower alkyl radical y is an integer ranging from about 1 to about 10, m is an integer ranging from about 1 to about 10, n is an integer ranging from about 0 to about 5 and o is an integer ranging from about 0 to about 5.

### Claim 7 (depends on 1)

The printing system of claim 1 wherein the polyvalent metal salt is selected from the group consisting of calcium chloride, magnesium chloride, calcium acetate hydrate, magnesium acetate tetrahydrate and mixtures thereof.

### Claim 8 (depends on 1)

The printing system of claim 1 wherein the glycol-based solvent is selected from the group consisting of tripropylene glycol, dipropylene glycol, 1,2-propanediol and mixtures of dipropylene glycol and 1,2-propanediol having a surface tension ranging from about 25 to about 45 dynes/cm.

### Claim 9 (depends on 1)

The printing system of claim 1 wherein the coating composition further comprises up to about 40% by weight deionized water.

### Claim 10 (depends on 1)

The printing system of claim 1 wherein the organic acid comprises a hydroxy acid selected from the group consisting of lactic acid, glycolic acid, citric acid and malic acid.

### Claim 11 (depends on 10)

The printing system of claim 10 wherein the hydroxy acid comprises citric acid.

### Claim 12 (depends on 1)

The printing system of claim 1 wherein the coating composition is applied to the print media in an amount ranging from 0.08 mg/cm2 to about 0.25 mg/cm2.

### Claim 13 (depends on 1)

A cellulosic web containing the coating composition of the printing system of claim 1.

### Claim 14

A method for improving print resolution comprising applying a coating composition to a cellulosic web to provide an ink receptive coating thereon and printing on the coated web prior to drying the coating composition, wherein the coating composition contains from about 0.25 to about 20% by weight of a first component selected from the group consisting of polyvalent metal salt and organic acid, a second component consisting of from about 1 to about 20% by weight amine polymer, from about 0.25 to about 2.0% by weight surfactant and from about 25 to about 96% by weight glycol-based solvent having a surface tension ranging from about 25 to below about 45 dynes/cm.

### Claim 15 (depends on 14)

The method of claim 14 wherein the amine polymer comprises a cationic amine polymer.

### Claim 16 (depends on 15)

The method of claim 15 wherein the cationic amine polymer is a compound of the formula
wherein x is an integer ranging from about 15 to about 2000.

### Claim 17 (depends on 15)

The method of claim 15 wherein the cationic amine polymer is derived from dimethylamine and epichlorohydrin and has a number average molecular weight ranging from about 7,500 to about 10,000 MWN.

### Claim 18 (depends on 15)

The method of claim 15 wherein the surfactant comprises a polysiloxane surfactant.

### Claim 19 (depends on 8)

The method of claim 8 wherein the polysiloxane surfactant is a compound having the following general structure:
wherein: PE comprises —CH2CH2CH2O(EO)n(PO)oZ, Me is a methyl group, EO is an ethyleneoxy group, PO is a 1,2-propyleneoxy group, Z is H or a lower alkyl radical y is an integer ranging from about 1 to about 10, in is an integer ranging from about 1 to about 10, n is an integer ranging from about 0 to about 5 and o is an integer ranging from about 0 to about 5.

### Claim 20 (depends on 14)

The method of claim 14 wherein the polyvalent metal salt is selected from the group consisting of calcium chloride, magnesium chloride, calcium acetate hydrate, magnesium acetate tetrahydrate and mixtures thereof.

### Claim 21 (depends on 14)

The method of claim 14 wherein the glycol-based solvent is selected from the group consisting of tripropylene glycol, dipropylene glycol, 1,2-propanediol and mixtures of dipropylene glycol and 1,2-propanediol having a surface tension ranging from about 25 to about 45 dynes/cm.

### Claim 22 (depends on 14)

The method of claim 14 wherein the coating composition further comprises up to about 40% by weight deionized water.

### Claim 23 (depends on 14)

The method of claim 14 wherein the organic acid comprises a hydroxy acid selected from the group consisting of lactic acid, glycolic acid, citric acid and malic acid.

### Claim 24 (depends on 23)

The method of claim 23 wherein the hydroxy acid comprises citric acid.

### Claim 25 (depends on 14)

The method of claim 14 wherein the coating composition is applied to the print media in an amount ranging from about 0.08 mg/cm2 to about 0.35 mg/cm2.

### Claim 26

A cellulosic web containing ink and a penetrant promoter coating, the coating being applied to the web prior to printing in an amount sufficient to reduce ink bleeding, promote ink drying and/or penetration of ink into the web, the promoter composition comprising from about 0.25 to about 20% by weight of a first component selected from the group consisting of polyvalent metal salt and organic acid, a second component consisting of from about 1 to about 20% by weight amine polymer, from about 0.25 to about 2.0% by weight surfactant and from about 25 to about 96% by weight glycol-based solvent having a surface tension ranging from about 25 to about 45 dynes/cm.

### Claim 27 (depends on 26)

The web of claim 26 wherein the penetrant promoter coating contains from about 5 to about 30% by weight cationic amine polymer.

### Claim 28 (depends on 27)

The web of claim 27 wherein the cationic amine polymer is a compound of the formula
wherein x is an integer ranging from about 15 to about 2000.

### Claim 29 (depends on 27)

The web of claim 27 wherein the cationic amine polymer is derived from dimethylamine and epichlorohydrin and has a number average molecular weight ranging from about 7,500 to about 10,000 MWN.

### Claim 30 (depends on 26)

The web of claim 26 wherein the penetrant promoter coating further comprises a polysiloxane surfactant.

### Claim 31 (depends on 30)

The web of claim 30 wherein the polysiloxane surfactant is a compound having the following general structure:
wherein: PE comprises —CH2CH2CH2O(EO)n(PO)oZ, Me is a methyl group, EO is an ethyleneoxy group, PO is a 1,2-propyleneoxy group, Z is H or a lower alkyl radical y is an integer ranging from about 1 to about 10, m is an integer ranging from about 1 to about 10, n is an integer ranging from about 0 to about 5 and o is an integer ranging from about 0 to about 5.

### Claim 32 (depends on 26)

The web of claim 26 wherein the polyvalent metal salt is selected from the group consisting of calcium chloride, magnesium chloride, calcium acetate hydrate, magnesium acetate tetrahydrate and mixtures thereof.

### Claim 33 (depends on 26)

The web of claim 26 wherein the ratio of ink to penetrant promoter coating ranges from about 6:1 to about 18:1 parts of ink per part of penetrant promoter coating by weight.

### Claim 34 (depends on 26)

The web of claim 26 wherein the penetrant promoter coating is applied to a cellulosic web in an amount ranging from about 0.08 mg/cm2 to about 0.25 mg/cm2.

### Claim 35 (depends on 26)

The web of claim 26 wherein the glycol-based solvent is selected from the group consisting of tripropylene glycol, dipropylene glycol, 1,2-propanediol and mixtures of dipropylene glycol and 1,2-propanediol having a surface tension ranging from about 25 to about 45 dynes/cm.

### Claim 36 (depends on 26)

The web of claim 26 wherein the coating composition further comprises up to about 40% by weight deionized water.

### Claim 37 (depends on 26)

The web of claim 26 wherein the organic acid comprises a hydroxy acid selected from the group consisting of lactic acid, glycolic acid, citric acid and malic acid.

### Claim 38 (depends on 37)

The web of claim 37 wherein the organic acid comprises citric acid.